Abstract
Abstract Strontium molybdate (SrMoO4) compound is synthesized using a solid-state reaction route. SrMoO4 was observed to form in tetragonal Scheelite structure with I41/a space group and is confirmed with the help of powder X-ray diffraction studies. The temperature-dependent dielectric constant measured at different frequencies indicated a maximum at around 795 K. The frequency-dependent dielectric maximum reveals the presence of a dielectric relaxation near 795 K. Further, the Nyquist plot analysis shows a depressed semi-circle and manifest the non-Debye type dielectric relaxation in SrMoO4. The SrMoO4 compound possesses a negative temperature coefficient of resistance and is confirmed by fitting the Nyquist plot with a suitable equivalent circuit. The AC conductivity studies ascertain that the observed conduction mechanism in the SrMoO4 as a translational type correlated barrier hopping. The temperature-dependent AC conductivity reveals that the obtained activation energies are comparable with the oxygen vacancies and are responsible for observed dielectric relaxation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Magnetic and transport properties of perovskites and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Dielectric materials for applications in microwave communications10.1039/b003681l ↗
2. Transport properties of materials with the scheelite structure and their modification by doping10.1007/BF02388670 ↗
3. NaY(MoO4)2:Eu3+ and NaY0.9Bi0.1(MoO4)2:Eu3+ submicrometer phosphors: hydrothermal synthesis assisted by room temperature-solid state reaction, microstructure and photo10.1016/j.matchemphys.2009.02.042 ↗
4. Anisotropy of optical properties of scheelite tungstates in the fundamental absorption region10.1016/S0168-9002(01)01077-4 ↗
5. Low-temperature sintering of Ba0.5Sr0.5TiO3-SrMoO4 dielectric tunable composite ceramics for LTCC applications10.1007/s11664-013-2621-0 ↗
6. Synthesis and luminescence properties of a novel red SrMoO4:Sm3+, R+ phosphor10.1016/j.solidstatesciences.2010.12.029 ↗
7. Luminescent properties of Dy3+ doped SrMoO4 phosphor10.1016/j.jlumin.2011.01.015 ↗
8. Microwave dielectric properties of scheelite (A = Ca, Sr, Ba) and wolframite (A = Mg, Zn, Mn) AMoO4 compounds10.1016/j.jeurceramsoc.2006.11.037 ↗
9. Microwave dielectric properties of tunable Ba0.5Sr0.5TiO3 and scheelite AMoO4 composite ceramics10.1016/j.jallcom.2012.10.189 ↗
10. Infrared spectra, Raman spectra, microwave dielectric properties and simulation for effective permittivity of temperature stable ceramics AMoO4-TiO2 (A = Ca, Sr)10.1039/C2DT31878D ↗
11. Structural, lattice vibrational, optical and microwave dielectric studies on Ca1-xSrxMoO4 ceramics with scheelite structure10.1016/j.materresbull.2014.04.064 ↗
12. Optical and dielectric properties of SrMoO4 powders prepared by the combustion synthesis method10.12989/amr.2012.1.3.191 ↗
13. Vibrational and XRD Study of the System CdWO4−CdMoO410.1021/jp963008x ↗
14. Concerning the high pressure allotropic modification of cerium10.1103/PhysRev.76.301 ↗
15. Critical behavior of the mott transition in Cr-doped V2O310.1103/PhysRevB.2.3751 ↗
16. Pressure induced isostructural and structural transitions in ThAl210.1016/S0921-4526(96)00483-8 ↗
17. An unusual temperature induced isostructural phase transition in a scheelite, Li0.5Ce0.5MoO410.1039/c3dt33033h ↗
18. Temperature-induced isostructural phase transition on NaCe(MoO4)2 system: a Raman scattering study10.1016/j.saa.2018.10.017 ↗
19. Effect of W doping on phase transition behavior and dielectric relaxation of CuMoO4 obtained by a modified sol-gel method10.1088/2053-1591/ab6546 ↗
20. Structural, dielectric, and thermal properties of pb free molybdate based ultralow temperature glass10.1021/acssuschemeng.6b00721 ↗
21. Impedance spectroscopy of Bi3.25La0.75Ti3O12 ceramics above and below ferroelectric transition temperatures10.1088/0022-3727/40/2/037 ↗
22. Impedance spectroscopy study of polycrystalline Bi6Fe2Ti3O1810.1007/BF02707799 ↗
23. Impedance spectroscopic analysis of the organic ferroelectric-diisopropylammonium bromide (DIPAB)10.1016/j.cap.2014.02.018 ↗
24. Impedance and modulus spectroscopy of semiconducting BaTiO3 showing positive temperature coefficient of resistance10.1063/1.344049 ↗
25. Electrical conductivity and impedance spectroscopy studies of cerium based aeschynite type semiconducting oxides: CeTiMO6 (M=Nb or Ta)10.1063/1.3481389 ↗
26. Frequency-dependent loss in amorphous semiconductors10.1080/00018738200101418 ↗
27. Transport properties of vanadium germanate glassy semiconductors10.1103/PhysRevB.42.5665 ↗
28. AC conduction in iron bismuthate glassy semiconductors10.1103/PhysRevB.42.1388 ↗
29. On the frequency dependence of conductivity in amorphous solids
30. AC conductivity of scandium oxide and a new hopping model for conductivity10.1103/PhysRevB.6.1572 ↗
31. Impedance spectroscopy of multiferroic PbZrxTi1−xO3∕CoFe2O4 layered thin films10.1103/PhysRevB.77.014111 ↗
32. Relations between the concentrations of imperfections in crystalline solids10.1016/S0081-1947(08)60135-6 ↗
33. X-ray, SEM and dielectric studies of Gd-modified sol–gel-prepared lead zirconate–lead titanate solid solution10.1016/S0167-577X(99)00027-0 ↗
34. Frequency-temperature response of ferroelectromagnetic Pb(Fe1∕2Nb1∕2)O3 ceramics obtained by different precursors. Part I. Structural and thermo-electrical characterization10.1063/1.1870099 ↗
35. AC conductivity in Gd doped Pb(Zr0.53Ti0.47)O3 ceramics10.1063/1.2988264 ↗
36. Dielectric properties and ac-conductivity analysis of Bi3.25La0.75Ti3O12 ceramic using impedance spectroscopy10.1016/j.jpcs.2007.09.004 ↗