Effect of hot forging and Mn content on austenitic stainless steel containing high carbon
Source abstract
Abstract
Abstract This paper is a trial to process austenitic stainless steel of different manganese contents 4.35, 6.48 and 9.27 wt%. The high temperature deformation was in range less than 1200 down to 950 °C to prevent the hot severe cracks. The tensile strength increase as the Mn contents increases before and after thermomechanical treatment. For 4.35 and 6.48 Mn steels, the high deformation temperature accelerates the dynamic recrystallization of Fe–Mn steels leading to fine grains. The ferrite phase increases as the Mn contents increases. Sigma phase after thermomechanical deformation miniaturizes and the final microstructure is fully austenitic surrounded by thin carbides on the grain boundaries. For 9 wt%Mn steel, partial dynamic recrystallization happens and this deteriorates the strength and ductility.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Rama Rao · Int. Mater. Rev. · 1989 · 34
2. Chesseret et al., United States Patent: 6,056,917 (2 May 2000).
3. Bayraktar · J. Mater. Process. Technol. · 2004 · 147 · 14510.1016/j.jmatprotec.2003.10.007 ↗
4. EL-Bitar · Can. Metall. Q. · 2000 · 39 · 36110.1179/cmq.2000.39.3.361 ↗
5. Kim et al., United States Patent: 5,647,922 (15 July 1997).
6. Cabanas · Metall. Mater. Trans. A · 2006 · 37A · 330510.1007/BF02586165 ↗
7. P. Cugy, A.Hildenbrand, M. Bouzekri, D. Cornette, S. Goklu, H. Hofmann, www.msm.cam.ac.uk/phase-trans/2005/LINK/92.pdf.
8. Tomota · Metall. Trans. A · 1986 · 17A · 53710.1007/BF02643961 ↗
9. Choi et al., United States Patent: 5,634,990 (3 June 1997).