Studies on hydrogen embrittlement in Zr- and Ni-based amorphous alloys
Source abstract
Abstract
Mechanical and structural properties of Zr 50 Ni 27 Ni 18 Co 5 (at.%) and Ni 55 Zr 16 Ti 13 Nb 7 Sn 3 Si 2 (at.%) amorphous alloys were studied before and after hydrogenation. In both alloys, upon hydrogenation, a significant reduction in mechanical properties was evident. The occurrence of hydrogen embrittlement was supported by fracture morphology and is further explained based on the corresponding structural changes induced by hydrogenation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Phase-change materials and chalcogenides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. Inoue · Acta Mater. · 2000 · 48 · 27910.1016/S1359-6454(99)00300-6 ↗
2. Eliaz · Adv. Perform. Mater. · 1999 · 6 · 510.1023/A:1008748627295 ↗
3. Yamaura · Mater. Trans. · 2004 · 45 · 33010.2320/matertrans.45.330 ↗
4. Lee · J. Mater. Res. · 2004 · 18 · 221
5. Jayalakshmi · J. Alloy Compd. · 2006 · 417 · 19510.1016/j.jallcom.2005.07.076 ↗
6. Luborsky · J. Appl. Phys. · 1976 · 47 · 364810.1063/1.323173 ↗
7. Ashok · Scripta Metall. · 1981 · 15 · 33110.1016/0036-9748(81)90355-0 ↗
8. Munoz-Morris · Scripta Mater. · 2002 · 47 · 3110.1016/S1359-6462(02)00093-3 ↗
9. Ding · Scripta Metall. · 1987 · 21 · 168510.1016/0036-9748(87)90158-X ↗
10. Schoeder · J. Non-Crystall. Solids · 1983 · 56 · 21310.1016/0022-3093(83)90470-2 ↗
11. Yamaura · Mater. Trans. · 2002 · 43 · 254310.2320/matertrans.43.2543 ↗
12. Zander · J. Non-Crystall. Solids · 1999 · 250–252 · 89310.1016/S0022-3093(99)00200-8 ↗
13. Li · J. Alloy Compd. · 2000 · 297 · 30310.1016/S0925-8388(99)00614-3 ↗
14. Cullity · 2001
15. Miracle · Nat. Mater. · 2004 · 3 · 69710.1038/nmat1219 ↗
16. Yan · J. Alloy Compd. · 2004 · 381 · 8610.1016/j.jallcom.2004.02.054 ↗