Endurance limit of pulsed laser hardened component-like specimens—Experiment and simulation
Source abstract
Abstract
The pulsed laser hardening with low-pulse frequencies enables a higher hardening depth compared with continuous wave laser hardening. To avoid melting a special pulse-to-pulse temperature control was developed. The temperature during hardening was calculated. Residual stresses after hardening were measured and simulated. Studies of the fatigue strength showed that pulsed laser hardening enables an increase of the fatigue strength of component-like specimens. The endurance limit was simulated with the weakest-link model on the base of hardness, roughness, and residual stresses. The weakest-link model also predicts crack initiation sites which were compared with the observed ones. The described calculations of the residual stresses and the endurance limit are applicable on variable geometries of components. So, in the field of development and construction it is possible to reduce the development cycles.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Messer · HTM—Härterei-Technische Mitteilungen · 1997 · 52 · 74
2. T.S. Do, Beitrag zur Prozesssimulation und Online-Prozesskontrolle der Temperatur auf der Bauteiloberfläche für das CO2-Laserstrahlhärten, Dissertation, TU Ilmenau, 1998.
3. Bonss · Proc. SPIE Int. Soc. Opt. Eng. · 2003 · 4831 · 53
4. Hosenfeldt · HTM—Härterei-Technische Mitteilungen · 2000 · 55 · 361
5. Hoffmann · Proc. Int. WLT-Conf. Lasers Manuf., LIM · 2003 · 2 · 23
6. Bachmann · HTM—Härterei-Technische Mitteilungen · 2004 · 59 · 21710.3139/105.100292 ↗
7. Pantsar · J. Laser Appl. · 2004 · 16 · 14710.2351/1.1710879 ↗
8. Wu · Steel Grips · 2004 · 2 · 140
9. B. Schürmann, Umwandlungshärten mit Dioden-Laserstrahlung in Mehrstrahltechnik, Dissertation, RWTH Aachen, 2000.
10. Heidkamp · Surf. Coat. Technol. · 2004 · 188/189 · 29410.1016/j.surfcoat.2004.08.047 ↗
11. Pertek · Inz. Mater. · 2003 · 24 · 539
12. G. Habedank, Neuartige Bearbeitungsverfahren zur Modifizierung senkerodierter Randschichten, Dissertation, University of Magdeburg, Shaker Verlag, Aachen, 2005.
13. Belló · J. Mater. Sci. · 1994 · 29 · 521310.1007/BF01151119 ↗
14. Chabrol · 1986 · 435
15. Meijer · Ann. CIRP · 1991 · 40 · 18310.1016/S0007-8506(07)61963-5 ↗
16. J. Domes Die Ausbildung von Makroeigenspannungen beim Laserstrahlrandschichthärten und anderen Verfahren der Lasermaterialbearbeitung, Dissertation, University of Erlangen-Nürnberg, 1995.
17. Müller · HTM—Härterei-Technische Mitteilungen · 1996 · 51 · 19
18. Velikih · Met. Sci. Heat Treat. · 1985 · 27 · 25810.1007/BF00652088 ↗
19. T. Hosenfeldt, Schwingfestigkeit des Stahls 42CrMo4 nach partieller Härtung mit gepulster Nd:YAG-Laserstrahlung, Dissertation, University of Bremen, Shaker Verlag, 2000.10.1515/htm-1999-540516 ↗
20. K. Obergfell, Charakterisierung der Mikrostruktur ausgewählter Stähle nach gepulsten Laserrandschichthärtungen, Dissertation, University of Karlsruhe, 2000.
21. Yilbas · Lasers Eng. · 2004 · 14 · 213
22. Schütz · Zeitschrift für Flugwissenschaften · 1967 · 15 · 407
23. Wohlfahrt · 1978
24. Lehr · Z. Metallkunde · 1928 · 20 · 78
25. Winderlich · HTM—Härterei-Technische Mitteilungen · 1988 · 43 · 229
26. Shur · Met. Sci. Heat Treat. · 1982 · 25 · 34110.1007/BF00782808 ↗
27. Singh · Met. Trans. A · 1981 · 12A · 13810.1007/BF02648519 ↗
28. R. Lin, On residual stresses and fatigue of laser hardened steels, Doctoral thesis, University of Linköping, 1992.10.4028/www.scientific.net/MSF.102-104.409 ↗
29. de la Cruz · Int. J. Fatigue · 1998 · 20 · 38910.1016/S0142-1123(98)00010-3 ↗
30. Cerny · J. Mater. Eng. Perform. · 1998 · 7 · 36110.1361/105994998770347800 ↗
31. Hosenfeldt · HTM—Härterei-Technische Mitteilungen · 1999 · 54 · 316
32. Merrien · Surf. Eng. · 1992 · 8 · 6110.1179/sur.1992.8.1.61 ↗
33. Lin · 1992 · 409
34. Liu · Materialwissenschaft und Werkstofftechnik · 1991 · 22 · 18710.1002/mawe.19910220602 ↗
35. Böhm · Zeitschrift fürWerkstofftechnik · 1982 · 13 · 12010.1002/mawe.19820130408 ↗
36. Heckel · Zeitschrift für Werkstofftechnik · 1975 · 6 · 5210.1002/mawe.19750060204 ↗
37. Krä · Materialwissenschaft und Werkstofftechnik · 1989 · 20 · 25510.1002/mawe.19890200803 ↗
38. S. Schnack, Berechnung der Dauerfestigkeit und der Rissausgangsorte gepulst laserstrahlgehärteter Proben aus den Stählen 42CrMo4 und 100Cr6, Dissertation, University of Bremen, Shaker Verlag, Aachen, 2003.
39. Jablonski · 2001
40. Bomas · HTM—Härterei-Technische Mitteilungen · 2005 · 60 · 33110.3139/105.100357 ↗
41. Dang Van · 1989 · 479
42. Murakami · Fatigue Fracture Eng. Mater. Struct. · 1998 · 21 · 147310.1046/j.1460-2695.1998.00128.x ↗
43. Hänel · 2002
44. Laue · HTM—Härterei-Technische Mitteilungen · 2004 · 58 · 19910.3139/105.100290 ↗
45. Macherauch · Z. für angewandte Physik · 1961 · 13 · 305