Macro/microstructure evolution and mechanical properties of Ti33.3Al alloys by adding WC particles
Source abstract
Abstract
Abstract In order to improve mechanical properties of binary TiAl alloys, Ti33.3Al (weight percent, hereafter in wt%) alloys with different WC particles content (1.5%, 3.0%, 4.5%, 6.0%, 7.5%) were prepared by vacuum arc melting. The phase constitution, macro/microstructure evolution and mechanical properties were investigated systematically. XRD results showed that WC disappeared and Ti2AlC phase appeared after adding WC particles because of WC reacting with Ti and Al. In addition, the lattice parameters of α2 phase increased due to the solid solubility of interstitial carbon atoms and substitutional tungsten atoms. For microstructure, rod-like Ti2AlC particles formed when WC content was more than 3.0%, and the length diameter ratio of Ti2AlC particles increased when WC content was 7.5%. It was found that the shape changing of Ti2AlC was in accordance with the morphology of lamellar colony, which indicated Ti2AlC firstly formed during solidification. The microstructure changed from coarse columnar to fine equiaxed and the average size of lamellar colony decreased from 189.7 to 66.5 µm with increasing WC content. Tungsten segregated and formed a little B2 phase in the lamellar colony when the WC content was more than 6.0%. Compressive testing showed that the strength and the strain were improved from 1847 to 2324 MPa and from 25.7% to 28.5%, respectively. The Vickers hardness of Ti33.3Al alloys was also improved by the addition of WC. The improvement of mechanical properties was caused by the grain refinement, solid solution of carbon and tungsten atoms, reinforcement of Ti2AlC phase and a little B2 phase.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. High-temperature structural intermetallics10.1016/S1359-6454(99)00301-8 ↗
2. Electrochemical corrosion and tribological evaluation of TiAl alloy for marine application10.1016/j.triboint.2017.06.027 ↗
3. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
4. Modeling concepts for intermetallic titanium aluminides10.1016/j.pmatsci.2016.01.001 ↗
5. Microstructure and mechanical properties of cast in-situ TiAl matrix composites reinforced with (Ti,Nb) 2 AlC particles10.1016/j.matdes.2017.08.012 ↗
6. Effects of Ti 5 Si 3 characteristics adjustment on microstructure and tensile properties of in-situ (Ti 5 Si 3 +TiBw)/Ti6Al4V composites with two-scale network architecture10.1016/j.msea.2016.07.112 ↗
7. Thermal stability of an intermediate strength fully lamellar Ti-45Al-2Mn-2Nb-0.8 vol% TiB2 alloy10.1016/j.intermet.2014.05.015 ↗
8. The microstructure and tensile properties of the Ti2AlC reinforced TiAl composites fabricated by powder metallurgy10.1016/j.msea.2014.06.009 ↗
9. Influence of nitrogen on the microstructure and solidification behavior of high Nb containing TiAl alloys10.1016/j.matdes.2016.04.071 ↗
10. Effect of Y2O3 particles on the fracture toughness of directionally solidified TiAl-based alloys10.1016/j.msea.2017.07.059 ↗
11. Mechanical properties and microstructure of Al2O3/TiAl in situ composites doped with Cr2O310.1016/j.msea.2011.01.006 ↗
12. Compression properties and work-hardening behavior of Ti2AlC/TiAl composites fabricated by combustion synthesis and hot press consolidation in the Ti–Al–Nb–C system10.1016/j.matdes.2011.05.041 ↗
13. Effect of carbon addition on solidification behavior, phase evolution and creep properties of an intermetallic β-stabilized γ-TiAl based alloy10.1016/j.intermet.2013.11.011 ↗
14. The effect of heat treatments on the microstructural stability of the intermetallic Ti-46.5Al-2W-0.5Si10.1016/S0966-9795(01)00014-0 ↗
