Abstract

Stress corrosion cracking (SCC) is an important failure mechanism for oil and gas pipelines. In the past, hydrostatic testing has been frequently used to assess and mitigate stress corrosion cracking. It is commonly agreed that an effective hydrostatic test not only eliminates critical crack-like flaws, but also blunts the sub-critical crack tip thereby suppressing further SCC propagation. However, little study has been done on the plastic deformation that results from the high stress intensity at the crack tip due to hydrostatic testing pressure and its possible role in subsequent SCC propagation. In this study, microstructural details were examined of an API 5L X52 SCC-containing pipe removed from field service. Plastic deformation generated by the hydrostatic testing pressure was revealed by using high-resolution imaging of a focused ion beam (FIB) microscope. The existence of the microscopic plastic zones around some crack tips suggests that caution should be taken when setting up pipeline hydrostatic tests.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Office of Pipeline Safety · 2003
2. Leis · 2004
3. Wood · Pipes Pipelines Int. · 2000 · 45 · 1
4. Zheng · 1998 · 459
5. Kiefner · 2000
6. Brooks · ASME · 1968
7. W. Zheng, R. Sutherby, R. W. Revie, W. R. Tyson, G. Shen, Corrosioneering J., http://www.corrosionsource.com/corrosioneering, 1998.
8. Phaneuf · Microsc. Microanal. · 2006 · 12 · 125810.1017/S1431927606066165 ↗
9. Li · CMQ · 2005 · 44 · 33110.1179/cmq.2005.44.3.331 ↗
10. Li · Corrosion · 2006 · 62 · 31610.5006/1.3280664 ↗
11. Li · 2001 · 26
12. Li · 1998
13. Jian Li · Microsc. Microanal. · 2006 · 12 · 130810.1017/S1431927606065482 ↗
14. Li · J. Metal · 2006 · 58 · 27
15. Lehockey · 2000 · 247
16. Glez · J. Appl. Crystallogr. · 2001 · 34 · 28010.1107/S0021889801003077 ↗
17. Kamaya · Acta Mater. · 2006 · 54 · 53910.1016/j.actamat.2005.08.046 ↗
18. Li · Mater. Sci. Eng. A · 2006 · 421 · 31710.1016/j.msea.2006.01.084 ↗
19. Patterson · Microsc. Microanal. · 2002 · 8 · 56610.1017/S1431927602105502 ↗
20. Phaneuf · Proc. Microsc. Microanal. · 1998 · 4 · 49210.1017/S1431927600022583 ↗
21. Su · Microsc. Microanal. · 2002 · 8 · 548
22. Wang · Fatigue Fract. Eng. Mater. Struct. · 1999 · 22 · 25110.1046/j.1460-2695.1999.00159.x ↗
23. Li · J. Mater. Charact. · 2006 · 57 · 6410.1016/j.matchar.2005.12.007 ↗
24. Giannuzzi · Micron · 1999 · 30 · 19710.1016/S0968-4328(99)00005-0 ↗
25. Irwin · 1961
26. Anderson · 1995
27. Alexandreanu · Scripta Mater. · 2006 · vol.54 · 104710.1016/j.scriptamat.2005.11.051 ↗
28. Garcia · Corros. Sci. · 2001 · 43 · 151910.1016/S0010-938X(00)00165-7 ↗