Study of age hardening in a Mg–2.2 wt%Nd alloy by in situ synchrotron X-ray diffraction and mechanical tests
Source abstract
Abstract
Abstract Microstructure evolution of a supersaturated solid solution Mg–2.2 wt%Nd alloy during aging at 240 °C for 6 h (stage I), at 295 °C for 3 h (stage II), and finally at 320 °C for 1 h (stage III) was studied by in situ synchrotron X-Ray diffraction. In stage I, diffraction from β 1 (Mg 3 Nd, FCC) precipitates was observed after ~ 15 min. Evolution of the volume, size, and aspect ratio of β 1 with the aging time were estimated from peak intensity and peak width analysis. In stage II, diffraction from β (Mg 12 Nd, tetragonal) precipitates was observed after ~ 36 min while β 1 remained in the material. In stage III, the volume of β 1 reduced substantially in relative to β . The identified precipitation sequence from the in situ aging experiment is supported by ex situ electron microscopy observations. β ′, which had not been detected by synchrotron X-rays, was additionally found using transmission electron microscopy in the material by the end of aging stage I. Tension and hardness tests using specimens with different aging conditions were further performed to understand how different precipitates affect the strength and ductility of the Mg–Nd alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Magnesium: properties–applications–potential10.1016/S0921-5093(00)01351-4 ↗
2. Magnesium: current and potential automotive applications10.1007/BF02701073 ↗
3. Preface to the viewpoint set on: the current state of magnesium alloy science and technology10.1016/j.scriptamat.2010.06.029 ↗
4. Current issues in magnesium sheet alloys: where do we go from here?10.1016/j.scriptamat.2014.04.017 ↗
5. Fabrication of extraordinary high-strength magnesium alloy by hot extrusion10.1016/j.scriptamat.2009.06.003 ↗
6. Towards the development of heat-treatable high-strength wrought Mg alloys10.1016/j.scriptamat.2010.01.038 ↗
7. High strength magnesium alloys through precipitation hardening and micro alloying: considerations for alloy design10.1007/s11837-015-1561-y ↗
8. Microstructure and strengthening mechanism of high strength Mg–10Gd–2Y–0.5Zr alloy10.1016/j.jallcom.2006.03.015 ↗
9. Strengthening and toughening mechanisms in Mg–Zn–Y alloy with a long period stacking ordered structure10.1016/j.actamat.2010.05.012 ↗
10. Physical factors controlling the observed high-strength precipitate morphology in Mg–rare earth alloys10.1016/j.actamat.2013.10.066 ↗
11. Fabrication of a high strength Mg–11Gd–4.5Y–1Nd–1.5Zn–0.5Zr (wt%) alloy by thermomechanical treatments10.1016/j.msea.2014.10.077 ↗
12. Precipitation evolution and hardening in Mg-Sm-Zn-Zr alloys10.1016/j.actamat.2016.03.068 ↗
13. Microstructure and mechanical properties in cast magnesium-neodymium binary alloys10.1016/j.msea.2007.05.058 ↗
14. The structures of precipitates in an Mg–0.5 at%Nd age-hardened alloy studied by HAADF-STEM technique10.2320/matertrans.M2011163 ↗
15. Homogeneous and heterogeneous precipitation mechanisms in a binary Mg–Nd alloy10.1007/s10853-014-8404-z ↗
16. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
17. Nano-precipitates made of atomic pillars revealed by single atom detection in a Mg-Nd alloy10.1063/1.3701272 ↗
18. Formation of high-strength β′ precipitates in Mg–RE alloys: the role of the Mg/β″interfacial instability10.1016/j.actamat.2014.09.024 ↗
19. Linear-chain configuration of precipitates in Mg-Nd alloys10.1016/j.actamat.2014.09.037 ↗
20. Solute clusters and GP zones in binary Mg–RE alloys10.1016/j.actamat.2015.12.047 ↗
21. On the early stages of precipitation in dilute Mg–Nd alloys10.1016/j.actamat.2016.01.055 ↗
22. Early precipitate morphologies in Mg-Nd-(Zr) alloys10.1016/j.scriptamat.2016.09.015 ↗
23. Willmott · 2011
24. Microstructural characterization of polycrystalline materials by synchrotron X-rays10.1007/s11706-013-0201-0 ↗
25. Tempering of a martensitic stainless steel: investigation by in situ synchrotron X-ray diffraction10.1016/j.actamat.2014.07.050 ↗
26. Lattice misfit during ageing of a polycrystalline nickel-base superalloy10.1016/j.actamat.2013.09.018 ↗
27. Introduction of the X-ray diffraction beamline of SSRF
28. Identification of NdH2 particles in solution-treated Mg–2.5%Nd (wt%) alloy10.1016/j.jallcom.2009.06.040 ↗
29. Effect of Nd content and heat treatment on the thermal conductivity of Mg–Nd alloys10.1016/j.jallcom.2016.05.261 ↗
30. The Scherrer formula for x-ray particle size determination10.1103/PhysRev.56.978 ↗
31. The role of crystallography and thermodynamics on phase selection in binary magnesium-rare earth (Ce or Nd) alloys10.1016/j.actamat.2012.04.039 ↗
32. A simulation study of β1 precipitation on dislocations in a Mg-rare earth alloy10.1016/j.actamat.2014.04.054 ↗
33. Simulation study of precipitation in a Mg–Y–Nd alloy10.1016/j.actamat.2012.05.013 ↗
34. Comprehensive study of phase transformation in age-hardening of Mg–3Nd–0.2Zn by means of scanning transmission electron microscopy10.1016/j.actamat.2015.05.001 ↗
35. The formation and structure of precipitates in a dilute magnesium-neodymium alloy10.1016/0022-5088(73)90007-6 ↗
36. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗
37. Characterisation of strengthening precipitate phases in a Mg–Y–Nd alloy10.1016/S1359-6454(00)00013-6 ↗
38. Predicting β’ precipitate morphology and evolution in Mg-RE alloys using a combination of first-principles calculations and phase-field modeling10.1016/j.actamat.2014.05.002 ↗
39. Interfacial structures and energetics of the strengthening precipitate phase in creep-resistant Mg-Nd-based alloys10.1038/srep40540 ↗