15. Creep of a beta phase-containing TiAl alloy10.1016/S0966-9795(00)00009-1 ↗
16. Room-temperature tensile properties of float-zone processed β-stabilized γ-TiAl(Nb,Cr,Zr) intermetallic10.1016/j.matlet.2016.10.103 ↗
17. Effect of aging on the tensile and creep behavior of a fully lamellar near γ-TiAl alloy10.1016/S0921-5093(01)01391-0 ↗
18. Dendrite core grain refining and interdendritic coarsening behaviour in W-containing γ-TiAl based alloys10.1016/j.jallcom.2012.10.059 ↗
19. B2 precipitates and distribution of W in a Ti–47Al–2W–0.5Si alloy10.1016/S0966-9795(02)00043-2 ↗
20. Phase stability, mechanical properties and electronic structure of TiAl alloying with W, Mo, Sc and Yb: first-principles study10.1016/j.jallcom.2015.10.270 ↗
21. Consolidation of a gamma TiAl–Mn–Mo alloy by elemental powder metallurgy10.1016/S0921-5093(97)00628-X ↗
22. Study of effect of Mn addition on the mechanical properties of Ti2AlC/TiAl composites through first principles study and experimental investigation10.1016/j.intermet.2012.03.053 ↗
23. Synthesis, microstructure and mechanical properties of (Ti1−x,Nbx)2AlC/Al2O3 solid solution composites10.1016/j.msea.2012.06.092 ↗
24. Low-temperature synthesis and characterization of Ti2AlC/TiAl in situ composites via a reaction hot-pressing process in the Ti3AlC2-Ti-Al system10.1007/s12540-015-1022-8 ↗
25. Interstitial solubility in gamma and alpha(2) phases of TiAl-based alloys10.1016/S1359-6454(96)00111-5 ↗
26. Investigation of macro/microstructure evolution and mechanical properties of directionally solidified high-Nb TiAl-based alloy10.1016/j.matdes.2015.09.116 ↗
27. Microstructure and mechanical properties of investment casted titanium matrix composites with B4C additions10.1016/j.msea.2015.01.067 ↗
28. Understanding the role of carbon atoms on microstructure and phase transformation of high Nb containing TiAl alloys10.1016/j.matchar.2016.12.008 ↗
29. Fracture behaviour of cast in-situ TiAl matrix composite reinforced with carbide particles10.1016/j.msea.2018.02.077 ↗
30. Microsegregation, macrosegregation and related phase transformations in TiAl alloys10.1016/j.intermet.2010.11.013 ↗
31. Tensile properties and fracture behavior of in-situ synthesized Ti 2 AlN/Ti48Al2Cr2Nb composites at room and elevated temperatures10.1016/j.msea.2016.09.105 ↗
32. Variations of microstructure and tensile property of gamma-TiAl alloys with 0-0.5 at% C additives10.1016/j.msea.2017.06.019 ↗
33. The impurity-drag effect in grain boundary motion10.1016/0001-6160(62)90092-5 ↗
34. Phase equilibria among α (hcp), β (bcc) and γ (L10) phases in Ti–Al base ternary alloys10.1016/S0966-9795(00)00015-7 ↗
35. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics: a review10.1016/S1005-0302(10)60064-3 ↗
36. The use of cast Ti−48Al−2Cr−2Nb in jet engines10.1007/BF02914685 ↗
37. Creep behaviors and stress regions of hybrid reinforced high temperature titanium matrix composite10.1016/j.compscitech.2009.04.009 ↗
38. Effect of carbon reactant on microstructures and mechanical properties of TiAl/Ti2AlC composites10.1016/j.msea.2016.12.069 ↗
39. Structural stability and the alloying effect of TiB polymorphs in TiAl alloys10.1016/j.intermet.2017.07.002 ↗
40. Influence of Mn addition on the microstructure and mechanical properties of a directionally solidified γ-TiAl alloy10.1016/j.matchar.2018.01.029 ↗
41. Microstructure determined fracture behavior of a high Nb containing TiAl alloy10.1016/j.msea.2016.04.074 ↗
42. Microstructure development and hardness of a powder metallurgical multi phase γ-TiAl based alloy10.1016/j.intermet.2011.11.015 ↗