Influence of the temperature on the strength and the subcritical crack growth rate of alumina
Source abstract
Abstract
Abstract Dynamic four-point-bending tests between 20 and 900 °C were carried out in laboratory air on an alumina ceramic with a few intergranular glass phases (MgO, SiO 2 , CaO). The inert strength decreases with increasing temperature from 25 to 900 °C. In this range the temperature has no influence on the values of the corrected Weibull modulus m k . This means, that the strength distribution of the alumina investigated did not depend on the test temperature. The subcritical crack growth parameter A increases with increasing temperature from 25 to 500 °C and then decreases with further increasing temperature up to 900 °C. In contrast to this behaviour, for the parameter n the opposite temperature dependence turns out; n decreases between 25 and 500 °C and then increases. From d a /d t - K I plots it can be seen that the subcritical crack growth behaviour changes at a temperature of about 500 °C. For a constant crack propagation rate K I decreases with increasing temperature from 25 to 500 °C and then increases with further increasing temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Fatigue and fracture mechanics · Probabilistic and Robust Engineering Design
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. D. Munz, T. Fett, Ceramics—Mechanical Properties, Failure Behaviour, Materials Selection, Springer-Verlag, Berlin, ISBN 3-540-65376-7, 1999.10.1007/978-3-642-58407-7 ↗
2. Fett · J. Mater. Sci. Lett · 2003 · 22 · 36310.1023/A:1022693009794 ↗
3. Charles · J. Appl. Phys · 1958 · 29 · 165710.1063/1.1723019 ↗
4. R. Nejma, K.-H. Lang, D. Löhe, in: Proceedings of the Material Week 2002 Conference on Lifetime Behaviour of Alumina at Room and Higher Temperatures, München, 30 September–2 October 2002, ISBN 3-88355-314-X, Mat. Info, Frankfurt/Main, Germany, 2003.
5. German Draft Standard DIN 51110, Prüfung von keramischen Hochleistungswerkstoffen Teil 1-3, Deutsches Institut für Normung (DIN), Berlin, 1990, passed into ENV 843/5.
6. German Draft Standard DIN 51109, Prüfung von keramischen Hochleistungswerkstoffen, Ermittlung der Risszähigkeit KIC, Deutsches Institut für Normung (DIN), Berlin, 1991.
7. H. Bügler, Thermische Ermüdung und Rissausbreitung in polykristallinem Aluminiumoxid, PhD Thesis, Universität Erlangen, 1983.
8. Powell-Dogan · J. Am. Ceram. Soc · 1990 · 73 · 367010.1111/j.1151-2916.1990.tb04274.x ↗
9. K. Hauffe, Reaktionen in und an Festen Stoffen, Springer-Verlag, Berlin, 1966.10.1007/978-3-642-88042-1 ↗
10. Clarcke · J. Mater. Sci · 1985 · 20 · 132110.1007/BF01026328 ↗
11. C. Wolf, Kriechverhalten von glasphasenhaltigem Aluminiumoxid, VDI-Fortschrittsberichte, Reihe 5, Nr. 386, VDI Verlag Düsseldorf, 1995.
12. J. Stark, Verformungsverhalten und Kriechporenbildung von reinem und glasphasenhaltigem Aluminiumoxid, PhD Thesis, Universität Hamburg, 1990.