Low formability and reduction of area in twinning-induced plasticity steels despite their excellent tensile elongation
Source abstract
Abstract
Abstract The mechanism for low formability and reduction of area (RA) in twinning-induced plasticity (TWIP) steels despite their excellent tensile elongation has been investigated in an attempt to understand and increase their formability. In metals, RA is strongly dependent on the post-necking elongation (PE) rather than uniform elongation (UE); in this study, UE and PE had 9% and 91% contributions to RA, respectively. Between the two representative ductility indicators in tensile tests, the RA is typically higher than the total elongation (TE) in conventional metals. However, the RA of TWIP steels was lower than the TE because TWIP steels had a higher UE and lower PE. This was attributed to the higher strain hardening exponent (n) and lower strain rate sensitivity (m) of TWIP steels. This indicates that TWIP steels have a higher resistance to fracture by the strain gradient, but a lower resistance to fracture by the strain rate gradient. In this study, the small and/or negative m value of TWIP steels reduced the RA value and formability in spite of their higher elongation. The negative m value led to a strain concentration at the necking region, leading to localized necking without diffuse necking followed by shear cracks, resulting in the lower RA and formability. Consequently, it is necessary to increase the m value of TWIP steels in order to increase the formability.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (63)
Show source-provided references
1. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
2. High strength Fe-Mn-(Al, Si) TRIP/TWIP steels development-properties-application10.1016/S0749-6419(00)00015-2 ↗
3. Mechanism of work hardening in Hadfield manganese steel10.1007/BF02648339 ↗
4. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
5. A general perspective of Fe–Mn–Al–C steels10.1007/s10853-018-2551-6 ↗
6. Microstructural evolution and deformation behavior of twinning-induced plasticity (TWIP) steel during wire drawing10.1016/j.msea.2015.07.034 ↗
7. Effects fo Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
8. Effects of aluminum addition on tensile and cup forming properties of three Twinning Iduced Plasticity steels10.1007/s11661-011-1007-2 ↗
9. Dynamic strain aging of twinning-induced plasticity (TWIP) steel in tensile testing and deep drawing10.1016/j.msea.2015.03.008 ↗
10. Stretch-flangeability of high Mn TWIP steel10.1002/srin.201000044 ↗
11. Formability of TWIP (twinning induced plasticity) automotive steels10.1016/j.ijplas.2010.03.006 ↗
12. Effect of copper and aluminum contents on wire drawing behavior in twinning-induced plasticity steels10.1016/j.msea.2018.09.049 ↗
13. Damage observation in a high-manganese austenitic TWIP steel by synchrotron radiation computed tomography10.1016/j.scriptamat.2010.08.042 ↗
14. Damage evolution in TWIP and standard austenitic steel by means of 3D X ray tomography10.1016/j.msea.2013.05.013 ↗
15. The premature necking of twinning-induced plasticity steels10.1016/j.actamat.2017.06.042 ↗
16. In situ observations of transgranular crack propagation in high-manganese steel10.1016/j.scriptamat.2014.12.005 ↗
17. Cracking in a Fe-25Mn-3Si-3Al steel10.1080/21663831.2014.915433 ↗
18. The effect of deformation twins on the quasi-cleavage crack propagation in twinning-induced plasticity steels10.1016/j.actamat.2018.03.004 ↗
19. Tensile fracture modes in Fe-22Mn-0.6C and Fe-30Mn-3Si-3Al twinning-induced plasticity (TWIP) steels10.1007/s11661-017-4263-y ↗
20. Post-uniform elongation and tensile fracture mechanisms of Fe-18Mn-0.6C-xAl twinning-induced plasticity steels10.1016/j.actamat.2017.04.011 ↗
21. Room-temperature blue brittleness of Fe-Mn-C austenitic steels10.1016/j.scriptamat.2017.07.017 ↗
22. Effects of diameter and preparation of round shaped tensile specimen on mechanical properties10.1016/j.msea.2019.138119 ↗
23. Effect of Al on microstructure and tensile properties of C-bearing high Mn TWIP steel10.1016/j.actamat.2011.12.004 ↗
24. The microstructure dependence of drawability in ferritic, pearlitic and TWIP steels during wire drawing10.1007/s10853-019-03499-4 ↗
25. Deformation behaviors of various Fe–Mn–C twinning-induced plasticity steels: effect of stacking fault energy and chemical composition10.1007/s10853-019-04018-1 ↗
