journal article·1995-02

High temperature dynamic fatigue performance of a hot isostatically pressed silicon nitride

A.A. Wereszczak, T.P. Kirkland, K. Breder, M.K. Ferber, Pramod Khandelwal

Materials Science and Engineering: A· Volume 191· Issue 1-2
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Advanced gas turbines
2. 1986 · 324
3. Current status of 300 kW industrial ceramic gas turbine R&D in Japan10.1115/1.2906685 ↗
4. Evaluation of tensile static, dynamic, and cyclic fatigue behavior for a HIPed silicon nitride at elevated temperatures
5. Slow crack growth in sintered silicon nitride
6. Dynamic and static fatigue behavior of sintered silicon nitrides
7. Thermodynamic analysis of the high-temperature stability of silicon nitride and silicon carbide10.1016/0390-5519(76)90022-3 ↗
8. Calculation of stresses and strains in four-point bending creep tests10.1111/j.1151-2916.1971.tb12263.x ↗
9. Evaluation of the strength and creep-fatigue behaviour of hot isostatically pressed silicon nitride10.1111/j.1151-2916.1992.tb05598.x ↗
10. Slow crack growth in brittle materials under dynamic loading conditions10.1007/BF00113930 ↗
11. Effects of oxidation and oxidation under load on strength distributions of Si3N410.1111/j.1151-2916.1982.tb10451.x ↗
12. Role of oxidation in the time-dependent failure behavior of hot isostatically pressed silicon nitride at 1370 °C10.1111/j.1151-2916.1993.tb04039.x ↗
13. Environment effects on the flexure strength of HIPed silicon nitride at elevated temperatures
14. Effects of oxidation and creep damage mechanisms on creep behavior in HIPed silicon nitrides
15. A.A. Wereszczak, M.K. Ferber, T.P. Kirkland, M.R. Foley and R.L. Yeckley, Evolution of stress failure resulting from stress/oxidation damage in a hot isostatically pressed silicon nitride at elevated temperatures, submitted to J. Am. Ceram. Soc.
16. Internal phase changes in dense Si3N4 associated with high-temperature oxidation10.1111/j.1151-2916.1981.tb10256.x ↗
17. Stress-enhanced oxidation of silicon nitride ceramics10.1111/j.1151-2916.1993.tb06614.x ↗
18. Microstructural evolution in near-eutectic yttrium silicate compositions fabricated from a bulk melt and as an intergranular phase in silicon nitride10.1111/j.1151-2916.1990.tb04260.x ↗
19. Crystallization of the glassy phase in an Si3N4 material by post-sintering heat treatments10.1007/BF01132031 ↗
20. Fracture toughness (KIc and γwof) of a HIPed Si3N4 at elevated temperatures
21. Strengthening of a sintered silicon nitride by a post-fabrication heat treatment10.1111/j.1151-2916.1982.tb10415.x ↗
22. A comparison of reducing and oxidizing heat treatments of hot-pressed silicon nitride10.1111/j.1151-2916.1983.tb09981.x ↗
23. Viscosities, glass transition temperatures, and microhardness of Y-Si-Al-O-N glasses10.1111/j.1151-2916.1984.tb19752.x ↗