Abstract
Abstract This study uses modified compact tension specimens to evaluate the fracture toughness of solder joints under a combination of tensile and shear loads. Copper substrates were coated with electroless nickel plating before they were soldered together. The samples were reflowed to peak temperatures of 215 and 240 °C for Sn–37Pb and Sn–3.5Ag, respectively, with appropriate preheating temperatures, holding time and cooling rates. Fracture toughness tests were conducted as per ASTM E399-90. Cross-sectional microstructural and fractography studies were carried out on the tested samples. Earlier fracture studies which were based on J integral as per ASTM E813-89 did not produce valid results because of brittleness of the solder joints. The current results showed that the fracture of the solder joints follows the general principles of a mixed mode fracture mechanism map and shear is the preferred mode of failure regardless of different mode of loadings, type of solders and substrate coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Mechanical Behavior of Composites · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Hutchinson · Adv. Appl. Mech. · 1991 · 29 · 6310.1016/S0065-2156(08)70164-9 ↗
2. Choi · Fatigue Fract. Eng. Mater. Struct. · 2001 · 23 · 110.1046/j.1460-2695.2001.00371.x ↗
3. Kang · Int. J. Fract. · 2002 · 113 · 19510.1023/A:1014264930542 ↗
4. Nayeb-Hashemi · Int. J. Fatigue · 2001 · 23 · S32510.1016/S0142-1123(01)00144-X ↗
5. Shi · Microelectron. Reliab. · 2004 · 44 · 84110.1016/j.microrel.2003.12.001 ↗
6. Pratt · J. Electron. Mater. · 1994 · 23 · 37510.1007/BF02671217 ↗
7. A. Buettner, Master's Thesis, University of Rochester, 1992.
8. Frear · Metall. Mater. Trans. A · 1994 · 25A · 150910.1007/BF02665483 ↗
9. Frear · J. Met. · 1996 · 48 · 49
10. Stromswold · J. Electron. Mater. · 1994 · 23 · 104710.1007/BF02650374 ↗
11. Pratt · IEEE CPMT Part A · 1996 · 19 · 134
12. Pratt · 1992 · 201
13. M. Manoharan, K.S. Siow, in: C.A. Volkert, A.H. Verbruggen, D. Brown (Eds.), Materials Research Society Symposium Proceedings (Mater. Reliab. Microelectron. IX) vol. 563, San Francisco, 1999, pp. 15–20.10.1557/PROC-563-15 ↗
14. Miglin · Res. Mech. · 1984 · 11 · 85
15. Schroth · Metall. Trans. · 1987 · 18A · 106110.1007/BF02668555 ↗
16. Manoharan · Acta Metall. Mater. · 1991 · 39 · 120310.1016/0956-7151(91)90208-I ↗
17. Manoharan · Scr. Metall. Mater. · 1992 · 26 · 118710.1016/0956-716X(92)90561-R ↗
18. Manoharan · Int. J. Fract. · 1995 · 73 · 4110.1007/BF00037649 ↗
19. Skipor · Eng. Fract. Mech. · 1995 · 52 · 64710.1016/0013-7944(95)00035-T ↗
20. Frear · 1991
21. Tu · Mater. Sci. Eng. Rev. · 2001 · R34 · 110.1016/S0927-796X(01)00029-8 ↗
22. Glazer · Int. Mater. Rev. · 1995 · 40 · 6510.1179/imr.1995.40.2.65 ↗
23. Manoharan · J. Test. Eval. · 1990 · 18 · 10610.1520/JTE12460J ↗
24. K.S. Siow, M. Manoharan, Proceedings of the First IPC/SMTA Electronics Assembly Expo, Institute PC and Surface Mount Technology Association, Providence, 1998, S19-3-1–S19-3-8.
25. McCormack · J. Met. · 1993 · 45 · 36
26. Morris · 1994 · 7
27. Morris · 1991 · 225
28. Sastry · 1992 · 1266
29. Marshall · Solder Surf. Mt. Tech. · 1997 · 9/3 · 11