journal article·2007-05

Effects of sintering parameters on the structures of Fe–Cr–Al extruded honeycombs

Y. Zhou, X.Q. Zuo, J.H. Sun, J. Mei, J.L. Sun

Materials Science and Engineering: A· Volume 457· Issue 1-2
Publisher page

Abstract

Abstract Pure Fe, Cr and Al powders were used to mix with an additive to prepare a powder-mixed paste. Fe–25Cr–5Al honeycombs were fabricated by extruding the powder-mixed paste, then dried and sintered. The volume shrinkage and the apparent density of extruded honeycombs after drying and sintering were measured. The effect of sintering temperature and time on the volume shrinkage, the apparent density and the structure of honeycombs had been studied. The results show that the volume shrinkage and the apparent density of metallic honeycombs increase with temperature, the volume shrinkage ranging from 25% to 53%, and the apparent density ranging from 1.0 g/cm3 to 1.7 g/cm3. When sintering at 1250 °C, the volume shrinkage and the apparent density of metallic honeycombs increase with time, reach a maximum at 35–40 min, then decrease. The structure of sintered honeycombs consists of α-Fe, Fe–Cr–Al compounds and Al2O3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Brake Systems and Friction Analysis · Heat and Mass Transfer in Porous Media · Cellular and Composite Structures

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Dempsey · Int. J. Heat Mass Transfer · 2005 · 48 · 52710.1016/j.ijheatmasstransfer.2004.09.013 ↗
2. Lu · Int. J. Heat Mass Transfer · 1999 · 42 · 203110.1016/S0017-9310(98)00306-8 ↗
3. Lu · Acta Mater. · 1998 · 46 · 361910.1016/S1359-6454(98)00031-7 ↗
4. Nonnenmann · SEA Trans. · 1985 · 1 · 1814
5. Wierzbicki · Int. J. Impact Eng. · 1983 · 1 · 15710.1016/0734-743X(83)90004-0 ↗
6. Cheng · Cailiao Daobao · 1999 · 13 · 22
7. L. Erison, J. Kutka, US Patent 5,578,265 (1995).
8. Y. Mikio, F. Masuhiro, F. Nobuhiro, WO 9,417,911 (1994).
9. Seely, L. Richard, US Patent 6,302,679 (2001).
10. Hayes · Mech. Mater. · 2004 · 36 · 69110.1016/j.mechmat.2003.06.001 ↗
11. Cochran · 2000 · 25
12. Cochran · 2002 · 127
13. Clark · 2002 · 116
14. Hayes · 2002 · 137
15. Hurysz · 2002 · 167
16. Clark · 2002 · 147
17. S. Morihiko, K. Kouichi, N. Mitsunobu, K. Takazi, US Patent 4,582,677 (1986).
18. Huang · 1997
19. Chinje · Ironmaking Steelmaking · 1989 · 13 · 90
20. Czyska-Filemonowicz · Solid State Ionics · 1999 · 117 · 1310.1016/S0167-2738(98)00243-4 ↗
21. Badini · Surf. Coat. Technol. · 2001 · 135 · 29110.1016/S0257-8972(00)00989-0 ↗
22. Hou · Appl. Surf. Sci. · 2001 · 178 · 15610.1016/S0169-4332(01)00327-0 ↗
23. Jelinski · Solid State Ionics · 1997 · 103 · 103310.1016/S0167-2738(97)00299-3 ↗