26. Estimations of the true stress and true strain until just before fracture by the stepwise tensile test and bridgman equation for various metals and alloys10.2320/matertrans.MD201112 ↗
27. Derivation and variation in composition-dependent stacking fault energy maps based on subregular solution model in high-manganese steels10.1007/s11661-009-0050-8 ↗
28. Influence of addition elements on the stacking-fault energy and mechanical properties of an austenite Fe-Mn-C steel10.1016/j.msea.2006.12.170 ↗
29. Stacking fault energy and deformation mechanisms in Fe-xMn-0.6C-yAl TWIP steel10.1016/j.msea.2016.08.106 ↗
30. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys10.1016/j.msea.2004.01.059 ↗
31. Texture evolution of cold rolled and annealed Fe-24Mn-3Al-2Si-1Ni-0.06C TWIP steel10.1016/j.msea.2011.02.055 ↗
32. Texture, misorientation and mechanical anisotropy in a deformed dual phase stainless steel weld joint10.1016/j.msea.2013.03.018 ↗
33. Quasi-static and dynamic deformation mechanisms interpreted by microstructural evolution in TWinning Induced Plasticity (TWIP) steel10.1016/j.msea.2016.12.037 ↗
34. Drawing direction effect on microstructure and mechanical properties of twinning-induced plasticity steel during wire drawing10.1007/s11665-019-04020-3 ↗
35. Hosford · 2007
36. Effect of stress states on the twinning behavior in twinning-induced plasticity steel10.1007/s11665-019-04254-1 ↗
37. Non-linear correlation between uniaxial tensile properties and shear-edge hole expansion ratio10.1007/s11665-014-1161-y ↗
38. The influence of strain hardening and strain-rate sensitivity on sheet metal forming10.1115/1.3443530 ↗
39. Post-uniform deformation in uniaxial and equi-biaxial stretching of aluminium alloy sheets10.1016/S0924-0136(97)00042-3 ↗
40. Deformation behaviors of flat rolled wire in twinning-induced plasticity steel
41. Tensile deformation behavior of aluminum alloys at warm forming temperatures10.1016/S0921-5093(02)00915-2 ↗
42. A numerical analysis of the tensile test for sheet metals10.1007/BF02643836 ↗
43. The effect of strain-rate sensitivity on formability of AA 5754-O at cold and warm temperatures10.1007/s11665-010-9652-y ↗
44. Effect of strain hardening capability on plastic deformation behaviors of material during metal forming10.1016/j.matdes.2013.08.101 ↗
45. Mechanism of macroscopic shear band formation in plane strain compressed fine-grained aluminium10.1016/j.msea.2015.06.056 ↗
46. The occurrence of shear bands in isothermal, hot forging10.1007/BF02643318 ↗
47. Revealing the fracture mechanism of twinning‐induced plasticity steels10.1002/srin.201700433 ↗
48. Effect of strain rate on tensile and serration behaviors of an austenitic Fe-22Mn-0.7C twinning-induced plasticity steel10.1016/j.msea.2017.10.074 ↗
49. Softening behavior by excessive twinning and adiabatic heating at high strain rate in a Fe-20Mn-0.6C TWIP steel10.1016/j.actamat.2015.09.061 ↗
50. Strain rate effects on tensile deformation behaviors for Fe-22Mn-0.6C-(1.5Al) twinning-induced plasticity steel10.1016/j.msea.2014.04.043 ↗
51. Strain rate sensitivity of C‐alloyed, high‐Mn, twinning‐induced plasticity steel
52. Dependence of tensile deformation behavior of TWIP steels on stacking fault energy, temperature and strain rate10.1016/j.actamat.2010.05.049 ↗
53. Different strain rate sensitivities between Fe–22Mn–0.6C and Fe–30Mn–3Si–3Al twinning-induced plasticity steels10.1016/j.msea.2016.01.003 ↗
54. Improving the formability of low carbon sheet steel by control of interstitial carbon content and temperature10.1007/BF02655108 ↗
55. Strain-rate sensitivity and effects of strain rate in sheet forming10.1179/030716980803287297 ↗
56. Plastic instabilities and uniaxial tensile ductilities10.1016/0001-6160(80)90144-3 ↗
57. The effect of strain rate sensitivity on theoretical prediction of limiting draw ratio for cylindrical cup drawing process10.1016/j.matdes.2006.05.014 ↗
58. The effects of temperature and forming speed on the forming limit diagram for type 5083 aluminum–magnesium alloy sheet10.1016/S0924-0136(01)00650-1 ↗
59. Enhanced ductility in coarse-grained Al-Mg alloys10.1007/BF02648411 ↗
60. On certain aspects of strain rate sensitivity of sheet metals10.1007/BF02649070 ↗
61. Strain hardening rate sensitivity and strain rate sensitivity in TWIP steels10.1016/j.msea.2015.01.080 ↗
62. Operant strain-rate sensitivity during tensile necking10.1007/BF02663315 ↗
63. Strain localization in the diffuse neck in sheet metal10.1007/BF02646332 ↗