Influence of silicon containing phases on the high-temperature fracture behavior of Ti-based diborides

A. Hirle, A. Bahr, T. Wojcik, P. Kutrowatz, J. Seltsam, P. Felfer, S. Kolozsvari, P. Polcik, K. Boebel, H. Riedl, R. Hahn

Materials & Design· Volume 264

Abstract

• Successful deposition of binary, ternary and quaternary Ti-(TM)-Si-B 2±z coatings. • Investigation of intrinsic fracture toughness at elevated temperatures up to 850 °C. • Transition from brittle to ductile at 600 °C for Ti-Si-B 2±z and Ti-Mo-Si-B 2±z. • Si distribution and phase constitution govern high-temperature fracture behavior. • Plasticity is promoted by the BDTT of Si segregations. Ti-TM-Si-B 2±z (TM = Ta, Mo) coatings are a new class of materials known for their excellent oxidation resistance and mechanical stability. This study explores their fracture characteristics, particularly at room and elevated temperatures. We synthesized hexagonal structured coatings including TiB 3.06 , Ti 0.26 Si 0.15 B 0.59 , Ti 0.23 Mo 0.07 Si 0.16 B 0.54 , and Ti 0.28 Ta 0.07 Si 0.12 B 0.53 using non-reactive DC magnetron sputtering. Conducting in-situ cantilever bending tests from room temperature to 850 °C revealed interesting insights into their plastic deformation capabilities. Specifically, Ti 0.26 Si 0.15 B 0.59 and Ti 0.23 Mo 0.07 Si 0.16 B 0.54 exhibited an onset of plastic deformation at approximately 600 °C, with a pronounced plastic response at 850 °C, which is attributed to Si-rich grain boundaries and Si nanoclusters identified by atom probe tomography. In contrast, the binary TiB 3.06 and quaternary Ti 0.28 Ta 0.07 Si 0.12 B 0.53 coatings exhibited fully linear-elastic behavior across all tested temperatures, despite silicide segregation in the quaternary coating. Notably, the Mo-containing coating exhibited the highest ductility, with strain to failure increasing from 1.7 % at room temperature to 3.3 % at 850 °C. Our findings indicate that the high-temperature fracture behavior of Ti-TM-Si-B 2±z coatings is mainly governed by Si distribution and the underlying segregation pathways: The formation of pure Si-nanoclusters is found to promote enhanced ductility, whilst (mixed) silicide formation stabilises a less compliant grain-boundary network.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (76)

