Microstructure and high temperature strength of SiCW/SiC composites by chemical vapor infiltration
Source abstract
Abstract
Abstract SiC W /SiC composites without an intergranular glassy phase are prepared by the CVI process. The microstructure and high temperature strength of SiC W /SiC composites are investigated. The high temperature strength of SiC W /SiC composites depends on the interfacial bonding strength between matrix and whiskers. The matrix is effectively strengthened and toughened by the whiskers, and SiC W /SiC composites show a constant strength of 475 ± 32 MPa below 1000 °C. The flexural strength gradually declines from 475 ± 32 MPa to 208 ± 15 MPa at the temperature from 1000 °C to 1500 °C due to the decreased whisker-matrix interfacial bonding strength. The interfacial bonding strength is too low to transfer stress from the matrix to the whiskers, and SiC W /SiC composites show a constant strength of 208 ± 15 MPa at temperatures from 1500 °C to 1800 °C. The fracture mode of SiC W /SiC composites changes from the toughened fracture below 1000 °C to the brittle fracture above 1000 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Pan · J. Eur. Ceram. Soc · 1999 · 19 · 178910.1016/S0955-2219(98)00280-5 ↗
2. Gallardo-López · Acta Mater · 1999 · 47 · 218510.1016/S1359-6454(99)00072-5 ↗
3. Magnani · J. Eur. Ceram. Soc · 2005 · 25 · 161910.1016/j.jeurceramsoc.2004.05.014 ↗
4. Chen · Acta Mater · 2000 · 48 · 459910.1016/S1359-6454(00)00246-9 ↗
5. Kim · J. Am. Ceram. Soc · 2001 · 84 · 206010.1111/j.1151-2916.2001.tb00958.x ↗
6. Guo · J. Eur. Ceram. Soc · 2003 · 23 · 202310.1016/S0955-2219(03)00030-X ↗
7. Choi · Scripta Mater · 2004 · 50 · 120310.1016/j.scriptamat.2004.02.008 ↗
8. Izhevskyi · J. Am. Ceram. Soc · 2005 · 88 · 111510.1111/j.1551-2916.2005.00212.x ↗
9. Kim · Acta Mater · 2007 · 55 · 72710.1016/j.actamat.2006.08.059 ↗
10. Magnani · J. Eur. Ceram. Soc · 2009 · 29 · 241110.1016/j.jeurceramsoc.2008.12.020 ↗
11. Kinoshita · Acta Mater · 1997 · 45 · 80110.1016/S1359-6454(96)00179-6 ↗
12. Wiederhorn · J. Eur. Ceram. Soc · 1999 · 19 · 227310.1016/S0955-2219(99)00121-1 ↗
13. Magnani · J. Eur. Ceram. Soc · 2001 · 21 · 63310.1016/S0955-2219(00)00244-2 ↗
14. Hirota · Mater. Sci. Eng. A · 2007 · 458 · 21610.1016/j.msea.2006.12.065 ↗
15. Tani · Composites: Part A · 1999 · 30 · 41910.1016/S1359-835X(98)00129-8 ↗
16. Hua · Mater. Sci. Eng. A · 2006 · 428 · 34610.1016/j.msea.2006.05.050 ↗
17. Hua · J. Mater. Sci · 2010 · 45 · 39210.1007/s10853-009-3953-2 ↗
18. Hua · Comput. Mater. Sci · 2009 · 46 · 13310.1016/j.commatsci.2009.02.014 ↗
19. Li · J. Mater. Sci · 2008 · 43 · 280610.1007/s10853-008-2539-8 ↗
20. Lillo · Ceram. Eng. Sci. Proc · 2003 · 24 · 35910.1002/9780470294802.ch53 ↗
21. Magnani · Ceram. Int · 2000 · 26 · 49510.1016/S0272-8842(99)00084-X ↗