Investigation of stress corrosion susceptibility of duplex (α + γ) stainless steel in a hot chloride solution
Source abstract
Abstract
The stress corrosion susceptibility of 25Cr–6Ni–3Mo duplex stainless steel (alloy 255, UNS S32550) in boiling 35% MgCl 2 solution has been examined in terms of the relationship between the critical cracking potential E cc for duplex stainless steel. Mill-annealed alloy 255 loaded to 90% of the yield strength in a boiling MgCl 2 solution is immune to stress corrosion cracking (SCC) at the open circuit corrosion potential ( E cc = − 470 mV vs. standard colomel electrode (SCE)); however, the susceptibility is induced by anodic polarization, exhibiting a critical potential ( E cc = − 335 mV vs. SCE) that is 135 mV more positive than the corrosion potential. A small amount of cold work significantly increases the susceptibility to SCC by shifting E cc in the negative direction without any effect on E oc . E cc for mill-annealed alloy 255 is shown to be a potential for crack initiation and varies from −335 to −380 mV vs. SCE, depending on the microstructural and loading conditions. For alloy 255, the minimum potential for crack propagation is constant at −380 mV, irrespective of any cold work and the loading mode. The potential (−380 mV) is indeed a critical potential, capable of passivating growing cracks completely, and is found to correspond to the repassivation potential for growing pits that is determined from the cyclic polarization curve measured at a slow scan rate in the unstressed state.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Streicher · Met. Prog. · 1985 · 128 · 29
2. Redmond · Chem. Eng. · 1986 · 27 · 153
3. Sridhar · 1983 · 481
4. Nielsen · Corrosion · 1964 · 20 · 10510.5006/0010-9312-20.3.104t ↗
5. Shimodaira · 1977 · 1003
6. Uhlig · 1977 · 174
7. Mohr · Corrosion · 1981 · 37 · 19910.5006/1.3577271 ↗
8. Vacarro · Corrosion · 1982 · 38 · 54910.5006/1.3593858 ↗
9. Locci · Corrosion · 1987 · 43 · 46510.5006/1.3583886 ↗
10. Kwon · Corrosion · 1992 · 48 · 83810.5006/1.3315883 ↗
11. Smialowski · Corrosion · 1967 · 23 · 21810.5006/0010-9312-23.7.218 ↗
12. Sridhar · Corrosion · 1987 · 43 · 64610.5006/1.3583843 ↗
13. Marek · Corrosion · 1970 · 26 · 510.5006/0010-9312-26.1.5 ↗
14. Scully · Corrosion Sci. · 1980 · 26 · 99710.1016/0010-938X(80)90080-3 ↗
15. Staehle · 1977 · 180
16. Uhlig · J. Electrochem. Soc. · 1969 · 116 · 17310.1149/1.2411789 ↗
17. Jones · Corrosion Sci. · 1978 · 18 · 63110.1016/0010-938X(78)90056-2 ↗
18. Tsujikawa · 1985 · 35
19. Suzuki · Corrosion · 1972 · 28 · 110.5006/0010-9312-28.1.1 ↗
20. Shamakian · 1979 · 116
21. Tamaki · 1990 · 207