Show source-provided references
1. Improved oxidation properties from a reduced B content in sputter-deposited TiBx thin films10.1016/j.surfcoat.2021.127353 ↗
2. Oxidation kinetics of overstoichiometric TiB2 thin films grown by DC magnetron sputtering10.1016/j.corsci.2022.110493 ↗
3. Improving the high-temperature oxidation resistance of TiB2 thin films by alloying with Al10.1016/j.actamat.2020.07.025 ↗
4. Influence of Si on the oxidation behavior of TM-Si-B2±z coatings (TM = Ti, Cr, Hf, Ta, W)10.1016/j.surfcoat.2022.128178 ↗
5. Effect of Si addition on mechanical properties and high temperature oxidation resistance of Ti–B–Si hard coatings10.1016/j.surfcoat.2013.12.011 ↗
6. Role of Si segregation in the structural, mechanical, and compositional evolution of high-temperature oxidation resistant Cr-Si-B2±z thin films10.1016/j.jallcom.2023.169203 ↗
7. Oxidation resistance of Si doped transition metal diborides at elevated temperatures10.1016/j.ijrmhm.2023.106172 ↗
8. The structure and mechanical properties of ti-Si-B coatings deposited by DC and pulsed-DC unbalanced magnetron sputtering10.1002/ppap.200731706 ↗
9. Characterization studies of pulse magnetron sputtered hard ceramic titanium diboride coatings alloyed with silicon10.1016/j.actamat.2008.04.047 ↗
10. Quaternary diborides—improving the oxidation resistance of TiB2 ± z coatings by disilicide alloying10.1080/21663831.2023.2225554 ↗
11. Oxidation behavior of ZrB2 composites doped with various transition metal silicides10.1016/j.corsci.2014.02.026 ↗
12. Understanding the oxidation behavior of a ZrB2–MoSi2 composite at ultra-high temperatures10.1016/j.actamat.2018.03.042 ↗
13. Microstructural characterization and isothermal oxidation behavior of hot-pressed TiB2–10wt.% TiSi2 composite10.1016/j.scriptamat.2009.03.027 ↗
14. Oxidation kinetics and mechanisms of hot‐pressed TiB2–MoSi2composites10.1111/j.1551-2916.2008.02656.x ↗
15. Oxidation behavior of melt-infiltrated SiC–TiB2 ceramic composites at 500–1300 °C in air10.1016/j.ceramint.2020.12.130 ↗
16. Thermodynamic analysis of ZrB2–SiC oxidation: Formation of a SiC‐depleted region10.1111/j.1551-2916.2006.01329.x ↗
17. Anisotropic hardness in TiB2±z thin films via depth-resolved crystallographic texture engineering10.1016/j.matdes.2025.115133 ↗
18. High-temperature oxidation resistance of ternary and quaternary Cr-(Mo)-Si-B2-z coatings — Influence of Mo addition10.1016/j.surfcoat.2023.129733 ↗
19. Structure and properties of Zr-Mo-Si-B-(N) hard coatings obtained by d.C. Magnetron sputtering of ZrB2-MoSi2 target10.3390/ma14081932 ↗
20. Microstructure evolution of ZrB2–MoSi2 composite coatings at middle and high temperatures10.1016/j.surfcoat.2015.03.029 ↗
21. High temperature oxidation resistance of metal silicide incorporated ZrB2 composite coatings prepared by vacuum plasma spray10.1016/j.ceramint.2015.08.015 ↗
22. Review of transition-metal diboride thin films10.1016/j.vacuum.2021.110567 ↗
23. Tissue phase affected fracture toughness of nano-columnar TiB2 + z thin films10.1080/21663831.2023.2204120 ↗
24. Unraveling the superlattice effect for hexagonal transition metal diboride coatings10.1016/j.scriptamat.2023.115599 ↗
25. Mechanical properties of DCMS and HiPIMS deposited Ti1-xMoxB2±z coatings10.1016/j.surfcoat.2025.131750 ↗
26. Hardness and fracture toughness enhancement in transition metal diboride multilayer films with structural variations10.1016/j.mtla.2024.102070 ↗
27. Revisiting the origins of super-hardness in TiB2+z thin films – Impact of growth conditions and anisotropy10.1016/j.surfcoat.2022.128806 ↗
28. Microstructure and materials properties of understoichiometric TiBx thin films grown by HiPIMS10.1016/j.surfcoat.2020.126537 ↗
29. Effects of Mo target power on the structure and tribological properties of AlB2 Ta1-xMoxB films by magnetron sputtering10.1016/j.ijrmhm.2024.106623 ↗
30. Influence of Tantalum on phase stability and mechanical properties of WB210.1557/mrc.2019.5 ↗
31. Strategy for simultaneously increasing both hardness and toughness in ZrB2-rich Zr1−xTaxBythin films10.1116/1.5093170 ↗
32. Thermally-induced structure evolution in ternary Ti1−xYxB2+Δ films10.1016/j.scriptamat.2019.01.042 ↗
33. Multifunctional ZrB2-rich Zr1-xCrxBy thin films with enhanced mechanical, oxidation, and corrosion properties10.1016/j.vacuum.2020.109990 ↗
34. Effect of temperature and atmosphere on the fracture toughness and failure mechanisms of two-dimensional plain-woven SiCf/SiC composites: Experiments and modeling10.1007/s10409-024-24333-x ↗
35. Annealing effect on the fracture toughness of CrN/TiN superlattices10.1016/j.ijrmhm.2017.11.008 ↗
36. Fracture toughness and structural evolution in the TiAlN system upon annealing10.1038/s41598-017-16751-1 ↗
