journal article·2026-10

The enhanced wear resistance of TaC/Cu0.9Ni0.1 composite by heterogeneous architecture

Kangping Sun, Qian Qi, Lujie Wang, Xiquan Zhang, Xiaoqi Yang, Ziheng Wang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Enhancement of mechanical properties and fatigue performance of pure copper through GP and TaC reinforcements in metal matrix composites10.1016/j.ijfatigue.2025.109282 ↗
2. Influence of solution-hardening on the mechanical properties and wear resistance of copper alloys10.1016/j.wear.2023.204869 ↗
3. Effect of adding copper-plated graphite on the organization and wear reduction of copper-nickel alloy composite coatings10.1016/j.surfcoat.2024.131661 ↗
4. Microstructure, wear and corrosion properties of laser melted CoCrNiFeTix high-entropy alloy coatings on copper alloys10.1016/j.jallcom.2025.179674 ↗
5. Integrity on properties of Cu-based composites with the addition of reinforcement: a review10.1016/j.matpr.2021.05.096 ↗
6. Thermal expansion characteristics of cast Cu based metal matrix composites10.1016/S1359-835X(97)00077-8 ↗
7. Development of Ni-Cu based alloy hybrid composites through induction furnace casting10.1016/j.matpr.2022.09.215 ↗
8. Microstructure and impact properties of Ta-TaC core–shell rod-reinforced iron-based composite fabricated by in situ solid-phase diffusion10.1016/j.jallcom.2018.07.267 ↗
9. Improving the mechanical properties of tantalum carbide particle-reinforced iron-based composite by varying the TaC contents10.1016/j.jallcom.2017.08.050 ↗
10. Structural features of tantalum carbide-copper composites obtained by liquid phase-assisted spark plasma sintering10.1016/j.ceramint.2022.07.322 ↗
11. Preparation of dispersion-strengthened coppers with NbC and TaC by mechanical alloying10.2320/matertrans1989.32.389 ↗
12. Effect of different types of reinforcement on tribological properties of aluminium metal matrix composites (MMCs) – a review of recent studies10.1016/j.matpr.2021.12.211 ↗
13. Fabrication methods of metal matrix composites (MMCs)10.1016/j.matpr.2021.04.432 ↗
14. Recent advances in zinc-based metal matrix composites: fabrication, properties, and future prospects10.1016/j.jalmes.2025.100173 ↗
15. Synergistic effect and strengthening mechanism of biphasic in-situ nanoparticles (ZrB2+Al2O3) on the microstructure and mechanical properties of 7A33 aluminum alloy10.1016/j.matchar.2026.116459 ↗
16. Corrosion and wear performance and mechanism study of ZrB2/AA601610.1088/2051-672X/ad8d6d ↗
17. Optimization of tribological properties and multi-parameter statistical analysis of 6016Al composites reinforced with in-situ synthesized (ZrB2 + Al2O3) binary ceramic particles10.1007/s10853-025-11824-3 ↗
18. The mechanical properties of in-situ composites10.1007/BF02914400 ↗
19. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
20. Design and property optimization of bimodal structures of WC-reinforced Cu matrix composites10.1016/j.msea.2025.148419 ↗
21. Synergistic enhancement of strength-ductility in ODS copper alloy by exploring heterogeneous structure10.1016/j.msea.2025.148194 ↗
22. Synergetic enhancement of strength and ductility by heterogeneous architecture in interpenetrating copper and graphene-copper composite
23. Heterostructured NiCr matrix composites with high strength and wear resistance10.1016/j.jmst.2021.06.076 ↗
24. Wetting and spontaneous infiltration: the case study of TaC/(Au, Al and Cu) compared to TiC/Cu10.1088/1757-899X/133/1/012020 ↗
25. Fabrication of Cu-Ta composite with high strength and electrical conductivity through thermomechanical processing10.1016/j.jallcom.2025.181815 ↗
26. The role of reactivity in wetting by liquid metals: a review10.1007/s10853-015-9331-3 ↗
27. Formation mechanism and single abrasive wear of TaC dense ceramic layer on surface of gray cast iron10.1016/j.ceramint.2019.05.067 ↗
28. Microstructure and kinetics study on tantalum carbide coating produced on gray cast iron in situ10.1016/j.surfcoat.2015.12.057 ↗
29. Can the H/E ratio be generalized as an index for the wear resistance of materials?10.1016/j.matchemphys.2021.125245 ↗
30. The influence of the H/E ratio on wear resistance of coating systems – insights from small-scale testing10.1016/j.surfcoat.2022.128272 ↗
31. XPS study of the Cu@Cu2O core-shell nanoparticles10.1016/j.apsusc.2008.08.110 ↗
32. Peak-fitting of Cu 2p photoemission spectra in Cu0, Cu1+, and Cu2+ oxides: a method for discriminating Cu0 from Cu1+10.1016/j.apsusc.2023.156960 ↗
33. Interpretation of Ni2p XPS spectra of Ni conductors and Ni insulators10.1007/s002690050265 ↗
34. New interpretations of XPS spectra of nickel metal and oxides10.1016/j.susc.2006.01.041 ↗
35. XPS investigation of monatomic and cluster argon ion sputtering of tantalum pentoxide10.1016/j.apsusc.2017.02.006 ↗
36. Optical and structural properties of TaC thin films: towards design of an efficient high temperature solar absorber coating10.1016/j.solener.2025.113459 ↗
37. Analysis of XPS spectra of Fe2+ and Fe3+ ions in oxide materials10.1016/j.apsusc.2007.09.063 ↗
38. Characterization of the “native” surface thin film on pure polycrystalline iron: a high resolution XPS and TEM study10.1016/j.apsusc.2006.09.047 ↗
39. Dry-sliding self-lubricating ceramics: CuO doped 3Y-TZP10.1016/j.wear.2009.06.033 ↗
40. Nanolubricants developed from tiny CuO nanoparticles10.1016/j.triboint.2016.01.050 ↗
41. Oxidation behavior of equiatomic TiNi alloy in high temperature air environment10.1016/0921-5093(96)10409-3 ↗
42. High temperature phase changes and oxidation behavior of cr–si–n coatings10.1016/j.surfcoat.2007.05.070 ↗
43. The oxidation mechanism of TaC/Ni composites10.1007/s11661-024-07553-y ↗
44. Analysis of thermally grown oxides on microperforated copper sheets10.1007/s11665-023-08328-z ↗
45. Oxidation mechanisms of tantalum carbides at extreme temperatures
46. Enhanced oxidation resistance of in-situ TaC/Ni composites by Cr2O3–CrTaO4 network in oxide scale10.1016/j.ijrmhm.2025.107570 ↗
47. Study of tribological property of laser-cladded FeCoCrNiMnx high-entropy alloy coatings via experiment and molecular dynamics simulation10.1016/j.triboint.2023.109106 ↗
48. Tribology and oxidation properties of graphite/CuNiTiCrNb HEA coatings produced by laser cladding10.1016/j.carbon.2026.121261 ↗