Behavior of polysulfone composite and nanocomposite membranes under hypochlorite ageing
Source abstract
Abstract
Polysulfone activated carbon or graphite composite membranes and polysulfone montmorillonite clay nanocomposite membranes were prepared by wet-phase inversion method. Its effectiveness against hypochlorite degradation by forming composite and nanocomposite structures was studied by means of an ageing experiment. The formation of some fissures on the composite membrane surface was observed through electron micrographs scanning. The number-average molecular weight of the polysulfone of all membranes was reduced. This reduction was more noticeable in the composite membranes owing to the lower interaction between polymer chains and filler, such interaction being also the reason for polydispersity increase. Fourier transform infrared spectroscopy detected the reduction of the PSf bands in the nanocomposite membranes; in the composite membranes, some PSf band intensities were probably increased owing to the exposure of the PSf groups to the ageing process. All membranes presented brittleness with ageing, which was more pronounced in the composite membranes due to the membrane defects formed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fuel Cells and Related Materials · Polymer Nanocomposites and Properties · Membrane Separation Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. 10.1002/978047027628010.1002/9780470276280 ↗
2. Anadão P · Ciência e Tecnologia de Membranas · 2010
3. 10.1016/j.progpolymsci.2010.12.00510.1016/j.progpolymsci.2010.12.005 ↗
4. 10.1016/j.progpolymsci.2008.07.00210.1016/j.progpolymsci.2008.07.002 ↗
5. 10.1016/j.progpolymsci.2010.11.00110.1016/j.progpolymsci.2010.11.001 ↗
6. 10.1016/j.memsci.2010.06.02410.1016/j.memsci.2010.06.024 ↗
7. Wang Z L (ed) · Characterization of Nanophase Materials · 2000
8. 10.1016/j.techsoc.2008.04.01610.1016/j.techsoc.2008.04.016 ↗
9. 10.1016/j.jmatprotec.2006.03.05210.1016/j.jmatprotec.2006.03.052 ↗
10. 10.1016/S0927-796X(00)00012-710.1016/S0927-796X(00)00012-7 ↗
11. 10.3390/ma203099210.3390/ma2030992 ↗
12. 10.1016/j.eurpolymj.2009.01.02710.1016/j.eurpolymj.2009.01.027 ↗
13. 10.1016/j.jiec.2008.01.01110.1016/j.jiec.2008.01.011 ↗
14. 10.1016/j.progpolymsci.2008.07.00810.1016/j.progpolymsci.2008.07.008 ↗
15. 10.1016/j.progpolymsci.2003.08.00210.1016/j.progpolymsci.2003.08.002 ↗
16. 10.1016/S1359-0286(02)00049-910.1016/S1359-0286(02)00049-9 ↗
17. 10.1016/j.desal.2007.09.04310.1016/j.desal.2007.09.043 ↗
18. 10.1016/S0376-7388(01)00661-510.1016/S0376-7388(01)00661-5 ↗
19. 10.1016/j.seppur.2011.05.02010.1016/j.seppur.2011.05.020 ↗
20. Hull D · An Introduction to Composite Materials · 1981
21. 10.1007/978-1-4757-3912-110.1007/978-1-4757-3912-1 ↗
22. 10.1016/j.memsci.2007.05.01510.1016/j.memsci.2007.05.015 ↗
23. 10.1016/j.desal.2006.03.14410.1016/j.desal.2006.03.144 ↗
24. 10.1016/j.clay.2009.12.01110.1016/j.clay.2009.12.011 ↗
25. 10.4028/www.scientific.net/MSF.660-661.108110.4028/www.scientific.net/MSF.660-661.1081 ↗
26. 10.1016/j.polymertesting.2015.08.01010.1016/j.polymertesting.2015.08.010 ↗
27. 10.1016/0376-7388(91)85016-X10.1016/0376-7388(91)85016-X ↗