Microstructure and mechanical properties of Ti–6Al–4V: Mill-annealed versus direct metal laser melted alloys
Source abstract
Abstract
Abstract Additive manufacturing processes such as direct metal laser melting (DMLM) are known to produce highly anisotropic microstructures. The present work compares the microstructure and mechanical properties of DMLM Ti–6Al–4V with that of mill-annealed alloys. Results show that the yield and hardening response of DMLM Ti–6Al–4V does not depend on the testing direction relative to the build direction, while the response of mill-annealed Ti–6Al–4V strongly depends on the testing direction. These results are discussed in light of the microstructure, texture, and polycrystal plasticity modeling.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Metal fabrication by additive manufacturing using laser and electron beam melting technologies10.1016/S1005-0302(12)60016-4 ↗
2. The topological design of multifunctional cellular metals10.1016/S0079-6425(00)00016-5 ↗
3. Wave propagation in equivalent continuums representing truss lattice materials10.1016/j.ijsolstr.2015.07.023 ↗
4. Advanced micro-lattice materials10.1002/adem.201400471 ↗
5. The microstructure and mechanical properties of deposited-IN718 by selective laser melting10.1016/j.jallcom.2011.10.107 ↗
6. Microstructure and mechanical properties of selective laser melted 18Ni-300 steel10.1016/j.phpro.2011.03.033 ↗
7. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
8. Highly anisotropic steel processed by selective laser melting10.1007/s11663-013-9875-z ↗
9. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
10. Direct fabrication of a Ti–47Al–2Cr–2Nb alloy by selective laser melting and direct metal deposition processes10.4028/www.scientific.net/AMR.89-91.586 ↗
11. M. Simonelli, Y.Y. Tse, C. Tuck, Further understanding of Ti6Al4V selective laser melting using texture analysis, in: Proceedings of the 23rd Annual International Solid Freeform Fabrication Symposium, Austin, TX., 2012, p. 480.
12. On the texture formation of selective laser melted Ti–6Al–4V10.1007/s11661-014-2218-0 ↗
13. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
14. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
15. As-fabricated and heat-treated microstructures of the Ti–6Al–4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
16. The thermomechanical processing of alpha/beta titanium alloys10.1007/BF02914711 ↗
17. Quantitative analysis of texture evolution in cold-rolled, continuous-cast AA 5xxx-series aluminum alloys10.1007/s11661-004-0127-3 ↗
18. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
19. Yield strength asymmetry predictions from polycrystal elastoplasticity10.1115/1.2812370 ↗
20. Defect evolution and pore collapse in crystalline energetic materials10.1088/0965-0393/17/3/035003 ↗
21. A three-dimensional crystal plasticity model for duplex Ti–6Al–4V10.1016/j.ijplas.2006.11.006 ↗
22. A. Anderson et al., Users Manual for ALE3D – an Arbitrary Lagrange/Eulerian 3D Code System, Lawrence Livermore National Laboratory, UCRL-MA-152204, 2003.
23. Laws for work-hardening and low-temperature creep10.1115/1.3443340 ↗
24. R. Pederson, Microstrcture and Phase Transformation of Ti-6Al-4V, Lulea University of Technology thesis, 2002, pp. 10–14.
25. Microstructure of Ti–6Al–4V produced by selective laser melting
26. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
27. On the change of the elastic limit and hardness of iron and steels through extension and compression, through heating and cooling, and through cycling
28. Mechanical behavior of Ti–6Al–4V at high and moderate temperatures—Part II: constitutive modeling10.1016/S0921-5093(01)01508-8 ↗
29. Mechanisms of ductility in CoTi and CoZr B2 intermetallics
30. The slip modes of titanium and the effect of purity on their occurrence during tensile deformation of single crystals
31. Mechanism of plastic flow in titanium-determination of slip and twinning elements
32. The deformation of alpha phase titanium
33. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