Recrystallization in a directionally solidified cobalt-base superalloy
Source abstract
Abstract
The recrystallization behavior in a range of annealing temperature from 1020 to 1280 degrees C in a directionally solidified cobalt-base superalloy was studied. Local recrystallization first appeared at 1040 degrees C. The recrystallized volume increased rapidly as increasing the annealing temperature. Pinning effect of all carbides (M23C6, M7C3 and MC) was observed and large amount of twin formed at low annealing temperature. The size of the recrystallized grains increased significantly at high annealing temperatures accompanied with the sharp decrease of twin. The effect of annealing temperature and the role of carbide and twin on the development of the recrystallization were discussed. (c) 2007 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Advanced Materials Characterization Techniques · Solidification and crystal growth phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Sims · 1987
2. Bűrgel · 2000 · 229
3. Okazaki · 2003 · 63
4. Cox · Mater. Sci. Technol. · 2003 · 19 · 44010.1179/026708303225010731 ↗
5. Jo · Mater. Sci. Technol. · 2003 · 19 · 166510.1179/026708303225008301 ↗
6. Wang · Scripta Mater. · 2006 · 55 · 45710.1016/j.scriptamat.2006.05.013 ↗
7. Khan · J. Met. · 1986 · 38 · 16
8. Sims · J. Met. · 1969 · 21 · 27
9. B.C. Yan, J. Zhang, L.H. Lou, Mater. Sci. Technol., in press.
10. Jiang · Mater. Sci. Eng. A · 1999 · 271 · 10110.1016/S0921-5093(99)00183-5 ↗
11. Mishin · Mater. Sci. Eng. A · 1999 · 260 · 5510.1016/S0921-5093(98)00978-2 ↗
12. Parthasarathy · Scripta Metall. · 1983 · 17 · 94310.1016/0036-9748(83)90267-3 ↗