Improving the ductility of nanostructured Al alloy using strongly textured nano-laminated structure combined with nano-precipitates
Source abstract
Abstract
Abstract A ductile nanostructured Al alloy with desired microstructure is tailored via the precipitation optimization and texture design. The microstructure consists of two-dimensional nano-laminated structure with strong texture and one-dimensional elongated sub-micron structure with intra-precipitations at nanoscale and sub-nanoscale level. The precipitation optimization is realized by the appropriate introduction of its embryo in the NS matrix before aging. The embryo is the solute-rich structures (solute clusters) segregated to dislocations due to strain-induced dissolution of initial precipitations into the matrix. These nano-precipitations not only impede dislocation motion but also accommodate plastic deformation during loading. The textured laminate activates the partial dislocation mechanism in high stacking-fault energy alloys and the extrinsic toughening mechanism during loading. In addition, the laminated structure exhibits significant texture strengthening. Therefore, both nano-precipitations and textured laminated structure are responsible for the simultaneous increase in strength and ductility. Additionally, the initial deformable precipitations play a positive role in microstructural refinement and the refined structure shows significant cluster strengthening, ~20% relative contribution to total strength. This paper provides a new understanding of designing nanostructured materials for achieving high ductility by several toughening strategies, which is expected to be applicable to other age-hardenable alloys and steels as well.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. Strengthening mechanisms in a high-strength bulk nanostructured Cu-Zn-Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
2. Nanostructured metals: retaining ductility10.1038/nmat1141 ↗
3. Stacking fault energies and slip in nanocrystalline metals10.1038/nmat1136 ↗
4. Deformation-mechanism map for nanocrystalline metals by molecular-dynamics simulation10.1038/nmat1035 ↗
5. Dislocation processes in the deformation of nanocrystalline aluminium by molecular-dynamics simulation10.1038/nmat700 ↗
6. In situ TEM observation of dislocation motion in thermally strained Al nanowires10.1016/S1359-6454(02)00348-8 ↗
7. In situ TEM observation of grain annihilation in tricrystalline aluminum films10.1016/j.actamat.2011.12.013 ↗
8. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
9. Achieving large uniform tensile ductility in nanocrystalline metals10.1103/PhysRevLett.105.215502 ↗
10. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
11. Simultaneously increasing the ductility and strength of ultra-fine-grained pure copper10.1002/adma.200601472 ↗
12. Simultaneously increasing the ductility and strength of nanostructured alloys10.1002/adma.200600310 ↗
13. Optimizing the strength and ductility of fine structured 2024 Al alloy by nano-precipitation10.1016/j.actamat.2007.06.043 ↗
14. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
15. Strong strain hardening in nanocrystalline nickel10.1103/PhysRevLett.103.205504 ↗
16. Double-peak age strengthening of cold-worked 2024 aluminum alloy10.1016/j.actamat.2012.11.039 ↗
17. Microalloying ultrafine grained Al Alloys with enhanced ductility
18. Segregation stabilizes nanocrystalline bulk steel with near theoretical strength10.1103/PhysRevLett.113.106104 ↗
19. Atomic-scale mechanisms of deformation-induced cementite decomposition in pearlite10.1016/j.actamat.2011.03.022 ↗
20. On strain-induced dissolution of θ′ and θ particles in Al-Cu binary alloy during equal channel angular pressing10.1016/j.msea.2010.12.060 ↗
21. Reprecipitation behavior in Al-Cu binary alloy after severe plastic deformation-induced dissolution of θ′ particles10.1016/j.msea.2012.03.010 ↗
22. Microstructure of two-phase Al–1.7at% Cu alloy deformed by equal-channel angular pressing10.1016/S1359-6454(00)00308-6 ↗
