Effect of loading rate on the monotonic tensile behavior and tensile strength of an oxide–oxide ceramic composite at 1200°C
Source abstract
Abstract
Abstract The influence of loading rate on monotonic tensile behavior and tensile properties of an oxide–oxide ceramic composite was evaluated in laboratory air at 1200 °C. The composite consists of a porous alumina matrix reinforced with woven mullite/alumina (Nextel™720) fibers, has no interface between the fiber and matrix, and relies on the porous matrix for flaw tolerance. Tensile tests conducted at loading rates of 0.0025 and 25 MPa/s revealed a strong effect of rate on the stress–strain behavior as well as on the ultimate tensile strength (UTS), elastic modulus and failure strain. At 0.0025 MPa/s, increase in stress results in non-monotonic change in strain, with the rate of change of strain reversing its sign at stresses ∼25 MPa/s. Several samples were subjected to additional heat treatments prior to testing in order to determine whether this unusual stress–strain behavior was an artifact of incomplete processing of fibers in the as-received material. The unusual material response in the 0–30 MPa stress range was further investigated in creep tests conducted with the applied stresses ≤26 MPa. Negative creep (i.e. decrease in strain under constant stress) was observed. Porosity measurements indicate that a decrease in matrix porosity and matrix densification may be taking place in the N720/A composite exposed to 1200 °C at stresses
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. Zok · J. Am. Ceram. Soc. · 2006 · 89 · 330910.1111/j.1551-2916.2006.01342.x ↗
