Spark plasma sintering and hydrogen pre-annealing of copper nanopowder
Source abstract
Abstract
Abstract Copper nanopowders were sintered using Spark Plasma Sintering (SPS). Special attention was paid to the presence of natural surface oxide and reductive thermal treatments under H 2 atmosphere were carried out to remove it. The sintering mechanisms were investigated by the means of disrupted experiments at various temperatures to reach different shrinkage rates. Optimized experiments were also carried out to reach a maximum densification. The samples were characterized and compared using density measurement, X-ray diffraction, mechanical tests (tension and compression) and analysis of the fracture surfaces with scanning electron microscope. On the one hand, it results that during the SPS treatment, the raw powder undergoes a series of oxide transformations from CuO to Cu 2 O. On the other hand, reductive treatment drastically decreases the sintering temperature, from 650 °C to 260 °C, to reach 90% density without grain growth. Higher mechanical strength, up to 750 MPa, also shows better consolidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Copper Interconnects and Reliability · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. The systems-based design of high-strength, high-conductivity alloys10.1007/BF02914659 ↗
2. High strength and high electrical conductivity copper alloy for high pin count leadframes
3. Nanostructured Cu-Cr alloy with high strength and electrical conductivity10.1063/1.4874655 ↗
4. Effect of grain size reduction and geometrical confinement in fine grained copper: potential applications as material for reversible electrical contacts10.1002/adem.200900346 ↗
5. Activation volume and deviation from Cottrell–Stokes law at small grain size10.1016/j.ijplas.2009.10.003 ↗
6. Competing regimes of rate dependent plastic flow in ultrafine grained metals10.1016/j.msea.2012.09.072 ↗
7. Mechanical properties of nanostructured materials10.1016/j.pmatsci.2005.08.003 ↗
8. Principles of equal-channel angular pressing as a processing tool for grain refinement10.1016/j.pmatsci.2006.02.003 ↗
9. Generation of metallic nanocomposites by severe plastic deformation10.1179/1743280412Y.0000000003 ↗
10. Challenges and advances in nanocomposite processing techniques10.1016/j.mser.2006.11.002 ↗
11. Consolidation/synthesis of materials by electric current activated/assisted sintering10.1016/j.mser.2008.09.003 ↗
12. Transparent MgAl2O4 ceramic produced by spark plasma sintering10.1016/j.scriptamat.2009.03.039 ↗
13. Viscous flow during spark plasma sintering of Ti-based metallic glassy powders10.1016/j.jallcom.2012.12.129 ↗
14. The critical role of heating rate in enabling the removal of surface oxide films during spark plasma sintering of Al-based bulk metallic glass powder10.1016/j.jnoncrysol.2013.05.001 ↗
15. A comparative study of nickel and alumina sintering using spark plasma sintering (SPS)10.1016/j.matchemphys.2012.02.059 ↗
16. Does the Branly effect occur in spark plasma sintering?10.1088/0022-3727/45/9/092001 ↗
17. Dense nanostructured nickel produced by SPS from mechanically activated powders: enhancement of mechanical properties10.1155/2013/674843 ↗
18. A study of microstructure and hardness of bulk copper sample obtained by consolidating nanocrystalline powders using plasma pressure compaction10.1016/S0921-5093(01)00931-5 ↗
19. Preparation and characterization of nanocrystalline copper powders10.1016/1359-6462(96)00170-4 ↗
20. Sintering of copper nanopowders under hydrogen: an in situ X-ray diffraction analysis10.1016/S0921-5093(03)00446-5 ↗
21. Oxidation mechanism of copper at 623–1073K
22. Mechanism of Spark Plasma Sintering and its application to ceramics
23. Neck formation between copper spherical particles under single-mode and multimode microwave sintering10.1016/j.msea.2009.12.032 ↗
24. Phases distribution dependent strength in metallic glass–aluminium composites prepared by spark plasma sintering10.1016/j.msea.2012.03.100 ↗
25. Compressive yield strengths of nanocrystalline Cu and Pd10.1016/S1359-6462(97)00157-7 ↗
26. S.M. Alam, F. Wei, C.L. Gan, C.V. Thompson, D.E. Troxel, Electromigration reliability comparison of Cu and Al interconnects, in: Proceeding of Quality of Electronic Design ISQED 2005 Sixth International Symposium on Quality Electronic Design, 2005.10.1109/ISQED.2005.51 ↗
27. Approach of the spark plasma sintering mechanism in Zr57Cu20Al10Ni8Ti5 metallic glass10.1016/j.jallcom.2010.09.158 ↗
28. Theory of the tensile test10.1016/0001-6160(67)90211-8 ↗
29. Strain rate sensitivity as a measure of ductility