23. Precipitation hardening and grain refinement in an Al-4.2wt% Mg-1.2wt% Cu processed by ECAP10.1007/s10853-008-2746-3 ↗
24. Microstructure and strengthening mechanisms in cold-drawn pearlitic steel wire10.1016/j.actamat.2011.02.017 ↗
25. Tailoring a gradient nanostructured age-hardened aluminum alloy using high-gradient strain and strain rate10.1016/j.matdes.2015.07.009 ↗
26. Deformation mechanism in nanocrystalline Al: partial dislocation slip10.1063/1.1594836 ↗
27. Deformation induced microtwins and stacking faults in aluminum single crystal10.1103/PhysRevLett.101.115505 ↗
28. Deformation twinning in nanocrystalline aluminum10.1126/science.1083727 ↗
29. Deformation-induced grain rotation and growth in nanocrystalline Ni10.1063/1.2828699 ↗
30. Strain-induced ultrahard and ultrastable nanolaminated structure in nickel10.1126/science.1242578 ↗
31. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility10.1073/pnas.1517193112 ↗
32. Make nanostructured metal exceptionally tough by introducing non-localized fracture behaviors10.1016/j.scriptamat.2008.04.048 ↗
33. Fracture of ECAP-deformed iron and the role of extrinsic toughening mechanisms10.1016/j.actamat.2013.01.057 ↗
34. Strength and biaxial formability of cryo-rolled 2024 aluminium subject to concurrent recovery and precipitation10.1016/j.actamat.2013.05.019 ↗
35. Precipitation behaviors in Al-Cu-Mg and 2024 aluminum alloys10.1007/BF02652342 ↗
36. Teixeira, quantifying the strain-induced dissolution of precipitates in Al alloy microstructures using nuclear magnetic resonance10.1016/j.actamat.2009.07.060 ↗
37. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
38. Nanocrystallization process and mechanism in a nickel alloy subjected to surface severe plastic deformation10.1016/j.actamat.2009.08.005 ↗
39. Deformation twins in nanocrystalline Al10.1063/1.1633975 ↗
40. Grain refinement in nanostructured Al-Mg alloys subjected to high pressure torsion10.1007/s10853-010-4604-3 ↗
41. Deformation of electrodeposited nanocrystalline nickel10.1016/S1359-6454(02)00421-4 ↗
42. Dimples on nanocrystalline fracture surfaces as evidence for shear plane formation10.1126/science.1084284 ↗
43. Strain hardening and ductility in a coarse-grain/nanostructure laminate material10.1016/j.scriptamat.2015.03.006 ↗
44. Achieving high strength and high ductility in precipitation-hardened alloys10.1002/adma.200500069 ↗
45. Optimization of strength and ductility of 2024 Al by equal channel angular pressing (ECAP) and post-ECAP aging10.1016/S1359-6462(03)00260-4 ↗
46. The dependence of final microstructure, texture evolution and mechanical properties of Al–Mg–Si–Cu alloy sheets on the intermediate annealing10.1016/j.msea.2015.02.029 ↗
47. Precipitation phenomena in an ultrafine-grained Al alloy10.1016/j.actamat.2012.12.037 ↗
48. Precipitation phenomena in ultrafine grained Al–Mg–Si alloy with heterogeneous microstructure10.1016/j.actamat.2015.10.030 ↗
49. Zirconium-vacancy binding and its influence on S′-precipitation in an Al–Cu–Mg alloy10.1016/0001-6160(89)90335-0 ↗
50. Nanostructural hierarchy increases the strength of aluminium alloys10.1038/ncomms1062 ↗
51. Formation of nanolaminated structure in an interstitial-free steel10.1016/j.scriptamat.2014.10.003 ↗
52. A model for the thermodynamics of and strengthening due to co-clusters in Al–Mg–Si-based alloys10.1016/j.actamat.2012.04.032 ↗
53. Microstructural evolution, strengthening and thermal stability of an ultrafine-grained Al–Cu–Mg alloy10.1016/j.actamat.2016.02.050 ↗
54. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
55. Slip system rheology of Al–1% Mn crystals deformed by hot plane strain compression10.1016/S0749-6419(00)00075-9 ↗
56. Reversible twinning in pure aluminum10.1103/PhysRevLett.102.205504 ↗
57. Combined effects of crystallographic orientation, stacking fault energy and grain size on deformation twinning in FCC crystals10.1080/14786430802438168 ↗