High-temperature thermal stability of Hi-Nicalon™ SiC fiber/SiC matrix composites under long term cyclic heating
Source abstract
Abstract
Abstract The high-temperature thermal stability of C-coated standard grade Nicalon™ SiC fiber and of C or BN-coated Hi-Nicalon™ SiC fiber-reinforced SiC matrix composites under long-term cyclic heat exposure in air has been studied. Woven fabric composites fabricated by the PIP process were cyclic heat-exposed at 1273 and 1673 K for up to 1000 h with one heat exposure cycle of 200 h. The degradation of the composites was evaluated by a three-point flexure test at room temperature. The oxidation of the composite occurred from the matrix phase due to the existence of macro- and micro-pores that exist in the matrix. Degradation of the strength was observed for the C-coated SiC fiber/SiC composites after heat exposure for 200 h at 1273 K. On the contrary, the BN-coated Hi-Nicalon™ SiC fiber/SiC composite showed only a slight degradation even after a 1000-h exposure at 1273 K. However, at 1673 K, this composite's strength degraded after an 800-h exposure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Cao · J. Am. Ceram. Soc. · 1990 · 73 · 169110.1111/j.1151-2916.1990.tb09814.x ↗
2. Prouhet · J. Am. Ceram. Soc. · 1994 · 77 · 64910.1111/j.1151-2916.1994.tb05344.x ↗
3. Droillard · J. Am. Ceram. Soc. · 1996 · 79 · 84910.1111/j.1151-2916.1996.tb08516.x ↗
4. Kagawa · J. Mater. Sci. Lett. · 1997 · 16 · 85010.1023/A:1018551129863 ↗
5. Becher · J. Am. Ceram. Soc. · 1998 · 81 · 191910.1111/j.1151-2916.1998.tb02567.x ↗
6. Filipuzzini · J. Am. Ceram. Soc. · 1994 · 77 · 45910.1111/j.1151-2916.1994.tb07015.x ↗
7. Filipuzzini · J. Am. Ceram. Soc. · 1994 · 77 · 46710.1111/j.1151-2916.1994.tb07016.x ↗
8. Windish · J. Am. Ceram. Soc. · 1997 · 80 · 56910.1111/j.1151-2916.1997.tb02868.x ↗
9. Evans · J. Am. Ceram. Soc. · 1996 · 79 · 234510.1111/j.1151-2916.1996.tb08982.x ↗
10. Heredia · J. Am. Ceram. Soc. · 1995 · 78 · 209710.1111/j.1151-2916.1995.tb08621.x ↗
11. Steyer · J. Am. Ceram. Soc. · 1998 · 81 · 214010.1111/j.1151-2916.1998.tb02598.x ↗
12. Gonczy · Ceram. Eng. Sci. Proc. · 1995 · 16 · 43310.1002/9780470314715.ch48 ↗
13. Prouhet · J. Am. Ceram. Soc. · 1994 · 77 · 64910.1111/j.1151-2916.1994.tb05344.x ↗
14. Moore · Ceram. Eng. Sci. Proc. · 1995 · 16 · 37
15. Tredway · Ceram. Eng. Sci. Proc. · 1996 · 17 · 291
16. Suyama · Ceram. Eng. Sci. Proc. · 1993 · 17 · 118
17. Morscher · J. Am. Ceram. Soc. · 1997 · 80 · 202910.1111/j.1151-2916.1997.tb03087.x ↗
18. Takeda · Ceram. Eng. Sci. Proc. · 1997 · 18 · 77910.1002/9780470294437.ch85 ↗
19. Llorca · Acta Mater. · 1998 · 46 · 244110.1016/S1359-6454(98)80027-X ↗
20. Zhu · J. Am. Ceram. Soc. · 1999 · 82 · 11710.1111/j.1151-2916.1999.tb01731.x ↗
21. Takeda · J. Am. Ceram. Soc. · 1999 · 82 · 157910.1111/j.1151-2916.1999.tb01960.x ↗
22. S.Q. Guo, Y. Kagawa, J. Am, Ceram. Soc., submitted for publication.
23. Takeda · Ceram. Eng. Sci. Proc. · 1993 · 14 · 54010.1002/9780470314180.ch79 ↗
24. Vaughn · J. Am. Ceram. Soc. · 1990 · 73 · 154010.1111/j.1151-2916.1990.tb09793.x ↗
25. Zheng · J. Electrochem. Soc. · 1990 · 137 · 281210.1149/1.2087080 ↗
26. Marsh · 1989 · 107
27. The Encyclopedia of Ceramics, second ed., Ceramic Society of Japan, Maruzen, Tokyo, 1997, p. 184.
28. Nicaloceram™, Nippon Carbon Data Sheet, Yokohama, Japan, 1995.
29. Sheldon · J. Am. Ceram. Soc. · 1996 · 79 · 53910.1111/j.1151-2916.1996.tb08163.x ↗
30. Oda · J. Mater. Sci. · 1993 · 28 · 656210.1007/BF00356394 ↗