Brittle failure of Alloy 693 at elevated temperatures
Source abstract
Abstract
Abstract This reports transgranular brittle failure during high temperature deformation of a wrought Alloy 693 received in solution annealed condition. This has been attributed to the inability to suppress the formation of γ′ precipitates during quenching after the solution annealing treatment. The fine γ′ precipitates severely strained the matrix and inhibited plasticity during subsequent deformation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Molten salt chemistry and electrochemical processes · Aluminum Alloy Microstructure Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. Donachie · 2002
2. Verma · Meas. Sci. Technol. · 2010 · 21 · 10510610.1088/0957-0233/21/10/105106 ↗
3. Singh · Eng. Fail. Anal. · 2013 · 32 · 23610.1016/j.engfailanal.2013.03.018 ↗
4. R. Yoda, Y. Sato, T. Watanabe, in: Proceedings of International Symposium on Structural Stability in Superalloys, 1968, 80.10.7449/1968/Superalloys_1968_80_114 ↗
5. Tapia · 2006
6. Rogen · Trans. Metall. Soc. AIME · 1960 · 180