journal article·2016-01

Consolidation of titanium hydride powders during the production of titanium PM parts: The effect of die wall lubricants

C. Machio, R. Machaka, H.K. Chikwanda

Materials & Design· Volume 90
Publisher page

Abstract

Abstract The effects of die wall lubricants on the cold compaction of titanium hydride powder are studied. Three commonly-used die wall powder metallurgy lubricants – zinc stearate, Acrawax® C dispersion and Mirror Glaze® – are compared. The influence of each lubricant on the cold compaction behaviour of titanium hydride powder was assessed with respect to the green density and strength, green compact ejection force, and the occurrence of green compact cracking. In addition, green compacts were sintered under vacuum at various sintering temperatures in order to determine the effect of the lubricants on oxygen content, phase compositions, microstructures and hardness of the sintered components. The results indicate that there is an immediate improvement in the cold compaction process when lubrication is used. The results further indicate that the lubricity of the lubricants is similar and most of the monitored variables are insensitive to the die wall lubricant used, the microstructures of the sintered components included. However, the use of Acrawax® dispersion resulted in more instances of green compact cracking, while zinc stearate tended to increase the oxygen content of sintered specimens due to the tentative decomposition of zinc oxide, a residual of the high temperature decomposition of zinc stearate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Powder Metallurgy Techniques and Materials · Advanced materials and composites · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (68)

