On the miscibility gap at 800 K in the Fe-Cr alloy system
Source abstract
Abstract
Issues pertinent to the miscibility gap at 800 K in a Fe 73.7 Cr 26.3 alloy viz. the kinetics of the phase decomposition and borders of the latter were investigated by means of the Mössbauer-effect spectroscopy. The kinetics was revealed to well follow the Johnson-Mehl-Avrami-Kolgomarov equation testifying to a nucleation and growth mechanism underlying the decomposition. A solubility limit of Cr in the Fe matrix was determined to be 17.3(6) at% and that of Fe in the Cr matrix was found as equal to 18.5(9) at%. The results obtained have been compared with various theoretical predictions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical and Alloy Processes · Microstructure and Mechanical Properties of Steels · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. 10.1080/1040843100378847210.1080/10408431003788472 ↗
2. 10.1016/0364-5916(87)90021-610.1016/0364-5916(87)90021-6 ↗
3. 10.1007/s11669-010-9782-910.1007/s11669-010-9782-9 ↗
4. 10.1016/j.calphad.2011.05.00210.1016/j.calphad.2011.05.002 ↗
5. 10.1016/j.jnucmat.2016.11.01710.1016/j.jnucmat.2016.11.017 ↗
6. 10.1016/j.calphad.2017.10.00210.1016/j.calphad.2017.10.002 ↗
7. 10.2320/matertrans1960.26.47310.2320/matertrans1960.26.473 ↗
8. 10.1016/j.matchemphys.2013.05.02310.1016/j.matchemphys.2013.05.023 ↗
9. 10.1016/j.matchemphys.2013.05.02310.1016/j.matchemphys.2013.05.023 ↗
10. 10.1016/j.matchar.2017.05.01710.1016/j.matchar.2017.05.017 ↗
11. 10.1016/0304-8853(81)90137-210.1016/0304-8853(81)90137-2 ↗
12. 10.1016/0168-583X(91)95681-310.1016/0168-583X(91)95681-3 ↗
13. Guy A G · Introduction to Materials Science · 1972 · 338