journal article·2018-01

Non-inclusion induced crack initiation in multiphase high-strength steel during very high cycle fatigue

P. Zhao, Z. Liu, R.D.K. Misra, F. Du, C. Zhang, Z.G. Yang, E. Yan

Publisher page

Abstract

Abstract During very high cycle fatigue (VHCF) crack can initiate at non-inclusion site in the interior of Mn-Si-Cr bainite/martensite (B/M) multiphase steels. The characteristics of non-inclusion induced crack initiation in B/M multiphase steels and the relationship between the size of granular bright facet (GBF) and VHCF limit were studied through ultrasonic fatigue testing, in terms of fracture surface analysis, crack initiation analysis, and failure mechanism. The current study reveals that GBF area became smaller with the increase of VHCF limit, i.e. the steel with higher fatigue-endurance strength exhibited smaller GBF area in the case of steel characterized by non-inclusion crack initiation in the VHCF regime. The relationship between GBF area, fatigue life, and applied stress was consistent with the following equation area GBF = 29.41LogNf − 0.2916 σ a + 47.51. The study provides an understanding of non-inclusion induced crack initiation in VHCF and a guidance for steel fatigue design.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels · Fire effects on concrete materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. The future of metals10.1126/science.1185866 ↗
2. Nishijima AI · 1989
3. Analysis of Microstructure Evolution in Quenching and Partitioning Automotive Sheet Steel10.1007/s11661-011-0869-7 ↗
4. Effect of mixed on the strength and toughness of low carbon alloy steels
5. WangQY, WangZG, Shou-XinLI.Extra-long life fatigue behavior of key materials for high-speed railway, Electric Drive for Locomotives. 2003.
6. Designing Fe–Mn–Si alloys with improved low-cycle fatigue lives10.1016/j.scriptamat.2014.11.024 ↗
7. Fatigue life improvement of 12Cr1МoV steel by irradiation with Zr + ion beam10.1016/j.ijfatigue.2014.10.011 ↗
8. Very high cycle fatigue behavior of shot-peened 3Cr13 high strength spring steel10.1016/j.matdes.2013.03.039 ↗
9. Effect of microstructure on fatigue behavior of advanced high strength steels produced by quenching and partitioning and the role of retained austenite10.1016/j.msea.2015.06.034 ↗
10. Study of crack initiation or damage in very high cycle fatigue using ultrasonic fatigue test and microstructure analysis10.1016/j.ultras.2013.05.008 ↗
11. Influence of inclusion size on fatigue behavior of high strength steels in the gigacycle fatigue regime10.1016/j.ijfatigue.2006.06.004 ↗
12. Gigacycle Fatigue Properties of High-Strength Steels According to Inclusion and ODA Sizes10.1007/s11661-007-9225-3 ↗
13. Rotating bending fatigue properties of two case hardening steels after nitriding treatment10.1016/j.matdes.2012.08.061 ↗
14. Ultra-high-cycle fatigue properties and fracture mechanism of modified 2.25Cr-1Mo steel at elevated temperatures10.1016/j.ijfatigue.2005.08.016 ↗
15. Very high cycle fatigue mechanism of carbide-free bainite/martensite steel micro-alloyed with Nb10.1016/j.msea.2009.08.024 ↗
16. Very high cycle fatigue behaviors of Mn-Si-Cr series Bainite/Martensite dual phase steels10.1016/j.matdes.2010.01.008 ↗
17. Competition mechanism between microstructure type and inclusion level in determining VHCF behavior of bainite/martensite dual phase steels10.1016/j.ijfatigue.2010.10.004 ↗
18. Effect of microstructure on the very high cycle fatigue behavior of a bainite/martensite multiphase steel10.1016/j.msea.2015.02.015 ↗
19. The significance of ultrafine film-like retained austenite in governing very high cycle fatigue behavior in an ultrahigh-strength MN-SI-Cr-C steel10.1016/j.msea.2015.07.095 ↗
20. The potential significance of microalloying with niobium in governing very high cycle fatigue behavior of bainite/martensite multiphase steels10.1016/j.msea.2015.10.044 ↗
21. Characteristic S-Nproperties of high-carbon-chromium-bearing steel under axial loading in long-life fatigue10.1046/j.1460-2695.2002.00574.x ↗
22. Subsurface crack initiation and propagation mechanism in high-strength steel in a very high cycle fatigue regime10.1016/j.ijfatigue.2005.08.015 ↗
23. Factors influencing the mechanism of superlong fatigue failure in steels10.1046/j.1460-2695.1999.00187.x ↗
24. A method for obtaining and analyzing sensitivity data10.1080/01621459.1948.10483254 ↗
25. Ultra high cycle fatigue behavior of a medium-carbon high strength spring steel NHS1
26. Factors influencing the GBF size of high strength steels in the very high cycle fatigue regime10.1016/j.msea.2010.10.017 ↗
27. Investigation of crack initiation and propagation behavior of AISI 310 stainless steel up to very high cycle fatigue10.1016/j.ijfatigue.2013.04.009 ↗
28. Diversity of damage evolution during cyclic loading at very high numbers of cycles10.1179/1743280411Y.0000000005 ↗
29. The physics of fatigue crack initiation10.1016/j.ijfatigue.2012.10.009 ↗
30. Notch effect on fatigue strength reduction of bearing steel in the very high cycle regime10.1016/j.ijfatigue.2005.04.017 ↗
31. Ultra-long cycle fatigue of high-strength carbon steels part I: review and analysis of the mechanism of failure10.1016/S0921-5093(03)00135-7 ↗
32. The formation of subsurface non-defect fatigue crack origins10.1016/j.ijfatigue.2005.06.060 ↗
33. S–N curve characteristics and subsurface crack initiation behaviour in ultra‐long life fatigue of a high carbon-chromium bearing steel10.1046/j.1460-2695.2001.00459.x ↗
34. Effect of hydrogen on very high cycle fatigue properties of high strength spring steel 60Si2CrVA
35. Ultra high cycle fatigue behavior of a medium-carbon high strength spring steel NHSⅠ
36. Factors influencing the GBF size of high strength steels in the very high cycle fatigue regime10.1016/j.msea.2010.10.017 ↗
37. The fatigue behaviors of zero-inclusion and commercial 42CrMo steels in the super-long fatigue life regime10.1016/j.actamat.2004.06.031 ↗
38. Effect of grain size on fatigue properties of 42CrMoVNb steel
39. Bainite in silicon steels: new composition–property approach Part 110.1179/030634583790420646 ↗
40. Microstructural examination of two experimental high-strength bainitic low-alloy steels containing silicon10.1179/mst.1987.3.6.441 ↗
41. Fatigue crack growth behaviour of a Si–Mn steel with carbide-free lathy bainite10.1023/A:1018565702991 ↗