Low-temperature sintering of BaTiO3 powders prepared by a hydrothermal process with ball milling system
Source abstract
Abstract
Abstract In this work, a hydrothermal process with ball milling system was developed to produce nanosized BaTiO 3 powders with low-temperature sintering capability. By using this apparatus, it was possible to synthesize nanosized BaTiO 3 powders from Ba(OH) 2 and titanium alkoxides at 100 °C after 2 h. The primary particle size was determined to be about 20 nm. Moreover, nanosized BaTiO 3 particles were uniformly agglomerated to about 150 nm. The green bodies prepared from these powders were densified above 95% at 900 °C, which is fairly lower than the ordinary sintering temperature. The densification was about 60% at 900 °C in the green bodies fabricated from powders synthesized by the hydrothermal reaction without ball milling system. The sinterability was found higher for the BaTiO 3 powders synthesized by ball milling-assisted hydrothermal process. The characterization of the synthesized powders and the sintered compacts was carried out by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. For the electrical properties, room temperature dielectric constants as high as 4000 were measured.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Dielectric materials and actuators · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Bruno · J. Am. Ceram. Soc. · 1993 · 76 · 123310.1111/j.1151-2916.1993.tb03747.x ↗
2. Yanez · Ceram. Inter. · 2000 · 26 · 27110.1016/S0272-8842(99)00053-X ↗
3. Mazdiyasni · J. Am. Ceram. Soc. · 1969 · 52 · 52310.1111/j.1151-2916.1969.tb09157.x ↗
4. Luan · Ceram. Inter. · 2001 · 27 · 64510.1016/S0272-8842(01)00012-8 ↗
5. Segal · J. Non-Cryst. Solids · 1984 · 63 · 18310.1016/0022-3093(84)90397-1 ↗
6. Shimooka · J. Mater. Chem. · 2000 · 10 · 151110.1039/b000792g ↗
7. Xia · J. Eur. Ceram. Soc. · 1995 · 15 · 117110.1016/0955-2219(95)00101-8 ↗
8. Xu · Mater. Lett. · 2004 · 58 · 158210.1016/j.matlet.2003.10.030 ↗
9. Pinceloup · J. Am. Ceram. Soc. · 1999 · 82 · 304910.1111/j.1151-2916.1999.tb02201.x ↗
10. Xu · J. Am. Ceram. Soc. · 2003 · 86 · 20310.1111/j.1151-2916.2003.tb03307.x ↗
11. Kajiyoshi · J. Am. Ceram. Soc. · 1991 · 74 · 36910.1111/j.1151-2916.1991.tb06889.x ↗
12. Clark · J. Mater. Chem. · 1999 · 9 · 8310.1039/a805756g ↗
13. Moon · J. Eur. Ceram. Soc. · 2003 · 23 · 215310.1016/S0955-2219(03)00016-5 ↗
14. Lencka · Chem. Mater. · 1995 · 7 · 1810.1021/cm00049a006 ↗
15. Dawson · Am. Ceram. Soc. Bull. · 1988 · 67 · 1673
16. Lencka · Chem. Mater. · 1993 · 5 · 6110.1021/cm00025a014 ↗
17. Bussem · J. Am. Ceram. Soc. · 1966 · 49 · 3310.1111/j.1151-2916.1966.tb13144.x ↗
18. Bussem · J. Am. Ceram. Soc. · 1992 · 75 · 292610.1111/j.1151-2916.1992.tb04363.x ↗
19. G. de With
20. Zhao · Phys. Rev. B · 2004 · 70 · 02410710.1103/PhysRevB.70.024107 ↗
21. Lin · Phys. Rev. B · 2006 · 74 · 13411510.1103/PhysRevB.74.134115 ↗