journal article·2021-05-01Open access

Synthesis of bulk nanostructured Mg-based alloy via spark plasma sintering through in situ crystallization of an amorphous precursor

Song-Yi Kim, Hyeon-Ah Kim, A-Young Lee, Do-Hyang Kim, Hyunkyu Lim, Min-Ha Lee

Materials Research Express· Volume 8· Issue 5

Abstract

Abstract We present the synthesis of a bulk nanostructured Mg-based alloy that has a grain size less than 300 nm. A nanostructured Mg-Zn-Cu-Nd alloy with an exceptionally high hardness can be obtained through simultaneous consolidation and in situ crystallization of the amorphous Mg84Zn7Cu3Nd6 alloy precursor using the spark plasma sintering process. We evaluate the relationship between the microstructure and preparation conditions on the grain size of nanostructured Mg-based alloys during the sintering process. The hardness of the bulk sample produced from the sintered amorphous Mg-Zn-Cu-Nd precursor at 260 °C is maximized via the nanocrystallization of intermetallic compounds using the sintering process. The populated crystallization and confined growth of phases contribute to the refinement of gains in nanostructured Mg-based alloys.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Metallic Glasses and Amorphous Alloys · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Novel hexagonal structure and ultrahigh strength of magnesium solid solution in the Mg-Zn-Y system10.1557/JMR.2001.0260 ↗
2. Physical properties of the multifunctional Mg80Ni10Gd10 alloy10.1016/j.msea.2017.01.085 ↗
3. Improved mechanical property and internal friction of pure Mg processed by ECAP10.1016/j.msea.2012.07.031 ↗
4. Optimizing the strength and ductility of AZ91 Mg alloy by ECAP and subsequent aging10.1016/j.msea.2013.09.052 ↗
5. Influence of mechanically milled powder and high pressure on spark plasma sintering of Mg-Cu-Gd metallic glasses10.1016/j.actamat.2013.04.011 ↗
6. Preparing Mg-Ni-Si amorphous powders by mechanical alloying and consolidation by pulsed current sintering10.1016/j.msea.2003.10.150 ↗
7. Mg-based amorphous alloys10.1016/0921-5093(93)90175-E ↗
8. Electron-band theory inspired design of magnesium-precious metal bulk metallic glasses with high thermal stability and extended ductility10.1038/s41598-017-03643-7 ↗
9. Increase of mechanical strength of a Mg85Zn12Ce3 amorphous alloy by dispersion of ultrafine hcp-Mg particles10.2320/matertrans1989.32.875 ↗
10. AE42 magnesium alloy prepared by spark plasma sintering10.1016/j.jallcom.2018.01.115 ↗
11. Synthesis of nanostructures from amorphous and crystalline phases10.1016/j.msea.2003.10.164 ↗
12. High strength nanostructured Al-based alloys through optimized processing of rapidly quenched amorphous precursors10.1038/s41598-018-19337-7 ↗
13. Hybrid nanostructured aluminum alloy with super-high strength10.1038/am.2015.129 ↗
14. Mg-based bulk metallic composites with plasticity and gigapascal strength10.1016/j.actamat.2004.12.036 ↗
15. New amorphous alloys with high strength and good bend ductility in the Mg-Ni-Nd system10.1016/0924-0136(94)01687-V ↗
16. Experimental determination of the phase equilibria of the Mg-Nd-Zn system at 320 °C10.1016/j.jallcom.2014.02.131 ↗
17. Formation of Mg-Cu-Zn-Y bulk metallic glasses with compressive strength over gigapascal10.1016/j.jallcom.2006.12.101 ↗
18. MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants10.1038/nmat2542 ↗
19. Ductile biodegradable Mg-based metallic glasses with excellent biocompatibility10.1002/adfm.201203738 ↗
20. Microstructure, corrosion resistance and cytocompatibility of Mg-5Y-4rare earth-0.5Zr (WE54) alloy10.1016/j.msec.2012.01.003 ↗
21. Synthesis of bulk amorphous composites with three amorphous phases by consolidation of milled amorphous powders10.1016/j.intermet.2010.03.040 ↗
22. Mechanical behavior of metallic glass reinforced nanostructured by spark plasma sintering10.1016/j.intermet.2010.03.032 ↗
23. Optimizing the magnetic properties of Fe-based amorphous powder by adjusting atomic structures from vitrification at different temperatures10.1063/1.5116843 ↗
24. Thermodynamics of rare earths in steelmaking10.1007/BF02652708 ↗
25. Effect of cerium addition on microstructure and mechanical properties of high-strength Fe85Cr4Mo8V2C1 cast steel10.1016/j.msea.2016.07.114 ↗
26. Room-temperature creep and structural relaxation of Mg-Cu-Y metallic glasses10.1016/j.actamat.2008.04.021 ↗
27. On the plastic flow beneath a blunt axisymmetric indenter10.1115/1.3427786 ↗
28. Selection thickness, macrohardness and yield strength in high-pressure diecast magnesium alloy AZ9110.1016/j.msea.2005.04.024 ↗
29. Study of mechanical deformation in bulk metallic glass through instrumented indentation10.1016/S1359-6454(01)00263-4 ↗
30. Novel heating-induced reversion during crystallization of Al-based glassy alloys10.1038/srep46113 ↗
31. Effect of geometrical constraint condition on the formation of nanoscale twins in the Ni-bsed metallic glass composite10.1080/09500839.2014.907509 ↗
32. Deformation behavior of a Ni59Zr20Ti16Si2Sn3 metallic glass matrix composite reinforced by copper synthesized by warm extrusion of powders10.1016/j.jnoncrysol.2004.03.107 ↗