Abstract

Quaternary CrSiCN and ternary CrSiC coatings with various Si concentrations were synthesized on Si(100) wafers via adjusting the flow of (CH3)3SiH (TMS) in precursor gases. The mechanical property and crack resistance of these coatings were evaluated and compared, as well as the influence of Si concentration was investigated. Compared with the CrSiC coatings, the CrSiCN coatings had higher elasticity and compressive stresses, and in turn, exhibited higher resistance to radial cracks in despite of the Si concentration. The greater thickness of CrSiCN coatings is, the better the crack resistance is. By increasing Si concentration, the compressive stress was released in both categories of coatings, but the trends of crack generation for the two categories of coatings were totally different. For the CrSiCN coatings, a reduction of compressive stress prevented parallel crack initiation around the impression edge after unloading. In contrast, as the compressive stress in the CrSiC coatings was released, radial cracks were generated at the impression corners and the length of radial crack increases with the stress release.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
2. Damage resistance of SiC and Si3N4 coatings with control of microstructure and thickness10.1016/j.porgcoat.2008.08.024 ↗
3. Comparison in microstructure and mechanical properties of porous Si3N4 ceramics with SiC and Si3N4 coatings10.1016/j.msea.2009.08.053 ↗
4. Mechanical and tribological behavior of silicon nitride and silicon carbon nitride coatings for total joint replacements10.1016/j.jmbbm.2013.05.002 ↗
5. Toward hard yet tough ceramic coatings10.1016/j.surfcoat.2014.07.007 ↗
6. Deposition of TiSiN coatings by arc ion plating process10.1016/j.apsusc.2007.10.079 ↗
7. Tribological properties of TiSiN thin films deposited by laser ablation10.1016/j.surfcoat.2013.12.064 ↗
8. Influence of bias voltages on the structure and wear properties of TiSiN coating synthesized by cathodic arc plasma evaporation10.1016/j.tsf.2007.07.087 ↗
9. TiSiN nanocomposite coatings by chemical vapor deposition in a fluidized bed reactor at atmospheric pressure (AP/FBR-CVD)10.1016/j.surfcoat.2006.03.029 ↗
10. Atomistic simulations of the characteristics of TiSiN nanocomposites of various compositions10.1016/j.surfcoat.2009.04.021 ↗
11. Ambient and elevated temperature properties of TiN, TiAlN and TiSiN PVD films and their impact on the cutting performance of coated carbide tools10.1016/j.surfcoat.2009.07.001 ↗
12. Effects of TiN sublayers on the response of TiSiN nanocomposite coatings to nanoidentation and scratching contacts10.1016/j.msea.2010.03.100 ↗
13. Mechanical and tribological properties of Cr–N and Cr–Si–N coatings reactively sputter deposited10.1016/j.surfcoat.2005.02.214 ↗
14. Effect of Si doping on the wear properties of CrN coatings synthesized by unbalanced magnetron sputtering10.1016/j.tsf.2005.08.027 ↗
15. Factors governing the mechanical behaviour of CrSiN coatings: combined nanoindentation testing and transmission electron microscopy10.1016/j.msea.2011.11.072 ↗
16. Microabrasive wear resistance of CrN and CrSiN coatings10.1002/ppap.200731415 ↗
17. Microstructure and mechanical properties of Cr–Si–N coatings prepared by pulsed reactive dual magnetron sputtering10.1016/j.surfcoat.2008.02.014 ↗
18. Structure and mechanical properties of reactive sputtering CrSiN films10.1016/j.apsusc.2008.11.036 ↗
