journal article·2017-04

An investigation on the compressive strength enhancing mechanism of directionally solidified Ti-47Al-2Nb-2Cr-0.2Er alloy in case of cyclic loading

Qiang Wang, Hongsheng Ding, Hailong Zhang, Ruirun Chen, Jingjie Guo, Hengzhi Fu

Publisher page

Abstract

Abstract In the present study the microstructure evolutions and compressive strengths of the directionally solidified Ti-47Al-2Nb-2Cr-0.2Er alloy undergoing single and cyclic loadings are studied. It is found that bending in lamellar structure can be caused by compression and the extent of this bend exacerbates with the increase of compression strain. For the sample under cyclic-loading, the density of dislocation is improved, resulting in a higher compressive strength in comparison with the sample subjected to single loading with the same strain. Enhancements of Peierls stress, long-range elastic interactions between dislocations, and jog quantity all contribute to the higher strength of the cyclic-loading sample. Dislocation loops releasing from the semi-coherent interfaces under the applied stress are the main dislocation multiplication mechanism during the room temperature compression.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Microstructural evolution of TiAl-based alloys deformed by high-pressure torsion10.1016/j.actamat.2015.07.012 ↗
2. Mechanical properties of high niobium TiAl alloys doped with Mo and C10.1016/j.matdes.2016.03.079 ↗
3. Influence of nitrogen on the microstructure and solidification behavior of high Nb containing TiAl alloys10.1016/j.matdes.2016.04.071 ↗
4. Phase transformation behavior and kinetics of high Nb-TiAl alloy during continuous cooling10.1016/j.jallcom.2016.01.205 ↗
5. Alloy design for aircraft engines10.1038/nmat4709 ↗
6. TiAl alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
7. Phase stability, mechanical properties and electronic structure of TiAl alloying with W, Mo, Sc and Yb: first-principles study10.1016/j.jallcom.2015.10.270 ↗
8. Crystal orientation control in TiAl-Nb alloys through a double directional solidification process10.1016/j.jallcom.2015.09.226 ↗
9. Design, processing, microstructure, properties, and applications of advanced intermetallic TiAl alloys10.1002/adem.201200231 ↗
10. Application of TiAl in a turbocharger for passenger vehicles10.1002/1527-2648(200105)3:5<307::AID-ADEM307>3.0.CO;2-3 ↗
11. Modeling concepts for intermetallic titanium aluminides10.1016/j.pmatsci.2016.01.001 ↗
12. Lamellar orientation control in TiAl base alloys by a two-step compression process at high temperature10.1016/j.msea.2008.12.027 ↗
13. Huang · 1993
14. Ordered intermetallic alloys, part III: gamma titanium aluminides10.1007/BF03220745 ↗
15. General aspects of the thermo-mechanical10.1007/BF02657854 ↗
16. Lanthanum hexaboride as advanced structural refiner/getter in TiAl-based refractory intermetallics10.1016/j.jallcom.2013.11.017 ↗
17. Intermetallics: why is it so difficult to introduce them in gas turbine engines?10.1016/j.intermet.2006.01.064 ↗
18. Microstructure and compressive properties of directionally solidified Er-bearing TiAl alloy using cold crucible10.1016/j.matdes.2016.03.042 ↗
19. Deformation mechanisms in micron-sized PST TiAl compression samples: experiment and model10.1016/j.actamat.2011.02.016 ↗
20. The role of the α2 phase in the transmission of slip in lamellar TiAl-based alloys10.1080/01418619808223753 ↗
21. Crystal orientation control in TiAl-Nb alloys through a double directional solidification process10.1016/j.jallcom.2015.09.226 ↗
22. Effect of growth rate on microstructure and tensile properties of Ti-45Al-2Cr-2Nb prepared by electromagnetic cold crucible10.1016/j.matdes.2015.07.122 ↗
23. Effect of power on microstructure and mechanical properties of Ti44Al6Nb1.0Cr2.0V0.15Y0.1B alloy prepared by cold crucible directional solidification10.1016/j.matdes.2014.12.006 ↗
