Abstract

Abstract Ti-Ni-Si compound was used to join carbon/carbon (C/C) composites by hot-pressing sintering. Effects of high temperature treatment and thermal shock on the bonding strength of Ti-Ni-Si joints were investigated. After the joints were treated for 10 h at 1000 °C, the average shear strength was increased to 30.89±0.75 MPa, which was 30.01% higher than the original ones, accompanied by homogeneous Ti-Ni-Si interlayer with few defects. Fracture toughness of the joints after thermal treated for 5 h possessed significant improvement from 1.44±0.32 to 4.10±0.56 MPa m 1/2 attributing to the decrease of free Si and the increase of ternary compound Ti 4 Si 7 Ni 4 in the interlayer. After heat treatment at 1000 °C for 5 h and thermal shock between 1000 °C and room temperature for 30 times, the average shear strength of those joints increased from 23.76±0.50 to more than 30 MPa. The improvement of the mechanical strength of Ti-Ni-Si joints was attributed to the multi-component diffusion reactions to seal the defects in the Ti-Ni-Si joints during heat treatment and thermal cycling tests. This work could provide new insight to understand strengthening of the bonding between C/C composites instead of weakening after the joints experiencing thermal shock.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Krenkel · 2008
2. Behavior of three-dimensional woven carbon composites in single – bolt bearing10.1016/j.compstruct.2015.03.022 ↗
3. Silicon carbide composites as fusion power reactor structural materials10.1016/j.jnucmat.2011.03.005 ↗
4. Failure of carbon composite-to-aluminum joints with combined mechanical fastening and adhesive bonding10.1016/j.compstruct.2006.04.013 ↗
5. Synthesis of a novel preceramic polymer (V-PMS) and its performance in heat-resistant organic adhesives for joining SiC ceramic10.1016/j.jeurceramsoc.2012.03.032 ↗
6. Fatigue life of a carbon fiber composite T-joint under a standard fighter aircraft spectrum load sequence10.1016/j.compstruct.2015.03.026 ↗
7. Strength of single-lap-joint assemblies of continuous unidirectional carbon fibre-reinforced thermoplastic matrix tapes under tensile loading10.1177/0021998314541308 ↗
8. Experimental study of silicone-epoxy dual adhesive joints for high temperature aerospace applications10.1002/mawe.201100809 ↗
9. A SiC whisker reinforced high-temperature resistant phosphate adhesive for bonding carbon/carbon composites10.1016/j.jallcom.2015.02.017 ↗
10. A user-friendly heat-resistant modified polymer-based adhesive for joining and repair of carbon/carbon composites10.1016/j.matdes.2015.07.178 ↗
11. A. Todt, K. Roder, D. Nestler, B. Wielage, Joining of glassy carbon with a C/C-SiC composite by brazing for an innovative high temperature sensor, in: L. Zhang and D. Jiang (eds), High Temperature Ceramic Matrix Composites 8: Ceramic Transaction, 248, 2014, pp. 661–667. http://dx.doi.org/10.1002/9781118932995.ch75.10.1002/9781118932995.ch75 ↗
12. Proposal for a modified non-active brazing alloy for joining CFC composites to copper10.1016/j.compositesb.2013.08.079 ↗
13. A new partial transient liquid-phase bonding process with powder-mixture interlayer for bonding Cf/SiC composite and Ti–6Al–4V alloy10.1016/j.matlet.2014.12.110 ↗
14. Effect of bonding temperature on the microstructure and strength of C/C composite/GH3044 alloy joints partial transient liquid phase (PTLP) bonded with multiple interlayers10.1007/s40195-014-0090-y ↗
15. The preparation and mechanical properties of carbon/carbon composite joints using Ti-Si-SiC-C filler as interlayer10.1016/j.msea.2013.03.007 ↗
16. Silicon carbide diffusion bonding by spark plasma sintering10.1080/10426914.2014.952019 ↗
17. Joining of C/SiC composites by spark plasma sintering technique10.1016/j.jeurceramsoc.2013.10.028 ↗
18. Pre-oxidation of carbon/carbon composites to improve the bonding strength of Ti-Ni-Si joints10.1016/j.msea.2014.09.107 ↗
19. Effect of SiC nanowires on the thermal shock resistance of joint between carbon/carbon composites and Li2O–Al2O3–SiO2 glass ceramics10.1016/j.jeurceramsoc.2014.03.011 ↗
20. Thermal shock resistance of SiC/MAS–LAS multilayer joint of carbon/carbon composites to LAS glass-ceramic10.1016/j.msea.2012.07.034 ↗
21. The study on joining carbon/carbon composites using Ti-Ni-Si compound10.1016/j.msea.2012.03.059 ↗
22. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
23. Microstructure and mechanical properties of spark plasma sintered zirconia-hydroxyapatite nano-composite powders10.1016/j.actamat.2005.01.039 ↗
24. The additivity of the energies of normal covalent bonds10.1073/pnas.18.6.414 ↗
25. A thermodynamic evaluation of the nickel-silicon system10.1007/BF02663838 ↗
26. A multi-interlayer LMAS joint of C/C-SiC composites and LAS glass ceramics10.1016/j.jmst.2014.11.024 ↗
27. Thermal oxidation of the silicides CoSi2, CrSi2, NiSi2, PtSi, TiSi2 and ZrSi210.1016/0040-6090(85)90142-7 ↗
28. Thermal stability of NiSi2 on high-dose ion-implanted (001) Si10.1063/1.351350 ↗
29. V and E phases in ternary systems with transition metals and silicon or germanium