journal article·2018-04

Effect of annealing treatment on the microstructure and mechanical properties of hot compression Au80Sn20 alloy

Yufeng Huang, Wensheng Liu, Yunzhu Ma, Siwei Tang, Baishan Chen

Publisher page

Abstract

Abstract Intrinsic fragility is the major bottleneck for expanding the application of the Au80Sn20 eutectic solder. Motivated by eliminating the deformation defects and internal stress, the microstructural evolution and mechanical properties have been studied in a hot compression Au80Sn20 alloy annealed at different temperatures and times. Results show that after annealing treatment, the microstructures of the Au80Sn20 develop from lamellar to equiaxed grains. All the diffraction peaks positions of Au80Sn20 alloy have a right shift revealing an elimination of the deforming residual stress and show a certain degree preferred orientation of (100) AuSn and (012) Au5Sn planes. The indentation depths have a sharp increase at the same load pressure after annealing, meanwhile the hardness and modulus of Au80Sn20 alloy drop evidently. Combining the result of microstructure and mechanical properties evolution, the Au80Sn20 alloy is optimized annealed at 260 °C for 5 h. The stamping performance of Au80Sn20 alloy foil has been significantly improved after annealing and no tearing phenomenon occurs. Our finding not only sheds light on future research on deformation mechanism of fragile metals but also provides practical guidance to the engineers in solder manufacture.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Additive Manufacturing Materials and Processes · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Effect of Au-Sn IMCs' formation and morphologies on shear properties of laser reflowed micro-solder joints10.1108/SSMT-07-2014-0016 ↗
2. Mechanical reliability of Sn-rich Au–Sn/Ni flip chip solder joints fabricated by sequential electroplating method10.1016/j.microrel.2008.09.008 ↗
3. Microstructural characterization and mechanical performance of wafer-level SLID bonded Au-Sn and Cu-Sn seal rings for MEMS encapsulation10.1007/s11664-015-3929-8 ↗
4. Power electronic assemblies: thermo-mechanical degradations of gold-tin solder for attaching devices10.1016/j.microrel.2016.07.028 ↗
5. Continuous strip casting, microstructure and properties of Au-Sn soldering alloy10.1007/s12540-011-0202-4 ↗
6. Evolution of primary phases and high-temperature compressive behaviors of as-cast AuSn20 alloys prepared by different solidification pathways10.1007/s13404-011-0004-y ↗
7. Interfacial microstructure evolution and shear behavior of Au-20Sn/(Sn)Cu solder joints bonded at 250 °C10.1016/j.msea.2015.11.025 ↗
8. Microstructural evolution of the Au-20 wt% Sn solder on the Cu substrate during reflow10.1016/j.jallcom.2009.06.018 ↗
9. A novel interface strengthening layer: nanoscale AuCu super-structure formed during Au80Sn20/Cu rapid solidification soldering process10.1016/j.matchar.2017.11.043 ↗
10. Microstructural evolution and mechanical properties in (AuSn)eut-Cu interconnections10.1007/s11664-016-4733-9 ↗
11. Au-Sn bonding material for the assembly of power integrated circuit module10.1016/j.jallcom.2016.02.065 ↗
12. Interfacial reactions in the Au/Sn- x Zn/Cu sandwich couples10.1016/j.jallcom.2017.03.285 ↗
13. First principles study of Au-Sn intermetallic compounds10.7498/aps.62.247102 ↗
14. Damping capacity of pre-compressed magnesium alloys after annealing10.1016/j.msea.2017.09.096 ↗
15. On hardening and yield surface motion in plasticity10.1007/BF01181054 ↗
16. Effect of annealing treatment on the microstructure and mechanical properties of a duplex Zr-2.5Nb alloy10.1016/j.msea.2017.08.107 ↗
17. Effect of annealing treatment on the microstructure and mechanical properties of ultrafine-grained aluminum10.1016/j.matdes.2013.06.075 ↗
18. Damping capacity of pre-compressed magnesium alloys after annealing10.1016/j.msea.2017.09.096 ↗
19. Effects of cooling rate and magnetic field on solidification characteristics of Au80Sn20 eutectic solder10.1007/s10854-017-7932-0 ↗
20. Continuous distribution of dislocations and the mathematical theory of plasticity (II)10.1002/pssb.2220100205 ↗
21. Effects of high-temperature annealing on microstructure and mechanical property of SiO2f /SiO2 composites10.1016/j.vacuum.2017.07.005 ↗
22. On plasticity and fracture of nano structured Cu/X (X =Au, Cr) multilayers: the effects of length scale and interface/boundary10.1016/j.actamat.2010.03.042 ↗
23. Length-scale-dependent deformation and fracture behavior of Cu/X (X = Nb, Zr) multilayers: the constraining effects of the ductile phase on the brittle phase10.1016/j.actamat.2011.08.016 ↗
24. On dislocation storage and the mechanical response of fine scale microstructures10.1016/0956-7151(94)90030-2 ↗
25. Microstructure evolution and enhanced performance of a novel Nb-Mo microalloyed medium Mn alloy fabricated by low-temperature rolling and warm stamping10.1016/j.matdes.2017.08.047 ↗