Hot corrosion behaviour of Ti–Al based intermetallics

Kai Zhang, Zhengwei Li, Wei Gao

Materials Letters· Volume 57· Issue 4
Publisher page

Abstract

Three types of hot corrosion tests were performed on TiAl-based intermetallics Ti–48Al, Ti–Ti–52Al and 48Al–2Cr (at.%). The salt mixture that was used in the present hot corrosion study consists of 80 wt.% Na2SO4+20 wt.% NaCl, with a melting point of ∼700 °C. The specimens were either suspended in the salt vapour, deposited with the mixed salt, or immersed in the molten salt, all at 800 °C. These testing methods represent different service conditions, and produced different results. However, these results are consistent in ranking the hot corrosion properties of materials. Electron microscopy and X-ray diffraction (XRD) were used to study the morphology and compositions of the corrosion products. The mechanisms of hot corrosion have also been discussed based on the experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Fores · J. Mater. Sci. · 1992 · 27 · 511310.1007/BF02403806 ↗
2. Austin · 1993 · 143
3. Huang · Metall. Trans. · 1991 · 22A · 42710.1007/BF02656810 ↗
4. Stringer · Mater. Sci. Technol. · 1987 · 3 · 48310.1080/02670836.1987.11782259 ↗
5. Rapp · Corrosion · 1986 · 42 · 56810.5006/1.3583026 ↗
6. Kim · JOM · 1989 · 42 · 2410.1007/BF03220267 ↗
7. Kim · JOM · 1995 · 47 · 3810.1007/BF03221228 ↗
8. Craig · 1989
9. Z. Li, W. Gao, Corrosion, oxidation and mechanical properties of titanium, titanium alloys and titanium composites, An Internal Report, The University of Auckland (2000) .
10. Birks · 1983
11. Zhu · 1995
12. Tang · Mater. Sci. Eng. · 2000 · 276 · 7010.1016/S0921-5093(99)00513-4 ↗
13. Tang · Intermetallics · 1999 · 7 · 127110.1016/S0966-9795(99)00044-8 ↗
14. Tang · Chin. Soc. Corros. Prot. · 1997 · 17 · 233
15. Guan · Corros. Sci. Prot. Technol. · 2000 · 12 · 134
16. Haanappel · Oxid. Met. · 1997 · 48 · 26310.1007/BF01670503 ↗
17. Takahashi · J. Eur. Ceram. Soc. · 1998 · 18 · 112110.1016/S0955-2219(98)00007-7 ↗
18. Yao · Mater. Sci. Eng. · 1995 · 192/193 · 99410.1016/0921-5093(95)03345-9 ↗
19. Hara · J. Jpn. Inst. Met. · 1999 · 63 · 123810.2320/jinstmet1952.63.10_1238 ↗
20. Tang · Oxid. Met. · 1999 · 51 · 23510.1023/A:1018818622547 ↗
21. Oxidation and Corrosion of Intermetallic Alloys
22. Copland · Acta Mater. · 1999 · 47 · 293710.1016/S1359-6454(99)00169-X ↗
23. Brady · Acta Mater. · 1997 · 45 · 235710.1016/S1359-6454(96)00362-X ↗
24. Brady · Acta Mater. · 1997 · 45 · 237110.1016/S1359-6454(96)00361-8 ↗