Hydrogen-assisted cracking in a precipitation-hardened stainless steel: effects of heat treatment and displacement rate
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Precipitation hardening in a PH 13-8 Mo stainless steel10.1016/0025-5416(81)90034-3 ↗
2. 1991 · Vol. 2
3. An investigation of the high-temperature and solidification microstructures of PH 13-8 Mo stainless steel10.1007/BF02646991 ↗
4. Hydrogen embrittlement of PH 13-8 Mo steel in simulated real-life tests and slow strain rate tests10.5006/1.3585104 ↗
5. Delayed failure of PH13-8Mo steel plated with Al-IVD10.1007/BF02650253 ↗
6. Hydrogen embrittlement of PH 13-8 Mo steel
7. Hydrogen effects on fracture of PH 13-8 Mo steel
8. Hydrogen assisted cracking of palladium modified PH 13-8 stainless steel
9. The influence of palladium on the hydrogen-assisted cracking resistance of PH 13-8 Mo stainless steel10.1007/BF02665009 ↗
10. Hydrogen embrittlement of PH 13-8 Mo stainless steel — the effect of surface condition10.5006/1.3581930 ↗
11. Investigation of the conditions for crack propagation and arrest under cathodic polarization by rising step load bend testing10.5006/1.3585857 ↗
12. Hydrogen embrittlement behavior of palladium modified PH 13-8 Mo stainless steel as a function of age Hardening10.1016/0956-716X(94)90162-7 ↗
13. Standard Test Method for Determining J R Curves, Designation E1152-87, Annual Book of ASTM Standards, 3.01, ASTM, Philadelphia, PA, pp. 825–835.
14. J-integral R-curve testing of high strength steels utilizing the direct-current potential drop method
15. Single specimen fracture toughness testing of low strength steel plate using the direct current electrical potential method10.1520/JTE10730J ↗
16. Hydrogen embrittlement of PH 13-8 Mo stainless steel
17. Application of the electrical potential method to crack length measurements using Johnson's formula10.1520/JTE11560J ↗
18. Direct current potential difference fatigue crack measurement techniques
19. J.R. Scully, personal communication, 1993.
20. Device for nondestructive measurement of hydrogen permeation in high strength steels
21. Environment assisted cracking in β-titanium alloys
22. Influence of displacement rate on environmentally assisted cracking of precracked ductile steel specimens
23. Evaluation of environmentally assisted cracking of a high strength steel using elastic-plastic fracture mechanics techniques
24. The hydrogen embrittlement susceptibility of ferrous alloys: the influence of strain on hydrogen entry and transport
25. The crack-tip system and its relevance to the prediction of cracking in aqueous environments
26. Derivation and use of fundamental life prediction algorithms for stress corrosion cracking of low-alloy and carbon steels in 288 C water
27. The stress corrosion cracking of reactor pressure vessel steel in high temperature water10.1016/0010-938X(85)90003-4 ↗
28. Dependence of KISCC on loading rate and crack orientation in Ti-6Al-6V-2Sn10.5006/0010-9312-35.11.509 ↗
29. Finite deformation analysis of crack-tip opening in elastic-plastic materials and implications for fracture10.1016/0022-5096(77)90003-5 ↗
30. Relationships between the J-integral and the crack opening displacement for stationary and extending cracks10.1016/0022-5096(81)90003-X ↗
31. Notch and stress effects on fracture
32. Hydrogen/plasticity interactions in stress corrosion cracking
33. Hydrogen effects on the properties and fracture modes of iron-based alloys
34. Mechanisms of hydrogen related fracture of metals