2. Zawada · J. Am. Ceram. Soc. · 2003 · 86 · 128210.1111/j.1151-2916.2003.tb03464.x ↗
3. Kerans · Am. Ceram. Soc. Bull. · 1989 · 68 · 429
4. Evans · J. Mater. Sci. · 1994 · 29 · 385710.1007/BF00355946 ↗
5. Kerans · Composites: Part A · 1999 · 30 · 52110.1016/S1359-835X(98)00144-4 ↗
6. Kerans · J. Am. Ceram. Soc. · 2002 · 85 · 259910.1111/j.1151-2916.2002.tb00505.x ↗
7. Prewo · J. Mater. Sci. · 1988 · 23 · 52310.1007/BF01174679 ↗
8. Mah · J. Mater. Sci. · 1984 · 19 · 119110.1007/BF01120029 ↗
9. Brennan · 1990
10. Heredia · J. Am. Ceram. Soc. · 1995 · 78 · 209710.1111/j.1151-2916.1995.tb08621.x ↗
11. Nutt · 1995
12. Evans · J. Am. Ceram. Soc. · 1996 · 79 · 234510.1111/j.1151-2916.1996.tb08982.x ↗
13. More · J. Am. Ceram. Soc. · 2000 · 83 · 21110.1111/j.1151-2916.2000.tb01172.x ↗
14. More · 1999
15. Ferber · 2000 · 210
16. Haynes · J. Am. Ceram. Soc. · 2000 · 83 · 65710.1111/j.1151-2916.2000.tb01250.x ↗
17. Opila · J. Am. Ceram. Soc. · 1997 · 80 · 19710.1111/j.1151-2916.1997.tb02810.x ↗
18. Opila · J. Am. Ceram. Soc. · 1994 · 77 · 73010.1111/j.1151-2916.1994.tb05357.x ↗
19. Opila · J. Am. Ceram. Soc. · 1999 · 82 · 62510.1111/j.1151-2916.1999.tb01810.x ↗
20. Hermes · 1988 · 73
21. A. Szweda, M.L. Millard, M.G. Harrison, U.S. Patent No. 5,601,674 (1997).
22. Sim · Ceram. Eng. Sci. Proc. · 1992 · 13 · 632
23. Moore · Ceram. Eng. Sci. Proc. · 1994 · 15 · 11310.1002/9780470314500.ch13 ↗
24. Lewis · 1995 · 41
25. Lange · Mater. Sci. Eng. A · 1995 · A195 · 14510.1016/0921-5093(94)06513-6 ↗
26. Lunderberg · 1995 · 95
27. Mouchon · Composites · 1995 · 26 · 17510.1016/0010-4361(95)91380-N ↗
28. Morgan · J. Am. Ceram. Soc. · 1995 · 78 · 155310.1111/j.1151-2916.1995.tb08851.x ↗
29. Tu · J. Am. Ceram. Soc. · 1996 · 79 · 41710.1111/j.1151-2916.1996.tb08138.x ↗
30. Levi · J. Am. Ceram. Soc. · 1998 · 81 · 207710.1111/j.1151-2916.1998.tb02590.x ↗
31. A.G. Hegedus. U.S. Patent No. 50,177,522 (May 21, 1991).
32. T.J. Dunyak, D.R. Chang, M.L. Millard, in: J.D. Buckley (ed.), Proceedings of 17th Conference on Metal Matrix, Carbon, and Ceramic Matrix Composites, NASA Conference Publication 3235, Part 2, NASA, 1993, pp. 675–690.
33. Zawada · 1994 · 267
34. Lu · J. Am. Ceram. Soc. · 1996 · 79 · 26610.1111/j.1151-2916.1996.tb07908.x ↗
35. Zok · Adv. Eng. Mater. · 2001 · 3 · 1510.1002/1527-2648(200101)3:1/2<15::AID-ADEM15>3.0.CO;2-A ↗
36. Sorensen · J. Am. Ceram. Soc. · 1996 · 79 · 31310.1111/j.1151-2916.1996.tb08122.x ↗
37. Choi · J. Am. Ceram. Soc. · 2004 · 87 · 191210.1111/j.1151-2916.2004.tb06340.x ↗
38. Choi · Int. J. Fatigue · 2005 · 27 · 50310.1016/j.ijfatigue.2004.10.001 ↗
39. Choi · J. Eur. Ceram. Soc. · 2005 · 25 · 162910.1016/j.jeurceramsoc.2004.05.024 ↗
40. Zawada · J. Am. Ceram. Soc. · 2003 · 86 · 98110.1111/j.1151-2916.2003.tb03406.x ↗
41. Ruggles-Wrenn · Composites: Part A · 2006 · 37 · 202910.1016/j.compositesa.2005.12.008 ↗
42. Mehrman · Comp. Sci. Technol. · 2007 · 67 · 142510.1016/j.compscitech.2006.09.005 ↗
43. Ruggles-Wrenn · Int. J. Fatigue · 2008 · 30 · 50210.1016/j.ijfatigue.2007.04.004 ↗
44. Jurf · J. Eng. Gas Turbines Power, Trans. ASME · 1999 · 122 · 20210.1115/1.483195 ↗
45. Zawada · 1997 · 69
46. COI Ceramics, unpublished data.
47. Milz · Eng. Sci. Proc. · 1999 · 20 · 19110.1002/9780470294567.ch23 ↗
48. Goering · Eng. Sci. Proc. · 1997 · 18 · 9510.1002/9780470294437.ch10 ↗
49. Wiederhorn · 1974 · 613
50. Evans · J. Mater. Sci. · 1972 · 7 · 113710.1007/BF00550196 ↗
51. Evans · Int. J. Fracture · 1974 · 10 · 25110.1007/BF00113930 ↗
52. Wilson · Ceram. Eng. Sci. Proc. · 1995 · 16 · 100510.1002/9780470314784.ch44 ↗
53. Deleglise · J. Eur. Ceram. Soc. · 2002 · 22 · 150110.1016/S0955-2219(01)00461-7 ↗
54. Carelli · J. Am. Ceram. Soc. · 2002 · 85 · 59510.1111/j.1151-2916.2002.tb00138.x ↗
55. Fujita · J. Am. Ceram. Soc. · 2004 · 87 · 26110.1111/j.1551-2916.2004.00261.x ↗
56. Fujita · J. Am. Ceram. Soc. · 2005 · 88 · 36710.1111/j.1551-2916.2005.00061.x ↗