Cobalt spinel CoAl2O4 via sol-gel process: elaboration and surface properties

S Chemlal, A Larbot, M Persin, J Sarrazin, M Sghyar, M Rafiq

Materials Research Bulletin· Volume 35· Issue 14-15
Publisher page

Abstract

Abstract In this work the preparation of cobalt spinel CoAl2O4 is described. The technique of colloidal solution destabilization was used as the sol-gel process. The powder obtained from the dried gel was characterized by thermal analysis (thermogravimetric and differential), X-ray diffraction, infrared spectroscopy, and specific surface area measurement. Crystallization of CoAl2O4 spinels occurs at about 400°C. The study of surface properties (surface charge and electrophoretic mobility) of the spinel powder fired at 600°C, in suspension in different electrolyte solutions (10−3 molar ionic strength), shows that the spinel material charge depends on the pH of the solution. The spinel sol was used for the preparation of membrane by the slip-casting method.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Pigment Synthesis and Properties · Nanomaterials for catalytic reactions · Advanced Photocatalysis Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (7)

Show source-provided references
1. P. Pascal, Nouveau Traité de Chimie Minérale, Masson, Paris, 1961, Vol. 6, p. 596.
2. Chokkaram · J Mol Catal A Chem · 1997 · 121 · 15710.1016/S1381-1169(97)00018-6 ↗
3. Meyer · J Mater Chem · 1999 · 9 · 175510.1039/a900014c ↗
4. C. Otero Areàn, M. Peñarroya Mentruit, E. Escalona Platero, F.X. Llabrés i Xamena, J.B. Parra, Mater Lett 39 (1999) 22.10.1016/S0167-577X(98)00209-2 ↗
5. Erokhina · Russ J Inorg Chem · 1979 · 24 · 500
6. Brunauer · J Am Chem Soc · 1938 · 60 · 30910.1021/ja01269a023 ↗
7. Onoda · 1984 · 374