19. Structure and properties of CrSiN nanocomposite coatings deposited by hybrid modulated pulsed power and pulsed dc magnetron sputtering10.1016/j.surfcoat.2012.11.053 ↗
20. The effect of ZrSiN diffusion barrier on the bonding strength of titanium porcelain10.1016/j.surfcoat.2006.07.023 ↗
21. Synthesis and properties of nanocomposite MoSiN hard films10.1016/j.surfcoat.2005.12.046 ↗
22. Thermal stability of TaN, CrTaN, TaSiN, and CrTaSiN hard coatings in oxygen-containing atmospheres10.1016/j.surfcoat.2014.02.005 ↗
23. Comparative study of electrochemical and impact wear behavior of TiCN, TiSiCN, TiCrSiCN, and TiAlSiCN coatings10.1016/j.surfcoat.2012.11.058 ↗
24. Ternary and quarternary TiSiN and TiSiCN nanocomposite coatings obtained by chemical vapor deposition10.1016/j.surfcoat.2012.10.067 ↗
25. Tribological behavior of a TiSiCN coating tested in air and coolant10.1016/j.surfcoat.2006.08.066 ↗
26. Microstructure and tribological properties of CrN and CrSiCN coatings10.1016/j.surfcoat.2010.06.033 ↗
27. Microstructure and corrosion behavior of CrN and CrSiCN coatings10.1007/s11665-009-9534-3 ↗
28. Effects of Si addition on the characteristic evolution and syntheses of nanocomposite Cr–Si–C–N coatings prepared by a hybrid coating system10.1016/j.surfcoat.2005.08.042 ↗
29. Gradient CrCN cathodic arc PVD coatings10.1016/j.tsf.2008.08.005 ↗
30. Hard CrCN/CrN multilayer coatings for tribological applications10.1016/j.surfcoat.2009.12.019 ↗
31. Arc-evaporated CrN, CrN and CrCN coatings10.1016/j.vacuum.2008.05.005 ↗
32. Effect of substrate bias voltage on the properties of CrCN and CrN coatings deposited by cathodic arc evaporation10.1016/j.vacuum.2012.04.039 ↗
33. The properties of multilayer CrCN/CrN coatings dependent on their architecture10.1002/ppap.201000167 ↗
34. Tribological behaviour and microstructure of TiCxN(1−x) coatings deposited by filtered arc10.1016/S0043-1648(02)00010-8 ↗
35. Influence of the C content on the mechanical and tribological properties of the TiCN coatings deposited by LAFAD technique10.1016/j.surfcoat.2011.02.032 ↗
36. Evaluation of mechanical properties of Ti(Cr)SiC(O)N coated cemented carbide tools10.1016/j.vacuum.2012.10.002 ↗
37. Microstructure and tribological properties of Ti(Cr)SiCN coating deposited by plasma enhanced magnetron sputtering10.1016/j.vacuum.2012.03.053 ↗
38. Q.Z. Wang, Z.W. Wu, F. Zhou, H. Huang, K. Niitsu, J.W. Yan, Evaluation of crack resistance of CrSiCN coatings as a function of Si concentration via nanoindentation. Surf. Coat. Technol. 272, 2015, 239-245.10.1016/j.surfcoat.2015.04.001 ↗
39. Corrosion behaviour of nanocomposite TiSiN coatings on steel substrates10.1016/j.corsci.2011.07.011 ↗
40. Arc plasma deposition of TiSiN/Ni nanoscale multilayered coatings10.1016/j.matchemphys.2012.12.010 ↗
41. Carbon based Si- and Cr-containing thin films: chemical and nanomechanical properties10.1016/j.solidstatesciences.2009.02.029 ↗
42. 〈http://srdata.nist.gov/xps/〉
43. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
44. Influence of ductile interlayers on mechanical behaviour of hard coatings under depth-sensing indentation: a numerical study on TiAlN10.1007/s10853-010-4436-1 ↗
45. Mechanical and tribological behavior of silicon nitride and silicon carbon nitride coatings for total joint replacements10.1016/j.jmbbm.2013.05.002 ↗
46. 〈http://accuratus.com/silicar.html〉
47. Effect of addition of Cu into ZrOx film on its properties10.1016/j.surfcoat.2005.10.022 ↗
48. Toughness of hard nanostructured ceramic thin films10.1016/j.surfcoat.2006.07.020 ↗