Compressive yield stress improvement using thermomechanical treatment of extruded Mg-Zn-Ca alloy

P. Dobroň, D. Drozdenko, J. Olejňák, M. Hegedüs, K. Horváth, J. Veselý, J. Bohlen, D. Letzig

Publisher page

Abstract

Abstract Thermomechanical treatment consisting of pre-compression and a subsequent isothermal aging was used to improve the compressive properties of extruded Mg-Zn-Ca (ZX10) alloy. Isothermal aging at 150 °C and 200 °C was performed on as-extruded samples for various times to find peak aged conditions. To achieve a different twin volume fraction in the alloy, samples were pre-compressed up to 2%, 3% and 4% along the extrusion direction. Afterwards, the peak-aged conditions were applied to the pre-compressed samples to enhance their mechanical properties. It was found that after the 4 h@150 °C thermomechanical treatment, deformation curves exhibit a distinctive yield plateau independently on the pre-strain level. Using the 2 h@200 °C condition, the yield plateau occurs only after pre-strain of 3%. Higher compressive yield strength values were observed for the thermomechanically treated samples at the lower temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Precipitation hardening of Mg-Ca-Zn alloys10.1016/S1359-6462(97)00294-7 ↗
2. TEM and 3DAP characterization of an age-hardened Mg–Ca–Zn alloy10.1016/j.scriptamat.2005.05.030 ↗
3. Age-hardening response of Mg–0.3at%Ca alloys with different Zn contents10.1016/j.msea.2009.07.027 ↗
4. Precipitation-hardened Mg–Ca–Zn alloys with superior creep resistance10.1016/j.scriptamat.2005.08.035 ↗
5. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
6. Effects of Zn addition on the mechanical properties and texture of extruded Mg-Zn-Ca-Ce magnesium alloy sheets10.1016/j.msea.2017.08.036 ↗
7. Threshold creep behaviour of an aged Mg–Zn–Ca alloy10.1016/j.msea.2017.04.104 ↗
8. Development of dilute Mg–Zn–Ca–Mn alloy with high performance via extrusion10.1016/j.jallcom.2016.01.195 ↗
9. The effects of microalloying on the precipitate microstructure at grain boundary regions in an Mg-Zn-based alloy10.1016/j.matdes.2017.01.073 ↗
10. Effect of Zn addition on hot tearing behaviour of Mg–0.5Ca–xZn alloys10.1016/j.matdes.2015.08.026 ↗
11. Microstructure, mechanical properties and bio-corrosion properties of Mg–Zn–Mn–Ca alloy for biomedical application10.1016/j.msea.2008.06.019 ↗
12. High-strength low-alloy (HSLA) Mg–Zn–Ca alloys with excellent biodegradation performance10.1007/s11837-014-0875-5 ↗
13. The yield asymmetry and precipitation behavior of pre-twinned ZK60 alloy10.1016/j.msea.2015.11.092 ↗
14. The influence of a secondary twin on the detwinning deformation of a primary twin in Mg–3Al–1Zn alloy10.1016/j.msea.2014.03.068 ↗
15. Improvement of formability and mechanical properties of magnesium alloys via pre-twinning: a review10.1016/j.matdes.2014.05.034 ↗
16. A new annealing hardening mechanism in pre-twinned Mg–3Al–1Zn alloy10.1016/j.msea.2015.12.046 ↗
17. Effect of heat treatment and pre-deformation on damping capacity of cast Mg-Y binary alloys10.1016/j.jallcom.2016.12.299 ↗
18. Microstructure and mechanical properties of an Mg-4.0Sm-1.0Ca alloy during thermomechanical treatment10.1016/S1002-0721(16)60145-X ↗
19. Microstructure analysis and corrosion behavior of biodegradable Mg–Ca implant alloys10.1016/j.matdes.2011.06.057 ↗
20. Influence of Ca and Zn on the microstructure and corrosion of biodegradable Mg–Ca–Zn alloys10.1016/j.corsci.2015.01.027 ↗
21. Three-dimensional analysis of the microstructure and bio-corrosion of Mg–Zn and Mg–Zn–Ca alloys10.1016/j.matchar.2015.12.008 ↗
22. Design and characterizations of novel biodegradable ternary Zn-based alloys with IIA nutrient alloying elements Mg, Ca and Sr10.1016/j.matdes.2015.05.089 ↗
23. Quantification of dislocation structure heterogeneity in deformed polycrystals by EBSD10.1088/0965-0393/20/2/024007 ↗
24. Grain size effects on deformation twinning in an extruded magnesium alloy tested in compression10.1016/j.scriptamat.2011.05.027 ↗
25. Evolution of twinning in extruded AZ31 alloy with bimodal grain structure10.1016/j.matchar.2017.02.017 ↗
26. Investigating a twinning-detwinning process in wrought Mg alloys by the acoustic emission technique10.1016/j.actamat.2016.03.013 ↗
27. Pseudoelastic behaviour of cast magnesium AZ91 alloy under cyclic loading-unloading10.1016/S1359-6454(03)00444-0 ↗
28. In situ neutron diffraction investigation of deformation twinning and pseudoelastic-like behaviour of extruded AZ31 magnesium alloy10.1016/j.ijplas.2008.08.002 ↗
29. Yield point elongation due to twinning in a magnesium alloy10.1016/j.actamat.2011.11.022 ↗
30. On the limits of acoustic emission detectability for twinning10.1016/j.matlet.2016.07.063 ↗
31. Solute strengthening of prismatic slip, basal slip and {1 0 -1 2} twinning in Mg and Mg-Zn binary alloys10.1016/j.ijplas.2013.01.012 ↗