Characterization of soldering alloy type Zn-In-Mg and the study of direct soldering of silicon and copper
Source abstract
Abstract
Abstract The aim of study was to characterize the Zn-In-Mg soldering alloy type and investigate the direct soldering of silicon and copper. The Zn-In-Mg solder type has a broad interval of melting, which depends on the indium content in the solder. Solder microstructure is formed of a matrix with pure Zn. The MgZn2 phases and solid solution (In) β-In are precipitated along the grain boundaries. Tensile strength attains values from 46 to 124 MPa and is dependent on indium content. The bond with silicon is formed due to the reactions of active metals - In and Mg with the substrate surface. Diffraction analysis has also revealed the In13Mg7 phase. In spite of that, the bond formation with a copper substrate in not affected by In and Mg content. The bond is formed owing to interaction between the zinc from the solder and copper substrates. Two phases, namely CuZn4 and Cu5Zn8 were observed. The shear strength of Cu/Zn-In-Mg/Cu joints attains values from 56 to 62 MPa and the shear strength of Si/Zn-In-Mg/Cu joint is within 34–42 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Effect of Au-Sn IMCs' formation and morphologies on shear properties of laser reflowed micro-solder joints10.1108/SSMT-07-2014-0016 ↗
2. Experimental investigation of Ge-doped Bi-11Ag as a new Pb-free solder alloy for power die attachment10.1007/s11664-002-0016-8 ↗
3. Microstructure, phases morphologies and hardness of a Bi-Ag eutectic alloy for high temperature soldering applications10.1016/j.matdes.2014.02.026 ↗
4. Wetting of Si-Al-O-N ceramic by Sn-5at%Ti-X ternary active solder10.1016/0921-5107(94)90199-6 ↗
5. Impact of thermal aging on the microstructure evolution and mechanical properties of lanthanum-doped tin-silver-copper lead-free solders10.1007/s11664-012-2351-8 ↗
6. Joining of zirconia to metal with Cu-Ga-Ti and Cu-Sn-Pb-Ti fillers10.1016/S0921-5093(00)00916-3 ↗
7. Research of joining graphite by use of active solder10.4028/www.scientific.net/AMR.875-877.1270 ↗
8. Active soldering of indium tin oxide (ITO) With Cu in air using an Sn3.5Ag4Ti(Ce,Ga) filler10.1361/105994903770342890 ↗
9. Microstructure, mechanical properties, and bonding mechanism of ultrasonic-assisted brazed joints of SiC ceramics with ZnAlMg filler metals in air10.1016/j.ceramint.2013.06.055 ↗
10. Building a nano-crystalline α-alumina layer at a liquid metal/sapphire interface by ultrasound10.1016/j.ultsonch.2014.05.008 ↗
11. Shear strength and wettability of active Sn3.5Ag4Ti(Ce,Ga) solder on Al2O3 ceramics10.1016/j.matdes.2011.03.022 ↗
12. Wettability and shear strength of active Sn2Ti solder on Al2O3 ceramics10.1108/09540911111169066 ↗
13. C. Peng, M. Chen, S. Liu Die bonding of silicon and other materials with active solder, in: Proceedings of the 11th International Conference on Electronic Packaging Technology & High Density Packaging, 2010, pp. 275–278, ISBN 978-1-4244–8140-8.10.1109/ICEPT.2010.5582418 ↗
14. Microstructure characterization of SnAgCu solder bearing Ce for electronic packaging10.1016/j.mee.2011.05.021 ↗
15. Bonding nature of rare-earth-containing lead-free solders10.1063/1.1435075 ↗
16. R. Koleňák, An active solder and soldering procedure: patent application No. 5011–2016, date of application submitting: April 28, 2016, In Vestník ÚPVSR 9/2016. Banská Bystrica: The Office of Industrial Property of the Slovak Republic. p. 6, 2016.
17. O.M. Baraballi, N.J.U. Kovaľ, Struktura i svojstva metalov i splavov, Kyjev Naukova Dumka, Kyjev, 1986.