Abstract
Ceramic matrix composites (CMCs) are commonly employed in situations where conventional materials face limitations or when they could provide substantial performance enhancements. However, when the latter condition is met, the increased performance must offset the higher costs associated with development and manufacturing. In this study, a methodological approach is introduced to concurrently reduce costs and optimize performance via virtual product development and tailored material customization. The effectiveness of this approach is demonstrated using an antenna strut in the context of space applications as an illustrative example. Moreover, strategies are proposed for the integration of pre-existing simulation models. Relevant diagrams are provided for CMC customization, alongside the introduction of a cost model based on the cost-performance ratio in contrast to a reference product. As a result, the study significantly enhances the competitiveness of CMC components compared to conventional materials, ultimately expanding their market potential.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Manufacturing Process and Optimization · Additive Manufacturing and 3D Printing Technologies · Product Development and Customization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Ashby · 2006
2. May · 2020
3. Production of mirrors made of HB-Cesic® for an airborne reconnaissance telescope system
4. Designing optimized, ultra-lightweighted mirror structures made of Cesic® for space and ground based applications
5. Recent achievements with a cryogenic ultra-lightweighted HB-Cesic® mirror
6. Ultra-lightweighted HB-Cesic® one-meter mirror demonstrator
7. Hofbauer · 2012
8. Multi-objective optimization in material design and selection10.1016/S1359-6454(99)00304-3 ↗
9. Degischer · 2009
10. Moeller · 2008
11. Bargel · 2005
12. Ostermann · 1998
13. Leyens · 2003
14. Bansal · 2015
15. Fracture toughness and fiber bridging of carbon fiber reinforced carbon composites10.1016/0266-3538(91)90083-2 ↗
16. Tensile strength of carbon/carbon composites10.1299/jsmea.46.290 ↗
17. Bansal · 2005
18. Bansal · 2012
19. Progress in processing and performance of porous-matrix oxide/oxide composites10.1111/j.1744-7402.2005.02016.x ↗
20. Time-dependent proportional limit stress of carbon fiber-reinforced silicon carbide ceramic-matrix composites considering interface oxidation10.2109/jcersj2.18176 ↗
21. Mahajan · 2020
22. Tailoring Multiphase and Composite Ceramics
23. Cryogenic optical testing of an 800 mm lightweight C/SiC composite mirror mounted on a C/SiC optical bench10.1364/AO.49.003941 ↗
24. Graves · 1994
25. Properties of chemical-vapor-deposited silicon carbide for optics applications in severe environments10.1364/AO.30.003166 ↗
26. Ashby · 1986
27. Der Einfluß der Korngröße, des Legierungsgehaltes und einer Kaltverformung auf die Bruchzähigkeit
28. Fracture toughness behaviour of service-exposed type 321 stainless steel at room and elevated temperature under normal and low straining rates10.1016/0013-7944(89)90031-3 ↗
29. Fracture mode and toughness vs temperature (−20–22∘C) for UNS-S15500 (15-5 PH) stainless steel10.1016/0013-7944(79)90077-8 ↗
30. Effect of microstructure on fracture toughness of AZ91 magnesium alloy10.1299/kikaia.62.1806 ↗
31. Weißbach · 2007
32. Roos · 2005
33. Salmang · 2007
34. Pierson · 1993
35. Burchell · 1999
36. Fracture Toughness of Carbon Fiber Reinforced Ceramic Composites
37. Ashby · 2005
38. Effects of fiber architecture on matrix cracking for melt-infiltrated SiC/SiC composites10.1111/j.1744-7402.2009.02422.x ↗
39. CMC design consequences
40. Mühlratzer · 2001 · 288
41. Effects of frequency on fatigue behavior of CVI C/SiC at elevated temperature10.1016/j.compscitech.2005.06.020 ↗
42. A comparative study on Cf/PyC/SiC minicomposites prepared via CVI process for hypersonic engine application10.1111/ijac.12898 ↗
43. Development of C/PyC/SiC CMCs by CVI process for hypersonic vehicle application10.1007/s41403-020-00180-0 ↗
44. Mechanical properties of 3D fiber reinforced C/SiC composites10.1016/S0921-5093(00)01533-1 ↗
45. Xu · 2001 · 772
46. Microstructural characterization and tensile behaviour of a 3D braided C/SiC composite fabricated by chemical vapour infiltration10.1177/096369350801700402 ↗
47. Experimental investigation on 2D and 3D braided C/SiC composites10.4028/www.scientific.net/KEM.326-328.1685 ↗
48. Krenkel · 2008
49. Krenkel · 2003
50. Daxer · 2020
51. Air intake ramp made from C/SiC via the polymer route for hypersonic propulsion systems
52. Development of a new cost-effective ceramic composite for re-entry heat shield applications10.1016/S0094-5765(97)00220-8 ↗
53. Gowayed · 2020