Show source-provided references
1. Titanium for automotive applications: challenges and opportunities in materials and processing
2. Christoph · 2003
3. Titanium powder metallurgy: a review — part 2
4. Optimization of blended-elemental powder-based titanium alloy extrusions for aerospace applications10.1007/s11661-012-1437-5 ↗
5. Effects of lubricant on green strength, compressibility and ejection of parts in die compaction process10.1016/j.powtec.2012.08.033 ↗
6. Brunette · 2001
7. Highly porous open cell Ti-foam using NaCl as temporary space holder through powder metallurgy route10.1016/j.matdes.2013.01.005 ↗
8. Effect of pore structure on the compressive property of porous Ti produced by powder metallurgy technique10.1016/j.matdes.2013.02.082 ↗
9. Titanium foam with coarser cell size and wide range of porosity using different types of evaporative space holders through powder metallurgy route10.1016/j.matdes.2014.05.054 ↗
10. Space-holder effect on designing pore structure and determining mechanical properties in porous titanium10.1016/j.matdes.2013.12.078 ↗
11. Designing, processing and characterisation of titanium cylinders with graded porosity: an alternative to stress-shielding solutions10.1016/j.matdes.2014.06.012 ↗
12. Fabrication of porous NiTi-shape memory alloy objects by partially hydrided titanium powder for biomedical applications10.1016/j.matdes.2009.05.034 ↗
13. Fabrication of Ti–Nb–Ag alloy via powder metallurgy for biomedical applications10.1016/j.matdes.2013.11.066 ↗
14. Remarkable superelasticity of sintered Ti–Nb alloys by Ms adjustment via oxygen regulation10.1016/j.matdes.2015.07.180 ↗
15. Kujala · 2003
16. Effects of initial powder compact thickness, lubrication, and particle morphology on the cold compaction behaviour of Ti powder
17. Analysis of the cold compaction behaviour of TiH2–316L nanocomposite powder blend using compaction models10.4028/www.scientific.net/MSF.828-829.121 ↗
18. An experimental evaluation of the Gerdemann–Jablonski compaction equation10.1007/s11661-015-2793-8 ↗
19. Analysis of the cold compaction behaviour of titanium powders: a comprehensive inter-model comparison study of compaction equations10.1007/s11661-015-3038-6 ↗
20. Compressibility of a Ti-based alloy with varying amounts of surfactant prepared by high-energy ball milling10.1016/j.powtec.2015.03.044 ↗
21. Improving the uniformity in mechanical properties of a sintered Ti compact using a trace amount of internal lubricant10.1016/j.jmatprotec.2014.03.022 ↗
22. Frykholm · 2014
23. Study of the properties of low-cost powder metallurgy titanium alloys by 430 stainless steel addition10.1016/j.matdes.2014.04.019 ↗
24. Powder metallurgy CP-Ti performances: hydride–dehydride vs. sponge10.1016/j.matdes.2014.04.005 ↗
25. Investigation of die stress profiles during powder compaction using instrumented die10.1007/s11665-008-9229-1 ↗
26. Study of compaction and ejection of hydrided–dehydrided titanium powder10.1007/s12540-011-0207-z ↗
27. Densification of titanium (Ti) from titanium hydride (TiH2) powder through dehydrogenation and pressureless sintering process
28. The investigation of die-pressing and sintering behaviour of ITP CP-Ti and ti–6Al–4V powders10.1016/j.jallcom.2012.06.131 ↗
29. Density gradient evolution during dry pressing
30. Friction measurement and lubrication in unloading and ejection stages in powder pressing cycle10.1179/174329008X271646 ↗
31. The effects of wall friction in powder compaction10.1016/S0927-7757(97)00210-0 ↗
32. Effects of lubrication procedure on the consolidation, sintering and microstructural features of powder compacts10.1016/S0261-3069(03)00155-9 ↗
33. Lubricants in pharmaceutical solid dosage forms10.3390/lubricants2010021 ↗
34. New technological approach to fabrication of high density PM parts by cold pressing sintering10.1179/003258904225020738 ↗
35. PM processing of elemental and prealloyed 6061 aluminium alloy with and without common lubricants and sintering aids10.1179/174329006X152460 ↗
36. Binder treated products for higher densities and better precision
37. Effect of lubricant addition on the powder properties and compacting performance of spray-dried molybdenum powders10.1016/S0263-4368(01)00062-2 ↗
38. Looking closely at PM lubes through the microscope to ‘see real effects’10.1016/S0026-0657(07)70020-6 ↗
39. Compaction, sintering and mechanical properties of elemental 6061 al powder with and without sintering aids10.1016/j.matdes.2007.01.027 ↗
40. Investigation on the effect of lubrication and forming parameters to the green compact generated from iron powder through warm forming route10.1016/j.matdes.2010.06.013 ↗
41. Tensile properties of phenol–formaldehyde nanoclay reinforced composites: a pilot study10.1002/app.35232 ↗
42. Paraffin oxidation studies
43. Microstructure and mechanical properties of titanium components fabricated by a new powder injection moulding technique10.1016/j.msec.2005.04.006 ↗
44. Comparison of sintering of titanium and titanium hydride powders10.1179/003258909X12450768327063 ↗
45. Tensile strength and fracture energy of pressed metal powder by diametral compression test10.1016/j.powtec.2007.02.030 ↗
46. Comparison of the green strength of warm compacted astaloy CrM and distaloy AE densmix* powder compacts10.1179/026708304225017292 ↗
47. The Brazilian disc test for rock mechanics applications: review and new insights10.1007/s00603-012-0257-7 ↗
48. Lubricant distribution on compacts and tool walls after P/M compaction
49. Newly developed iron-based powder mixture, high density SEGLESS, for high density compaction
50. Benefits of die wall lubrication for powder compaction
51. A new approach to die wall lubrication for P/M applications
52. Cold compaction study of Armstrong process® Ti–6Al–4V powders10.1016/j.powtec.2011.08.007 ↗
53. Unloading of powder compacts and their resulting tensile strength10.1016/S1359-6454(03)00296-9 ↗
54. Density gradients and springback: environmental influences10.1016/S0032-5910(03)00083-4 ↗
55. The compressibility and compactibility of powder systems10.1016/0378-5173(82)90132-6 ↗
56. Compressibility and compactibility of metal powders
57. Luk · 1998
58. Tensile strength of concrete
59. A performance comparison of current P/M lubricants and routes to improvement
60. Review of densification of titanium based powder systems in press and sinter processing10.1179/174329009X434293 ↗
61. Lubricant pyrolysis during sintering of powder metallurgy compacts10.1007/s11663-004-0038-0 ↗
62. Oven operation in sintering powder components plasticized with zinc stearate10.1007/BF00561276 ↗
63. Effects of the decomposition residue of compound additive on resintering behaviour
64. Determination of the local oxygen distribution in a commercial titanium alloy by 3-dimensional atom probe10.3139/146.030771 ↗
65. The thermal decomposition of zinc oxide10.1246/bcsj.37.1181 ↗
66. Atomic number and crystallographic contrast images with the SEM: a review of backscattered electron techniques10.1180/minmag.1987.051.359.02 ↗
67. Thermal stability and recrystallization of nanocrystalline Ti produced by cryogenic milling10.1007/BF02586127 ↗
68. Synthesis and phase transformations of beta metastable Ti-based alloys containing biocompatible Ta, Mo and Fe beta-stabilizer elements10.1002/adem.200600106 ↗