Calculations of dominant factors of glass-forming ability for metallic glasses from viscosity

Akira Takeuchi, Akihisa Inoue

Publisher page

Abstract

Abstract The calculation models in which the viscosity is used as a main parameter are proposed for the estimation of the three glass-forming ability (GFA) factors: critical cooling rate ( R c ) for formation of glassy phase, reduced glass transition temperature ( T g / T m ) and supercooled liquid range (Δ T x ≡ T x − T g ), where T g , T m and T x are the glass transition, melting and crystallization temperature, respectively. The R c and T g / T m were analyzed on the basis of the homogeneous nucleation and growth theory by the construction of a time-transformation diagram for the crystallization of metallic glass. On the other hand, Δ T x was calculated on the basis of a free volume theory proposed by Beukel and Sietsma, and then was related with R c calculated from the time–transformation curve. The calculations were carried out for Fe-, Pd-, Pt-, Zr-, Mg-based metallic glasses for which the viscosity is expressed by Vogel–Fulcher–Tammann equation or the Doolittle equation. The calculated results summarized in R c − T g / T m and R c −Δ T x diagrams agree with the experimental data qualitatively. It was shown that all the GFA factors of metallic glasses can be calculated from viscosity. These results indicate that the viscosity is the key parameter for the determinations of R c , T g / T m and Δ T x .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Material Dynamics and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. A. Inoue, Bulk Amorphous Alloys—Preparation and Fundamental Characteristics, Materials Science Foundations 4, Trans Tech Publications, Netherlands, 1998, pp. 1–116.
2. Lu · J. Non-Cryst. Solids · 2000 · 270 · 10310.1016/S0022-3093(00)00064-8 ↗
3. Lu · Scripta Mater · 2000 · 42 · 66710.1016/S1359-6462(99)00417-0 ↗
4. H.A. Davies, in: B. Cantor (Ed.), Rapid Quenching and Formation of Metallic Glasses, Rapidly Quenched Metals III, 1, The Metal Society, 1978, p. 11.
5. van den Beukel · Acta Metall. Mater · 1990 · 38 · 38310.1016/0956-7151(90)90142-4 ↗
6. Takeuchi · Mater. Trans · 2001 · 42 · 237410.2320/matertrans.42.2374 ↗
7. Takeuchi · Mater. Trans · 2002 · 43 · 120510.2320/matertrans.43.1205 ↗
8. Ramachandrarao · J. Mater. Sci · 1977 · 12 · 248810.1007/BF00553936 ↗
9. Jha · Phys. Chem. Glasses · 1989 · 30 · 220
10. D.R. Uhlmann, N.J. Kreidl (Eds.), Viscosity and Relaxation Glass: Science and Technology, vol. 3, Academic Press, New York, 1986, p. 244.
11. Inoue · Acta Mater · 2001 · 49 · 264510.1016/S1359-6454(01)00181-1 ↗