Effect of Al-Sr-Y intermediate alloy on microstructure and mechanical properties of A356 alloy

Zhongyue Huang, Jing Li, Changwen Yuan, Qihang Wang, Feng Yan, Fangqiu Zu

Materials Research Express· Volume 11· Issue 3

Abstract

Abstract In this experiment, an intermediate alloy (Al-3Sr-8Y) that can refine and modify A356 alloy simultaneously was developed, and the synergistic effect of Sr and Y on the microstructure and mechanical properties of A356 alloy was investigated. The results show that when the content of Al-3Sr-8Y intermediate alloy reaches 0.3 wt%, the morphology of α-Al dendrites is significantly refined and the secondary dendrite arm spacing (SDAS) was significantly reduced. Moreover, the morphology of eutectic Si transforms from acicular to small fibrous, and the average area and aspect ratio of eutectic Si decrease to 0.81 μm2, and 2.01. This change is caused by the twin plane re-entrant edge (TPRE) poisoning mechanism, where the addition of Al-3Sr-8Y can poison the intrinsic growth position of the Si phase, reduce the growth rate of the Si phase, promote isotropic growth, and achieve a highly branched morphology of the Si phase to form a fibrous structure. Due to the excellent synergistic effect of Sr and Y, the tensile strength and elongation of the alloy reached the maximum values of 303.5 MPa and 9.5% when 0.3 wt% Al-3Sr-8Y was added after heat treatment, which is an increase of 18.2% and 86.3% compared with the untreated A356 alloy, respectively.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Numerical prediction of fatigue life of an A356-T6 alloy wheel considering the influence of casting defect and mean stress10.1016/j.engfailanal.2020.104903 ↗
2. Review of high-strength aluminium alloys for additive manufacturing by laser powder bed fusion10.1016/j.matdes.2022.110779 ↗
3. Selective laser melting of 7075 aluminum alloy inoculated by Al–Ti–B: Grain refinement and superior mechanical properties10.1016/j.vacuum.2022.111030 ↗
4. Microstructure and mechanical properties of as-cast and T6 treated Sc modified A356-5TiB2 in situ composite - sciencedirect10.1016/j.msea.2018.10.080 ↗
5. Microstructure and mechanical properties of in situ nano γ-Al2O3p/A356 aluminum matrix composite10.1016/j.jallcom.2019.02.045 ↗
6. Grain refinement of pure aluminium and Al–7Si with Al–3B master alloy10.1179/1743284711Y.0000000041 ↗
7. The microstructure and compressive properties of aluminum alloy (A356) foams with different Al-Ti-B additions10.5755/j01.ms.22.3.8559 ↗
8. Microstructural features of as-cast A356 alloy inoculated with Sr, Sb modifiers and Al–Ti–C grain refiner simultaneously10.1016/j.matlet.2007.05.020 ↗
9. Nucleation and growth of eutectic Si in Al-Si alloys with na addition10.1007/s11661-014-2702-6 ↗
10. The role of strontium in modifying aluminium-silicon alloys10.1016/j.actamat.2012.03.031 ↗
11. Modification of eutectic Si in Al–Si alloys with Eu addition10.1016/j.actamat.2014.10.064 ↗
12. The microstructure and crystallography of aluminium-silicon eutectic alloys10.1098/rspa.1968.0128 ↗
13. The mechanism of silicon modification in aluminum-silicon alloys: Impurity induced twinning10.1007/BF02646204 ↗
14. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al–7.5Si–0.5 Mg alloy10.1016/j.matdes.2010.08.040 ↗
15. Al–9.00%Si–0.25%Mg alloys modified by ytterbium10.1007/s12598-014-0378-0 ↗
16. Effect of strontium modification on porosity formation in A356 alloy10.1007/s40962-018-00300-1 ↗
17. Mutual poisoning effect between Sr and B in Al–Si casting alloys10.1016/S1359-6462(02)00648-6 ↗
18. A mechanism for the poisoning effect of silicon on the grain refinement of Al–Si alloys10.1016/j.actamat.2006.09.046 ↗
19. Effect of the addition of La and Ce on the solidification behavior of Al–Cu and Al–Si–Cu Cast Alloys10.1007/s40962-019-00351-y ↗
20. The use of rare earth metals in Al–Si–Cu casting alloys10.1007/s40962-021-00640-5 ↗
21. Influence of strontium and lanthanum simultaneous addition on microstructure and mechanical properties of the secondary Al-Si-Cu-Fe alloy10.1016/S1002-0721(17)60938-4 ↗
22. Solidification behavior and microstructure of Al-7Si alloys with individual and combined additions of Sr and Yb10.1155/2019/9750526 ↗
23. Utilizing a novel modifier to realize multi-refinement and optimized heat treatment of A356 alloy10.1016/j.jallcom.2019.03.327 ↗
24. The effects of Y on primary α-Al and precipitation of hypoeutectic Al-Si alloy10.1016/j.matlet.2020.127795 ↗
25. Effects of yttrium and heat treatment on the microstructure and tensile properties of Al–7.5 Si–0.5 Mg alloy10.1016/j.matdes.2010.08.040 ↗
26. Study on microstructure and mechanical properties of ZL107 alloy added with yttrium10.1016/S1002-0721(12)60258 ↗
27. Investigation on the modification behavior of A356 alloy inoculated with a Sr-Y composite modifier10.1016/S1002-0721(12)60259-2 ↗
28. The role of strontium in modifying aluminium–silicon alloys10.1016/j.actamat.2012.03.031 ↗
29. Solute adsorption and entrapment during eutectic Si growth in A–Si-based alloys10.1016/j.actamat.2014.09.040 ↗
30. Effect of Sc and Sr on the eutectic Si morphology and tensile properties of Al-Si-Mg alloy10.1007/s11665-017-2599-5 ↗
31. Synergistic effect of Sr and La on the microstructure and mechanical properties of A356. 2 alloy10.1016/j.matdes.2016.10.061 ↗
32. The effect of scandium addition on microstructure and mechanical properties of Al–Si–Mg alloy: a multi-refinement modifier10.1016/j.matchar.2015.10.030 ↗
33. Nano-yttrium-containing precipitates of T6 heat-treated A356. 2 alloy when trace yttrium (Y less than 0.100 wt%) added10.1007/s12598-020-01671-3 ↗
34. Microstructure and mechanical properties of A356 alloy with yttrium addition processed by hot extrusion10.1016/j.jre.2018.11.008 ↗
35. Effect of trace yttrium addition and heat treatment on the microstructure and mechanical properties of as-cast ADC12 aluminum alloy10.3390/app9010053 ↗
36. Effect of alloy composition on the dendrite arm spacing of multicomponent aluminum alloys10.1007/s11661-010-0183-9 ↗
37. Last-stage solidification of alloys: Theoretical model of dendrite-arm and grain coalescence10.1007/978-3-662-07969-0_16 ↗
38. Effects of Sr, Ce and P on the microstructure and mechanical properties of rapidly solidified Al7Si alloys10.1016/j.matchar.2018.04.018 ↗
39. The heat treatment of Al–Si–Cu–Mg casting alloys10.1016/j.jmatprotec.2010.03.020 ↗
40. Effect of hot extrusion on mechanical properties and microstructure of near eutectic Al-12.0%Si-0.2%Mg alloy. materials science & engineering, a. structural10.1016/j.msea.2010.07.068 ↗