54. U.S. Department of Defense · 2002
55. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
56. Silicon carbide (NicalonTM) fibre-reinforced borosilicate glass composites: mechanical properties10.1023/A:1018642723310 ↗
57. Wachtman · 2009
58. Ceramic composites: a review of toughening mechanisms and demonstration of micropillar compression for interface property extraction10.1557/jmr.2017.473 ↗
59. Appropriate thickness of pyrolytic carbon coating on SiC fiber reinforcement to secure reasonable quasi-ductility on NITE SiC/SiC composites10.1016/j.ceramint.2018.07.158 ↗
60. Li · 2020
61. Quantification of crack area in ceramic matrix composites at single-fiber push-out testing and influence of pyrocarbon fiber coating thickness on interfacial fracture toughness10.1016/j.jeurceramsoc.2015.04.033 ↗
62. Effects of fiber volume fraction on the densification and mechanical properties of unidirectional SiCf/SiC-matrix composites10.1016/j.jeurceramsoc.2020.09.024 ↗
63. Effect of microstructure on the mechanical behavior of continuous-fiber-reinforced ceramic-matrix composites10.1111/j.1151-2916.1999.tb02152.x ↗
64. Damage initiation under transverse loading of unidirectional composites with arbitrarily distributed fibers10.1016/S0266-3538(98)00122-5 ↗
65. A micromechanical analysis of inter-fiber failure in long reinforced composites based on the phase field approach of fracture combined with the cohesive zone model
66. Characterizing fiber-matrix debond and fiber interaction mechanisms by full-field measurements10.1016/j.jcomc.2022.100229 ↗
67. SiC fiber reinforced SiC-Si matrix composites prepared by melt infiltration (MI) for gas turbine engine applications
68. Failure analysis of unidirectional ceramic matrix composite lamina and cross-ply laminate under fiber direction uniaxial tensile load: cohesive zone modeling and brittle fracture mechanics approach10.1007/s11665-020-04724-x ↗
69. Stress/strain behavior of a 3-D woven composite based on the SiC/SiC system
70. BepiColombo HGA ARA C/SiC struts: a thermo - mechanical challenge for support structures in harsh environments
71. High temperature fracture toughness of a C/SiC (CVI) composite as used for screw joints in re-entry vehicles
72. Environmental properties and applications of 3D C/SiC and SiC/SiC composites by chemical vapor infiltration
73. Effect of thermal cycling on modulus and tensile strength of 3D needled C/SiC composite in controlled environments10.1016/j.msea.2008.08.009 ↗
74. Mentz · 2003
75. Carbon fiber reinforced silicon carbide ceramic matrix composites
76. Riedel · 2008
77. Experimental and numerical evaluation of bending and tensile behaviour of carbon-fibre reinforced SiC10.1016/j.compositesa.2012.07.017 ↗
78. Multiscale model of woven ceramic matrix composites considering manufacturing induced damage10.1016/j.compstruct.2015.02.015 ↗
79. Finite element modeling of reactive liquid silicon infiltration10.1016/j.jeurceramsoc.2019.09.041 ↗
80. Computational design of hierarchically structured materials10.1126/science.277.5330.1237 ↗
81. Fundamental mechanisms with reactive infiltration of silicon melt into carbon capillaries10.1002/adem.201900184 ↗
82. In-situ-Messung und Simulation der Flüssigphasensilicierung
83. Effects of oxygen on the liquid silicon infiltration (LSI) process
84. Schmitz · 2017
85. Development of bond strength model for FRP plates using back-propagation algorithm10.1002/app.24069 ↗
86. Design of nano-micro-composite ceramic tool and die material with back propagation neural network and genetic algorithm10.1007/s11665-011-9974-4 ↗
87. Optimisation of manufacturing process parameters using deep neural networks as surrogate models
88. Artificial intelligence in materials modeling and design10.1007/s11831-020-09506-1 ↗
89. Application of deep neural network learning in composites design10.1080/26889277.2022.2053302 ↗
90. Inverse design of materials by machine learning10.3390/ma15051811 ↗
91. Matzka · 2021
92. Feature engineering of material structure for AI-based materials knowledge systems10.1063/5.0011258 ↗
93. Inverse technique identification of material parameters using finite element and neural network computation10.1007/s00170-008-1809-6 ↗
94. Deep learning framework for material design space exploration using active transfer learning and data augmentation
95. Inverse design of two-dimensional materials with invertible neural networks
96. Torrisi · 2022 · 65
97. Friedrich · 2013
98. Klein · 2020
99. CPR a general cost performance ratio in manufacturing - a KPI for judgement of different technologies and development scenarios10.1016/j.procir.2018.03.106 ↗
100. Integration of CMC brake disks in automotive brake systems10.1111/j.1744-7402.2012.02812.x ↗