Abstract The changes in intermetallic phases of Mg-6%Al-5%Pb (Mg-Al-Pb) alloy prepared by powder metallurgy and their effects on electrochemical properties were studied. Experimental results showed that coarse Mg17Al12 phases (with size ranges from 20 μm to 70 μm) and fine Mg2Pb phases (with the size of 100 nm scale) formed in the mixed Al, Pb and Mg powder during the hot press sintering procedure. Fine Mg2Pb phases exhibit strong diffusional ability to diffuse into Mg17Al12 phases. Extruding further promotes the diffusion of Mg2Pb phases into Mg17Al12 phases. Solution treatment produced a mixed microstructure which is Mg17Al12 phase containing Mg2Pb phases inside and made other Mg2Pb phases homogeneously distributed in Mg matrix. Mg17Al12 phases and the gathered Mg2Pb phases will accumulate the Mg(OH)2 corrosion products, which impedes the subsequent discharge behavior. Homogeneously distributed Mg2Pb phases will fall off during discharge, which makes the discharge curve more stable. The mixed microstructure has positive effect on corrosion resistance and discharge potential. Therefore, solution-treated alloy shows the highest negative potential and the smoothest curve during the galvanostatic discharge test. Compared with the commercial AZ61 sheet, solution-treated alloy exhibit much higher anode properties in Mg/PbCl2 battery test. Thus, the solution-treated alloy could serve as an excellent anode in seawater-activated batteries.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Practical application of a sea-water battery in deep-sea basin and its performance10.1016/j.jpowsour.2008.10.105 ↗
2. Microstructure effects on the electrochemical corrosion properties of Mg-4.1%Ga-2.2%Hg alloy as the anode for seawateractivated batteries10.1016/j.corsci.2011.01.040 ↗
3. Development of a seawater battery for deep-water applications10.1016/S0378-7753(96)02483-4 ↗
4. Composition optimization and electrochemical properties of Mg-Al-Pb-(Zn) alloys as anodes for seawater activated battery10.1016/j.electacta.2016.02.088 ↗
5. Performance of Mg-14Li-1Al-0.1Ce as anode for Mg-air battery10.1016/j.jpowsour.2010.07.097 ↗
6. Influence of allotropic modifications of sulphur on the cell voltage in Mg-CuI(S) seawater activated battery10.1016/S0254-0584(99)00022-X ↗
7. Influence of Ga and Hg on microstructure and electrochemical corrosion behavior of Mg alloy anode materials10.1016/S1003-6326(07)60278-7 ↗
8. AgCl and Ag2S as additives to CuI in Mg-CuI seawater activated batteries10.1023/A:1018481314511 ↗
9. Electrochemical oxidation behavior of Mg-Li-Al-Ce-Zn and Mg-Li-Al-Ce-Zn-Mn in sodium chloride solution10.1016/j.jpowsour.2008.06.005 ↗
10. Influence of aluminium and lead on activation of magnesium as anode10.1016/S1003-6326(09)60312-5 ↗
11. An exploratory study of the corrosion of Mg alloys during interrupted salt spray testing10.1016/j.corsci.2009.03.014 ↗
12. Influence of microstructure on the corrosion of diecast AZ91D10.1016/S0010-938X(98)00121-8 ↗
13. In vitro corrosion and biocompatibility of binary magnesium alloys10.1016/j.biomaterials.2008.10.021 ↗
14. Influence of the β phase on the corrosion performance of anodised coatings on magnesium-aluminium alloys,10.1016/j.corsci.2004.11.004 ↗
15. Discharge performance of Mg-Al-Pb-La anode for Mg-air battery10.1016/S1003-6326(18)64872-1 ↗
16. Phase diagrams of Pb-free solders and their related materials systems10.1007/s10854-006-9010-x ↗
17. Structural analysis of Al-Ce compound phase in AZ-Ce cast magnesium alloy10.1016/j.jmrt.2019.07.042 ↗
18. Powder metallurgy science
19. Synthesis, microstructure and mechanical properties of porous Mg-Zn scaffolds10.1016/j.jmbbm.2013.01.023 ↗
20. Microstructure, mechanical properties, biocorrosion behavior, and cytotoxicity of as-extruded Mg-Nd-Zn-Zr alloy with different extrusion ratios10.1016/j.jmbbm.2012.02.002 ↗
21. The effect of surface modification on the corrosion protection ability of the passive films of sensitized UNS S31803 duplex stainless steel10.1080/1478422X.2018.1556865 ↗
22. Corrosion of pure Mg as a function of grain size and processing route10.1002/adem.200800046 ↗
23. Corrosion behavior of as-cast Pb-Mg-Al alloys in 3.5% NaCl solution10.5006/0570 ↗
24. Corros. eng., corrosion of novel Pb-Mg-Al-B nuclear shielding alloy in fluoride medium
25. Effects of yttrium on the microstructure and corrosion behavior of Pb-39Mg-10Al-1B-Y alloys10.1007/s11665-020-05317-4 ↗
26. Microstructures and electrochemical corrosion properties of Mg-Al-Pb and Mg-Al-Pb-Ce anode materials10.1016/S1003-6326(16)64242-5 ↗
27. Enhancement of mechanical properties and corrosion resistance of Mg-Ca alloys through microstructural refinement by indirect extrusion10.1016/j.corsci.2014.01.041 ↗
28. In vitro degradation performance and biological response of a Mg-Zn-Zr alloy,10.1016/j.mseb.2011.05.032 ↗
29. Evaluating the performance of zinc and aluminum sacrificial anodes in artificial seawater10.1016/j.electacta.2019.05.067 ↗
30. Corrosion behavior of equal-channel-angular-pressed pure magnesium in NaCl aqueous solution10.1016/j.corsci.2009.10.004 ↗
31. Performance of Al-1Mg-1Zn-0.1Ga-0.1Sn as anode for Al-air batter10.1016/j.electacta.2014.02.080 ↗
32. The corrosion behaviour of Al-Zn-In-Mg-Ti alloy in NaCl solution, X. V. Chunhua10.1016/j.corsci.2009.10.010 ↗
33. Effect of grain size and twins on corrosion behaviour of AZ31B magnesium alloy10.1016/j.corsci.2009.10.018 ↗
34. Discharge and corrosion performance of AP65 magnesium alloy in simulated seawater: effect of temperature10.1007/s11665-014-1222-2 ↗