Contributions to yield strength in an ultrafine grained 1050 aluminum alloy after DC current annealing
Source abstract
Abstract
Abstract The ultrafine grained (UFG) 1050 aluminum alloy was prepared by equal channel angular pressing at cryogenic temperature (cryoECAP). The evolution of the yield strength and microstructures of UFG 1050 aluminum alloy after direct electric current (DC current) annealing at 150–400 °C for 1 h were investigated by tensile test, electron back scattering diffraction pattern (EBSD) and transmission electron microscopy (TEM). For the cryoECAPed and annealed samples at 150–250 °C, the predominant boundaries are high angle boundaries (HABs) (>60%), many dislocations accumulate at subgrain and/or grain boundaries, the yield strength (126–159 MPa) mainly comes from the dislocation and grain boundary strengthening contributions. While an unusual increase in the yield strength (by 8.1–11.2%) observed in samples annealed at 150–200 °C is attributed to an additional strengthening contribution from the more HABs having stable structures which can act as effective barriers to dislocation motion during tensile deformation. When annealing at 300–400 °C, the microstructures are free of dislocations, the yield strength (29–45 MPa) comes from the grain boundary strengthening contribution. With the application of DC current, the larger grain size, lower dislocation density and higher fraction of LABs having misorientation angle between 3−7° in samples annealed at 150–250 °C result in the lower yield strength, while the smaller average grain sizes in samples annealed at 300–400 °C cause the higher yield strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electromagnetic Effects on Materials · Microstructure and mechanical properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Ultra-fine grained bulk steel produced by accumulative roll-bonding (ARB) process10.1016/S1359-6462(99)00015-9 ↗
2. Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation10.1016/S0921-5093(00)01660-9 ↗
3. Improving both strength and ductility of a Mg alloy through a large number of ECAP passes10.1016/j.msea.2009.01.040 ↗
4. Strength and ductility of ultrafine grained aluminum and iron produced by ARB and annealing10.1016/S1359-6462(02)00282-8 ↗
5. Enhanced tensile ductility and toughness in nanostructured Cu10.1063/1.1465528 ↗
6. Strengthening mechanisms in nanostructured high-purity aluminium deformed to high strain and annealed10.1016/j.actamat.2009.05.017 ↗
7. Transition of tensile deformation behaviors in ultrafine-grained aluminum10.1016/j.actamat.2005.05.005 ↗
8. Nanostructured aluminium alloys produced by severe plastic deformation: New horizons in development10.1016/j.msea.2012.09.020 ↗
9. Hall-Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
10. Microstructural evolution of IF-steel during cold rolling10.1016/j.actamat.2003.10.040 ↗
11. Microstructure and strength of nickel at large strains10.1016/S1359-6454(00)00082-3 ↗
12. Microstructure and strength of commercial purity aluminium (AA 1200) cold-rolled to large strains10.1016/S1359-6454(02)00174-X ↗
13. Quantitative analysis of structure-strength relation of commercial purity aluminium deformed by accumulative roll bonding and annealed at low temperature10.4028/www.scientific.net/MSF.426-432.405 ↗
14. Tailoring dislocation structures and mechanical properties of nanostructured metals produced by plastic deformation10.1016/j.scriptamat.2009.02.018 ↗
15. Hardening by annealing and softening by deformation in nanostructured metals10.1126/science.1124268 ↗
16. Mechanical properties of submicron-grained aluminum10.1016/j.scriptamat.2004.10.035 ↗
17. Effects of electropulse duration and frequency on grain growth in Cu10.1016/0956-716X(90)90270-Q ↗
18. Enhancement of homogeneity of grain boundary microstructure by magnetic annealing of electrodeposited nanocrystalline nickel10.1016/S1359-6462(03)00329-4 ↗
19. Evolution of mechanical properties of ultrafine grained 1050 alloy during annealed with d.c. current10.1016/j.matchar.2016.01.007 ↗
20. Effect of an electric field on the recovery and recrystallization of Al and Cu10.1016/0036-9748(89)90252-4 ↗
21. Effect of prior cold work on the influence of electric current pulses on the recrystallization of copper10.1016/0036-9748(84)90522-2 ↗
22. Magnetically enhanced recrystallization in an aluminum alloy10.1016/j.scriptamat.2006.08.018 ↗
23. Enhanced phase transformation and variant selection by electric current pulses in a Cu-Zn alloy10.1557/jmr.2014.76 ↗
24. Effects of d.c. current on the phase transformation in 7050 alloy during homogenization10.1016/j.matchar.2014.07.017 ↗
25. Increased hardenability of steel by an external electric field10.1016/0167-577X(90)90127-8 ↗
26. Effect of an electric field on the superplasticity of 7475 Al10.1016/0036-9748(89)90514-0 ↗
27. Effect of pulse electric current stimulation on the microstructure, mechanical properties and thermal fatigue behavior of cast-hot-working die steel10.2355/isijinternational.48.212 ↗
28. Influences of magnetic annealing on the grain growth in a cryoECAPed 1050 aluminum alloy10.1016/j.matchar.2013.07.020 ↗
29. The role of dislocations in the flow stress-grain size relationships10.1007/BF02900225 ↗
30. New discoveries in deformed metals10.1007/s11661-001-0167-x ↗
31. Effects of electric current on solid state phase transformations in metals10.1016/S0921-5093(00)00780-2 ↗
32. Effect of driving forces on atom motion10.1016/0040-6090(75)90047-4 ↗
33. The combined action of a surface-active melt and irradiation on zinc single crystals10.1007/BF01115923 ↗
34. Effect of electric current pulses on the recrystsallization of metals10.1016/0036-9748(83)90183-7 ↗
35. Microstructure and electrical conductivity of Cu-Cr-Zr alloy aged with dc electric current10.1016/j.jallcom.2008.03.054 ↗
36. Electrical and mechanical properties of Cu-Cr-Zr alloy aged under imposed direct continuous current10.1016/S1003-6326(11)61290-9 ↗
37. Humphreys · 1995