Effect of service exposure on the mechanical properties of 2.25Cr–1Mo pressure vessel steel in a hot-wall hydrofining reactor
Source abstract
Abstract
Abstract Life assessment for hydrocarbon processing plant components is important for both service life extension and also to minimize the potential for premature catastrophic failure. In this paper, the degradation of 2.25Cr–1Mo pressure vessel steel in a hot-wall hydrofining reactor is investigated. A test block containing a weld is exposed to the chemical service environment present within a reactor. After removal from the reactor, chemical composition, tensile behavior, impact performance are quantified and the microstructure characterized using scanning electron microscopy (SEM). Results from the tensile tests indicate that the irradiated weld and base material had similar stress–strain response. Results from the Charpy V-Notch (CVN) impact tests demonstrated that the toughness of both the base material and weld were degraded with the degradation and embrittlement of the weld zone being significantly higher than the base material. Through careful processing of additional samples extracted from the test block, using (a) de-hydrogen treatment to remove the hydrogen, (b) hydrogen charging to enrich the hydrogen content to saturated condition and (c) de-brittleness treatment, additional fracture experiments confirmed that the toughness degradation was mainly caused by high temperature tempering and not by the effects of hydrogen embrittlement due to long-term exposure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. 1982 · 283
2. Buscemi · ASME J. Eng. Mater. Technol. · 1991 · 113 · 32910.1115/1.2903414 ↗
3. Task Group I of the Subcommittee on Hydrogen Embrittlement of Japan Pressure Vessel Research Council · Weld. Res. Counc. Bull. · 1985 · 305 · 1
4. Task Group II of the Subcommittee on Hydrogen Embrittlement of Japan Pressure Vessel Research Council · Weld. Res. Counc. Bull. · 1985 · 305 · 9
5. Moss · Fatigue Fracture Eng. Mater. Struct. · 1994 · 17 · 36910.1111/j.1460-2695.1994.tb00237.x ↗
6. Tan · Petro-Chem. Equipment · 2003 · 32 · 9
7. Kawakami · Weld. Res. Abroad · 1999 · 45 · 19
8. Byeong Ook Kong · ASME, Pressure Vessels and Piping Division, PVP-413 · 2000 · 151
9. Kayano Rinzo · ASME, Pressure Vessels and Piping Division, PVP-442 · 2002 · 67
10. Islam · J. Mater. Eng. Perform. · 2003 · 12 · 24410.1361/105994903770343079 ↗
11. Yaguchi · ASME, Pressure Vessels and Piping Division, PVP-490 · 2004 · 161
12. Islam · J. Mater. Eng. Perform. · 2004 · 13 · 60010.1361/10599490420610 ↗
13. Murakami · ASTM STP · 1985 · 755 · 383
14. Viswanathan · 1989
15. Sreenivasan · J. Eng. Mater. Technol. · 2003 · 12510.1115/1.1543969 ↗
16. GB228-87, Metallic Materials—Tensile Testing, China, 1987 (in Chinese).
17. ASTM A370, Standard Test Method and Definitions for Mechanical Testing of Steel Products, 1990.
18. GB229-94, Metallic Materials—Charpy V-Notch Impact Testing, China, 1994 (in Chinese).