37. Fracture properties of thin film TiN at elevated temperatures10.1016/j.matdes.2020.108885 ↗
38. Deformation of hard coatings at elevated temperatures10.1016/j.surfcoat.2014.06.048 ↗
39. High temperature fracture toughness of ceramic coatings evaluated using micro-pillar splitting10.1016/j.scriptamat.2018.11.013 ↗
40. High temperature fracture toughness of single-layer CrAlN and CrAlSiN hard coatings10.1016/j.surfcoat.2021.126909 ↗
41. Influence of Si segregates on the structural evolution, mechanical properties, and high-temperature fracture toughness of Cr-Si-B2±z coatings10.1016/j.jallcom.2023.170354 ↗
42. Measurement of thin film mechanical properties using nanoindentation10.1557/S0883769400041634 ↗
43. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
44. Ultrasonic determination of the temperature and hydrostatic pressure dependences of the elastic properties of ceramic titanium diboride10.1023/A:1017982508001 ↗
45. Critical review of analysis and interpretation of nanoindentation test data10.1016/j.surfcoat.2005.03.018 ↗
46. The HighScore suite10.1017/S0885715614000840 ↗
47. Measuring fracture toughness of coatings using focused-ion-beam-machined microbeams10.1557/JMR.2005.0048 ↗
48. A comparative micro-cantilever study of the mechanical behavior of silicon based passivation films10.1016/j.tsf.2009.07.143 ↗
49. Small-scale high-cycle fatigue testing by dynamic microcantilever bending10.1557/mrc.2020.31 ↗
50. Stress intensity factor dependence on anisotropy and geometry during micro-fracture experiments10.1016/j.scriptamat.2016.08.027 ↗
51. On the influence of microcantilever pre-crack geometries on the apparent fracture toughness of brittle materials10.1016/j.actamat.2017.07.014 ↗
52. Direct observation of crack arrest after bridge notch failure: a strategy to increase statistics and reduce FIB-artifacts in micro-cantilever testing10.1016/j.matdes.2023.112188 ↗
53. Elevated temperature,in situindentation with calibrated contact temperatures10.1080/14786435.2012.674647 ↗
54. P. Felfer, Atom-Probe-Toolbox: Matlab toolbox for APT analysis, Github, n.d. https://github.com/peterfelfer/Atom-Probe-Toolbox (accessed July 23, 2025).
55. Experiment and simulation of the compositional evolution of Ti–B thin films deposited by sputtering of a compound target10.1063/1.2978211 ↗
56. Others, Influence of Ta on the oxidation resistance of WB2- z coatings10.1016/j.jallcom.2020.158121 ↗
57. Age hardening in superhard ZrB2-rich Zr1-xTaxBy thin films10.1016/j.scriptamat.2020.09.026 ↗
58. Strategic lattice manipulation in transition metal nitrides for improved solubility10.1016/j.actamat.2024.120514 ↗
59. PDF-5+: a comprehensive Powder Diffraction FileTM for materials characterization10.1017/S0885715624000150 ↗
60. Thermal stability of superhard Ti–B–N coatings10.1016/j.surfcoat.2006.08.132 ↗
61. Fracture mechanics of micro samples: fundamental considerations10.1016/j.matdes.2018.09.004 ↗
62. Oxidation behaviour and mechanical properties of sputter-deposited TMSi2 coatings (TM = Mo, Ta, Nb)10.1016/j.jallcom.2022.167532 ↗
63. In-situ TEM investigation of toughening in Silicon at small scales10.1016/j.mattod.2021.03.009 ↗
64. Microscale fracture behavior of single crystal silicon beams at elevated temperatures10.1021/acs.nanolett.6b03461 ↗
65. Effect of temperature on fracture toughness in a single-crystal-silicon film and transition in its fracture mode10.1088/0960-1317/18/1/015026 ↗
66. Isothermal section of the Ti-Si-B system at 1250 ° C in the Ti-TiSi2-TiB2 region10.1590/S1516-14392013005000172 ↗
67. Plastic deformation of single crystals of CrB2, TiB2 and ZrB2 with the hexagonal AlB2 structure10.1016/j.actamat.2021.116857 ↗
68. Atomistic study of crack-tip cleavage to dislocation emission transition in silicon single crystals10.1103/PhysRevLett.104.235502 ↗
69. Temperature dependent fracture initiation in microscale silicon10.1016/j.scriptamat.2016.11.016 ↗
70. From nano-twinning to the glide of full dislocations: Micropillar compression tests on silicon up to 900 °C10.1016/j.matdes.2025.114730 ↗
71. Exploring the high-temperature deformation behavior of monocrystalline silicon – an advanced nanoindentation study10.1016/j.matdes.2023.112198 ↗
72. Mechanical behavior of MoSi2 and MoSi2 composites, Mater. Sci. Eng. a
73. Ductile-to-brittle transition in MoSi210.1557/PROC-288-1099 ↗
74. On the ductile-to-brittle transition temperature in MoSi210.1016/0956-716X(92)90224-3 ↗
75. Plasticity enhancement mechanisms in MoSi2, Mater. Sci. Eng. a
76. C.L. Briant, J.J. Petrovic, B.P. Bewlay, A.K. Vasudevan, H.A. Lipsitt, editors, “High Temperature Silicides and Refractory Alloys: Symposium, (n.d.). https://apps.dtic.mil/sti/tr/pdf/ADA278373.pdf.