Investigation of Cu particles size and bonding time on the microstructure and shear property of Cu/In-45Cu/Cu solder joints
Source abstract
Abstract
Abstract The effect of Cu particles size and bonding time on the microstructure and shear property of Cu/In-45Cu/Cu solder joint was studied, and the shedding mechanism of intermetallic compounds (IMCs) in the solder joint during transient liquid phase (TLP) bonding process was investigated. The results showed that the microstructure of Cu/In-45Cu/Cu solder joint was composed of Cu11In9 phase, residual In phase and Cu particles, and the microstructure of solder joints prepared by small Cu particles was dense. The content of IMCs was increased with increasing bonding time, and the Cu/In-45Cu/Cu solder joint was composed of Cu11In9 phase and Cu particles under bonding time 30 min. The Cu2In phase was formed in the solder joint at 60 min, and many cracks appeared at the interface of Cu11In9 and Cu2In phases. The shear strength of Cu/In-45/Cu solder joints with brittle fracture was increased firstly and then decreased with increasing bonding time, and the maximum shear strength of the solder joint was 16.35 MPa at 30 min.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Multifunctional wearable smart device based on conductive reduced graphene oxide/polyester fabric10.1016/j.apsusc.2018.05.127 ↗
2. Effect of different amount of silicon carbide on SAC Solder-Cu joint performance by using microwave hybrid heating method10.1088/1757-899X/469/1/012110 ↗
3. Effect of processing variables on the mechanical reliability of copper pillar SnAg solder joints10.1109/ECTC.2017.250 ↗
4. Effect of bonding time and homogenization heat treatment on the microstructure and mechanical properties of the transient liquid phase bonded dissimilar GTD-111/FSX-414 TLP superalloys10.1016/j.jallcom.2017.10.105 ↗
5. Effect of CuZnAl particles addition on microstructure of Cu/Sn58Bi/Cu TLP bonding solder joints10.1016/j.vacuum.2019.06.024 ↗
6. Effect of pulsed current on the microstructure evolution of Cu-Sn intermetallic compounds10.1080/02670836.2017.1348652 ↗
7. IMC growth and shear strength of Sn–Ag–Cu/Co–P ball grid array solder joints under thermal cycling10.1007/s10854-014-2489-7 ↗
8. Effects of Mn nanoparticles on tensile properties of low-Ag Sn-0.3Ag-0.7Cu-xMn solder alloys and joints10.1016/j.jallcom.2017.05.182 ↗
9. Effect of Ni addition on the wettability and microstructure of Sn2.5Ag0.7Cu0.1RE solder alloy10.1016/j.matdes.2017.01.046 ↗
10. Influence of Ce addition on Sn-3.0Ag-0.5Cu solder joints: thermal behavior, microstructure and mechanical properties10.1016/j.jallcom.2016.12.191 ↗
11. Properties and interfacial microstructure of Sn–Zn–Ga solder joint with rare earth Pr addition10.1016/j.matdes.2012.10.034 ↗
12. Impact toughness, hardness and shear strength of Fe and Bi added Sn-1Ag-0.5Cu lead-free solders10.1016/j.microrel.2016.05.004 ↗
13. Solderability, IMC evolution, and shear behavior of low-Ag Sn0.7Ag0.5Cu-BiNi/Cu solder joint10.1007/s10854-012-0649-1 ↗
14. Influence of small addition of antimony (Sb) on thermal behavior, microstructural and tensile properties of Sn-9.0Zn-0.5Al Pb-free solder alloy10.1016/j.msea.2017.06.092 ↗
15. Effect of iron and indium on IMC formation and mechanical properties of lead-free solder10.1016/j.msea.2012.05.086 ↗
16. Influences of Ag addition to Sn-58Bi solder on SnBi/Cu interfacial reaction10.1016/j.matlet.2017.11.127 ↗
17. Microstructural evolution and joint strength of Sn-58Bi/Cu joints through minor Zn alloying substrate during isothermal aging10.1016/j.jallcom.2016.07.084 ↗
18. Abnormal Intermetallic Compound Evolution in Ni/Sn/Ni and Ni/Sn-9Zn/Ni Micro Solder Joints Under Thermomigration10.1007/s11664-016-5149-2 ↗
19. Enhancing the microstructure and tensile creep resistance of Sn-3.0Ag-0.5Cu solder alloy by reinforcing nano-sized ZnO particles10.1016/j.microrel.2017.07.034 ↗
20. Study of the oxidation effects on isothermal solidification based high temperature stable Pt/In/Au and Pt/In/Ag thick film interconnections on LTCC substrate
21. Behavior of eutectic Sn-Bi powder in Cu nanoparticle joints during the thermal treatment10.1007/s10854-017-6602-6 ↗
22. Strong coupling effects during Cu/In/Ni interfacial reactions at 280 °C10.1016/j.intermet.2014.12.002 ↗
23. Sequential interfacial reactions of Au/In/Au transient liquid phase-bonded joints for power electronics applications10.1016/j.tsf.2018.04.039 ↗
24. Phase transformation and fracture behavior of Cu/In/Cu joints formed by solid-liquid interdiffusion bonding10.1007/s10854-014-2145-2 ↗
25. Wetting and reaction of Sn-2.8Ag-0.5Cu-1.0Bi solder with Cu and Ni substrates10.1007/s11664-005-0239-6 ↗
26. Rapid formation of superhydrophobic surfaces with fast response wettability transition10.1021/am100808v ↗
27. Effect of phosphorus content on Cu/Ni–P/Sn-3.5Ag solder joint strength after multiple reflows10.1007/s11664-006-0322-7 ↗
28. Wettability and strength of In–Bi–Sn lead-free solder alloy on copper substrate10.1016/j.jallcom.2010.07.182 ↗
29. Direct integration of the collisionless boltzmann equation in, six-dimensional phase space: self-gravitating systems10.1016/j.jallcom.2006.07.125 ↗
30. Formation and growth of intermetallic phases in diffusion soldered Cu/In–Bi/Cu interconnections10.1016/j.jallcom.2008.09.045 ↗
31. Influence of indium addition on electromigration behavior of solder joint10.1557/jmr.2011.283 ↗
32. A new compound in the Cu–In system-the synthesis and structure of Cu10In710.1002/zaac.200800275 ↗
33. Reliability enhancement of Sn-1.0Ag-0.5Cu nano-composite solders by adding multiple sizes of TiO2 nanoparticles10.1016/j.jallcom.2016.12.037 ↗
34. In-situ atomic-scale studies of the mechanisms and dynamics of metal dissolution by high-speed STM10.1016/S0013-4686(01)00654-5 ↗
35. Wetting and non-wetting near critical points in solids10.1016/S0378-4371(99)00513-0 ↗
36. Reversible ‘Wetting’ of grain boundaries by the second solid phase in the Cu–In system10.1134/S0021364014200107 ↗
37. Reinforcement of vanadium on the microstructure and properties of Sn-58Bi lead-free solder joints10.1088/2053-1591/ab07f6 ↗