24. Directional solidification of titanium alloys by electromagnetic confinement in cold crucible10.1016/j.matlet.2004.11.053 ↗
25. The role of ordered domains and slip mode of α2 phase in the plastic behaviour of TiAl crystals containing oriented lamellae10.1016/0956-7151(93)90163-M ↗
26. The influence of second phase Ti3Al on the deformation mechanisms in TiAl10.1080/09500838908206358 ↗
27. Deformation behavior of α2-lamellae in fully lamellar Ti-48Al-2Mn-2Nb at room temperature10.1016/S1359-6462(97)00538-1 ↗
28. The activation and the spreading of deformation in a fully lamellar Ti-47at% Al-1at% Cr-0.2at% Si alloy10.1080/14786430600606826 ↗
29. Microstructural control and mechanical properties of Ti–47Al–2Cr–2Nb alloy by directional solidification electromagnetic cold crucible technique10.1016/j.matdes.2012.02.057 ↗
30. Microstructure control of TiAl alloys containing β stabilizers by directional solidification10.1016/S0921-5093(01)01494-0 ↗
31. An investigation on the mechanical properties changing mechanism of high speed steel by pulsed magnetic treatment10.1016/j.msea.2014.04.100 ↗
32. Microstructure-properties relationship in a one-step quenched and partitioned steel10.1016/j.msea.2013.09.063 ↗
33. Estimation of lattice strain in nanocrystalline silver from X-ray diffraction line broadening10.1007/s10853-007-2300-8 ↗
34. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray Debye-Scherrer spectrum10.1080/14786435608238074 ↗
35. Effect of strain rate on the compression behavior of TiAl and TiAl-2Mn alloys fabricated by combustion synthesis and hot press consolidation10.1016/j.intermet.2013.07.003 ↗
36. Measurement of the effective activation volume in 45XD titanium aluminides by repeated transient tests10.1016/j.msea.2007.10.029 ↗
37. In situ straining investigation of slip transfer across α2 lamellae at room temperature in a lamellar TiAl alloy10.1080/09500830500497066 ↗
38. Deformation process related to the interfacial boundaries in two-phase γ-titanium aluminides10.1016/0956-7151(93)90191-T ↗
39. Deformation behaviour and 6H-LPSO structure formation at nanoindentation in lamellar high Nb containing TiAl alloy10.1080/09500839.2015.1009515 ↗
40. Slip transfer across hetero-interfaces in two-phase titanium aluminum intermetallics10.1007/s11661-010-0332-1 ↗
41. Deformation mechanisms in TiAl intermetallics—experiments and modeling10.1016/S0749-6419(01)00036-5 ↗
42. Microstructure development during directional solidification of Ti-45Al-8Nb alloy10.1016/j.jallcom.2010.06.151 ↗
43. A newly developed hot worked TiAl alloy for blades and structural components10.1016/S1359-6462(02)00158-6 ↗
44. Microstructure evolution, hot deformation behavior and mechanical properties of Ti-43Al-6Nb-1B alloy10.1016/j.intermet.2012.07.016 ↗
45. Micro segregation in high Nb containing TiAl alloy ingots beyond laboratory scale10.1016/j.intermet.2006.10.003 ↗
46. Polysynthetic twinned TiAl single crystals for high-temperature applications10.1038/nmat4677 ↗
47. The science, technology, and implementation of TiAl alloys in commercial aircraft engines10.1557/opl.2013.44 ↗
48. Work hardening in heterogeneous alloy – a microstructural approach based on three internal state variables10.1016/S1359-6454(00)00289-5 ↗
49. Dislocations in a simple cubic lattice10.1088/0959-5309/59/2/309 ↗
50. A microphysical model of Harper-Dorn creep10.1016/1359-6454(95)00281-2 ↗
51. The Peierls stress of dislocations: an analytic formula10.1103/PhysRevLett.78.266 ↗
52. Hull · 2011
53. Coherency stresses and interface-related deformation phenomena in two-phase titanium aluminides10.1016/S0966-9795(99)00030-8 ↗
54. Shear boundaries in lamellar TiAl10.1080/09500839208229275 ↗
55. TEM investigation on the interfacial boundaries in as-cast Ti3Al+TiAl alloy10.1016/0956-7151(91)90003-J ↗
56. Appel · 2011