Suppressing hydrogen blistering in a magnesium-rich healable laser powder bed fusion aluminum alloy analyzed by in-situ high resolution techniques
Source abstract
Abstract
Hydrogen blistering, i.e. precipitation of supersaturated hydrogen at elevated temperatures, increases porosity during heat treatments in 4xxx series Al alloys manufactured by laser powder bed fusion (LPBF), as demonstrated by 3D X-ray nano-imaging in AlSi12. This paper proposes the design of a healable Al alloy to suppress hydrogen blistering and improve the damage management. The strategy consists of solute atoms diffusing towards nano-voids and precipitating on their surface, thereby filling the damage sites. A new healable Al alloy was thus developed and successfully manufactured by LPBF. 3D X-ray nano-imaging evidenced that the addition of Mg in 4xxx series Al alloys suppresses the hydrogen blistering. This is expectedly due to Mg in solid solution which increases the hydrogen solubility in the Al matrix and due to the healing of these hydrogen pores. Moreover, a significant healing of voids smaller than 500 nm diameter is observed. In-situ heating inside transmission electron microscopy pointed out that Al matrix diffuses inside the fractured Mg2Si particles, thereby demonstrating the healing ability of the new alloy. This has opened the doors to development of new healable Al alloys manufactured by LPBF as well as to new post-treatments to tailor mechanical properties and microstructure without hydrogen blistering.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. 12 – Additive manufacturing (AM)
2. Microstructure and wear behavior of in-situ hypereutectic Al–high Si alloys produced by selective laser melting10.1016/j.matdes.2016.03.053 ↗
3. Influence on microstructure, strength and ductility of build platform temperature during laser powder bed fusion of AlSi10Mg10.1016/j.actamat.2020.10.001 ↗
4. Laser powder bed fusion AlSi10Mg damage and fatigue resistance improvement by post-processing
5. Ductilisation and fatigue life enhancement of selective laser melted AlSi10Mg by friction stir processing10.1016/j.scriptamat.2019.05.044 ↗
6. P. Van Cauwenbergh, G. Krishna Muralidharan, P. Bigot, L. Thijs, B. Van Hooreweder, K. Vanmeensel, Reducing hydrogen pores and blisters by novel strategies and tailored heat treatments for Laser Powder Bed Fusion of AlSi7Mg0.6, Euro PM19, Euro PM2019, Maastricht, The Netherlands, 2019, pp. 1–7.
7. Laser powder bed fusion of high strength aluminum
8. AlSi10Mg lattice structures produced by Selective Laser Melting: from microstructure characterization to impact resistance
9. Gerrard · 2014
10. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
11. Laser powder bed fusion of potential superalloys: a review10.3390/met11010058 ↗
12. A. Schmets, G. Zaken, S. Zwaag, Self healing materials: an alternative approach to 20 centuries of materials science, 2007.
13. Self-healing materials10.1002/adma.201003036 ↗
14. Grabowski · Self-Healing Metals · 2015
15. Self-healing in metal-based systems
16. van der Zwaag, Self-healing of deformation damage in underaged Al–Cu–Mg alloys10.1016/j.scriptamat.2007.11.039 ↗
17. In situ electron microscopy investigation of void healing in an Al–Mg–Er alloy at a low temperature10.1016/j.actamat.2014.02.004 ↗
18. A new healing strategy for metals: Programmed damage and repair10.1016/j.actamat.2022.118241 ↗
19. Damage mechanisms in selective laser melted AlSi10Mg under as built and different post-treatment conditions10.1016/j.msea.2019.138210 ↗
20. Precipitation induced densification in a sintered Al–Zn–Mg–Cu alloy10.1016/j.scriptamat.2006.04.021 ↗
21. Solute trapping: comparison of theory with experiment10.1103/PhysRevLett.56.2489 ↗
22. Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments10.1016/j.msea.2017.08.029 ↗
23. Defect-induced Au precipitation in Fe–Au and Fe–Au–B–N alloys studied by in situ small-angle neutron scattering10.1016/j.actamat.2013.08.015 ↗
24. Susceptibility of ternary aluminum alloys to cracking during solidification10.1016/j.actamat.2016.12.028 ↗
25. Efficient optimization methodology for laser powder bed fusion parameters to manufacture dense and mechanically sound parts validated on AlSi12 alloy10.1016/j.matdes.2020.109433 ↗
26. Fast in situ 3D nanoimaging: a new tool for dynamic characterization in materials science10.1016/j.mattod.2017.06.001 ↗
27. Microstructural porosity in additive manufacturing: The formation and detection of pores in metal parts fabricated by powder bed fusion10.1002/amp2.10021 ↗
28. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
29. Hydrogen trapping in Mg2Si and Al7FeCu2 intermetallic compounds in aluminum alloy: first-principles calculations10.2320/matertrans.MT-M2020201 ↗
30. Intensity of hydrogen trapping in pure Al, Al-4 wt % Cu and Al-1 wt % Mg2Si alloys measured by tritium release10.1007/BF00633523 ↗
31. Analysis of the effects of alloying elements on hydrogen solubility in liquid aluminum alloys10.1016/0956-716X(95)00373-4 ↗
32. Nanoscale periodic gradients generated by laser powder bed fusion of an AlSi10Mg alloy10.1016/j.matdes.2020.109264 ↗
33. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
34. Self-healing phenomena in metals10.1002/admi.201800226 ↗
35. A Review of self-healing metals: fundamentals, design principles and performance
36. S.H. Huo, M. Qian, G.B. Schaffer, E. Crossin, 21 – Aluminium powder metallurgy, in: R. Lumley (Ed.), Fundamentals of Aluminium Metallurgy, Woodhead Publishing 2011, pp. 655-701.10.1533/9780857090256.3.655 ↗
37. Low temperature annealing dedicated to AlSi10Mg selective laser melting products10.1016/j.jallcom.2016.12.019 ↗
38. Shrinkage and splitting of microcracks under pressure simulated by the finite-element method10.1007/s11661-002-0213-3 ↗
39. High-temperature oxidation performance of Ni-based GH3536 superalloy fabricated by laser powder bed fusion10.1038/s41529-022-00276-8 ↗
40. 5 - Diffusion in metals and alloys
41. Grown-in defects in silicon crystals10.1016/S0022-0248(01)02323-5 ↗
42. Unravelling the multi-scale structure–property relationship of laser powder bed fusion processed and heat-treated AlSi10Mg10.1038/s41598-021-85047-2 ↗
43. Revision of the solvus limit of Al-Mg2Si pseudo binary phase diagram10.1016/j.mspro.2015.04.171 ↗
44. Severe plastic deformation induced sensitization of cryo-milled nanocrystalline Al-7.5 Mg10.1007/s11661-014-2227-z ↗