Fracture toughness of a lamellar orientation-controlled TiAl-based alloy processed by either one-step or two-step compression at high temperature
Source abstract
Abstract
Abstract In this work, the effects of lamellae orientation and the distribution of fine grains and fine lamellar colonies on the fracture toughness of orientation-controlled Ti-43 mol%Al alloy were examined. Fracture toughness was determined by three-point bending tests following the introduction of a chevron notch, and thermomechanical processing to control lamellar orientation consisted of high temperature compression in the α single-phase and (α + γ) two-phase regions. Materials processed via one-step compression in the α single-phase region exhibited tilting of the lamellae interface by approximately 20–30° relative to the compression plane. Further compression in the (α + γ) two-phase region (termed two-step compression) arranged the lamellae interface nearly parallel to the compression plane. Fine grains were also observed around the orientation-controlled lamellar colonies, and were converted into fine lamellar colonies during heat treatment following processing in the (α + γ) two-phase region. The proportion of fine grains decreased with an increase in the true strain rate during compression in the (α + γ) two-phase region. Specimens processed by one-step compression had fracture toughness values lower than those of two-step compression specimens. In addition, specimens processed using two-step compression and exhibiting a crack arrester orientation had higher fracture toughness values than those with a crack divider orientation. The fine grains and colonies formed at the lamellar colony boundaries were found not to affect the fracture toughness of specimens with either of these crack orientations. However, decreased quantities of fine grains and colonies may increase the toughness of specimens for which crack propagation occurs in conjunction with crack arrester orientation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Progress in the understanding of gamma titanium aluminides10.1007/BF03221103 ↗
2. Ordered intermetallic alloys, Part III: gamma titanium aluminides10.1007/BF03220745 ↗
3. Fatigue-crack growth and fracture resistance of a two-phase (γ+α2) TiAl alloy in duplex and lamellar microstructures10.1016/0921-5093(94)03264-5 ↗
4. Strength and ductility in TiAl alloys10.1016/S0966-9795(98)00037-5 ↗
5. The effect of microstructure on fracture toughness and fatigue crack growth behavior in γ-titanium aluminide based intermetallics10.1007/s11661-999-0048-2 ↗
6. Quantitative evaluation of toughening mechanisms of TiAl with lamellar structure10.2320/jinstmet1952.58.4_418 ↗
7. Effects of lamellae spacing and colony size on the fracture resistance of a fully-lamellar TiAl alloy10.1016/0956-7151(94)00278-P ↗
8. Fracture behavior and toughness of PST crystals of TiAl10.1016/1359-6454(95)00255-3 ↗
9. Deformation and fracture of PST crystals and directionally solidified ingots of TiAl-based alloys10.1016/S0966-9795(98)00055-7 ↗
10. Fracture in lamellar TiAl simulated with the cohesive model10.1016/j.engfracmech.2006.09.022 ↗
11. Effects of niobium addition on the sustained-load cracking characteristics in lamellar microstructure γ-base TiAl10.1016/0921-5093(95)09831-3 ↗
12. The relationship between fracture toughness and microstructure of fully lamellar TiAl alloy10.1007/s10853-006-1382-z ↗
13. Micromechanisms and micromechanics of fracture of TiAl intermetalics
14. Fracture behaviour of TiAl intermetalics
15. Effect of microstructure change on cracking behaviour in heat treated Ti-Al-V alloy10.2320/jinstmet.74.481 ↗
16. Crack resistance characterization in TiAl intermetallics with enhanced toughness10.4028/www.scientific.net/KEM.741.13 ↗
17. Control of lamellar arrangement in TiAl alloys by high-temperature deformation in α single phase and subsequent annealing in two phase region10.2320/matertrans1989.36.610 ↗
18. Orientation control of (α2 + γ) lamellae in TiAl intermetallic compounds by two-step compression at high temperature10.2320/jinstmet1952.61.5_378 ↗
19. Deformation behavior of Ti-43 mol% aluminum in α single phase region and orientation distribution of lamellae after cooling10.2320/jinstmet1952.66.4_425 ↗
20. Production of Ti-43mol%Al with oriented lamellar microstructure and its creep characteristics10.2464/jilm.55.343 ↗
21. Lamellar orientation control in TiAl base alloys by a two-step compression process at high temperature10.1016/j.msea.2008.12.027 ↗
22. Effect of formed fine grains on creep property in lamellar orientation controlled TiAl base alloy processed by a two-step compression at high temperature10.2320/jinstmet.74.475 ↗
23. Microstructural evolution during hot working of Ti aluminide alloys: influence of phase constitution and initial casting texture
24. Microstructure and texture formation during hot rolling of niobium-rich γ TiAl alloys with different carbon contents10.1002/adem.200600127 ↗
25. Texture evolution of the γ- and the α/α2-phase during hot rolling of γ-TiAl based alloys10.1016/j.intermet.2005.07.002 ↗
26. The use of chevron notched specimens for fracture toughness determination of bearing steels
27. Kassner · 2009
28. Formation mechanism of texture during dynamic recrystallization in γ-TiAl, nickel and copper examined by microstructure observation and grain boundary analysis based on local orientation measurements10.1016/S1359-6454(03)00218-0 ↗
29. Reassessment of the binary aluminum-titanium phase diagram10.1361/154770306X109809 ↗