Subsurface gallium in aluminium: Regime-dependent electrochemical behaviour and composition-dependent corrosion and dissolution response
Source abstract
Abstract
The electrochemical behaviour of aluminium and binary Al–Ga alloys (0.01–0.20 wt.% Ga) was investigated in 2 M NaCl to assess the influence of gallium on both spontaneous corrosion and anodic response. An integrated approach was used, combining electrochemical measurements (OCP, EIS, potentiodynamic and galvanostatic polarisation) with XPS/EDS analysis and 3D optical profilometry. The results show that gallium is not incorporated into the surface film but remains confined to the metallic matrix as Ga(0), indicating a subsurface mode of action. Its presence is associated with a clear difference between spontaneous and anodic behaviour. Under open-circuit conditions, corrosion is reduced and the surface film becomes more resistive, while under anodic polarisation, hydrogen evolution decreases, the negative differential effect is less pronounced, and anodic efficiency increases. Morphological analysis reveals reproducible microanodic structures characteristic of anodic dissolution. Among the investigated compositions, the Al–0.10 wt.% Ga alloy shows the most favourable balance between corrosion resistance and anodic activity. Overall, the results point to a consistent relationship between subsurface gallium and electrochemical behaviour, without clear evidence of its direct involvement in surface film formation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Metal–air batteries—A review10.3390/en14217373 ↗
2. Metal–air batteries: progress and perspective10.1016/j.scib.2022.11.027 ↗
3. Metal–air battery: a sustainable and low-cost material for energy storage10.1088/1742-6596/1913/1/012065 ↗
4. Aqueous metal–air batteries: fundamentals and applications10.1016/j.ensm.2019.12.011 ↗
5. Aluminum as anode for energy storage and conversion: a review10.1016/S0378-7753(01)01014-X ↗
6. Developments in electrode materials and electrolytes for aluminium–air batteries10.1016/j.jpowsour.2013.01.141 ↗
7. Recent developments in materials for aluminum–air batteries: a review10.1016/j.jiec.2015.08.004 ↗
8. An overview and future perspectives of aluminum batteries10.1002/adma.201601357 ↗
9. A comprehensive review on recent progress in aluminum–air batteries10.1016/j.gee.2017.06.006 ↗
10. Electrochemical energy storage by aluminum as a lightweight and cheap anode10.1039/C7SE00050B ↗
11. A review of Al alloy anodes for Al–air batteries
12. Modern aspects of electrochemistry
13. The kinetics of hydrogen evolution on aluminium10.1023/A:1003447018115 ↗
14. Introductory lecture on corrosion chemistry10.1039/C5FD00066A ↗
15. The mechanism of hydrogen evolution during anodic polarization of aluminium10.1016/j.electacta.2015.08.076 ↗
16. The effect of small addition of tin and indium on the corrosion behavior of aluminium in chloride solution10.1016/j.jallcom.2010.06.055 ↗
17. Corrosion behaviour of aluminium alloys10.1149/1.2100325 ↗
18. Corrosion behaviour of aluminium–lanthanide alloys10.1016/S0013-4686(96)00420-3 ↗
19. Electrochemical behaviour of aluminium in chloride solutions10.5006/1.3292104 ↗
20. Electrochemical behaviour of aluminium in neutral chloride solutions10.1023/A:1003684219989 ↗
21. Effect of Ga and Pb on anodic activation of aluminium10.1016/j.corsci.2017.12.009 ↗
22. Electrochemical behaviour of aluminium anodes for Al–air batteries10.1016/j.jpowsour.2005.11.097 ↗
23. Electrochemical properties of aluminium anodes10.1007/s10800-012-0465-6 ↗
24. Aluminium alloys containing indium and tin10.1016/j.matchemphys.2010.02.040 ↗
25. Performance of al–mg–ga–sn based alloys10.1016/j.jpowsour.2013.12.053 ↗
26. Electrochemical performance of al–mg–zn–ga–sn alloys10.1016/j.electacta.2014.02.080 ↗
27. Al–mg–Sn based alloys for Al–air batteries10.1149/2.1241608jes ↗
28. Role of Sn and Ga in al–mg–sn–ga alloys
29. Melt-spinning of al–mg–sn alloys10.1016/j.ijhydene.2017.02.185 ↗
30. Effect of Ga and Pb additions in al–mg–sn alloys10.1016/j.jallcom.2016.11.176 ↗
31. In/Ga/Bi additions in al–mg–sn alloys10.1007/s10008-019-04341-2 ↗
32. Al–Mg–Ga–In based alloys for aluminium–air batteries10.1016/j.ijhydene.2019.03.081 ↗
33. The role of gallium and indium in improving the electrochemical characteristics of Al–Mg–Sn-Based alloy for Al–air battery anodes in 2 M NaCl solution10.1007/s10853-020-04755-8 ↗
34. Effects of Ga on the microstructure and electrochemical properties of al–zn–in–mg alloys10.3390/coatings12010053 ↗
35. Electrochemical behavior of al–mg–sn–ga–bi alloys as anode for Al–air batteries in NaCl and KOH10.3390/cryst12121785 ↗
36. Influence of Ga on hydrogen evolution and discharge properties of al–bi–pb alloy in alkaline and neutral electrolytes
37. In situ activation of aluminum anode by Ga3+ for stable hydrogen production
38. Orazem · 2017
39. On the intrinsic coupling between constant-phase element parameters α and Q in electrochemical impedance spectroscopy10.1016/j.electacta.2012.04.020 ↗
40. Electrochemical impedance spectroscopy: a tutorial10.1021/acsmeasuresciau.2c00070 ↗
41. Improved corrosion resistance of AA5083 after 2 years of exposure in seawater splash and tidal zones: formation of a protective surface film10.1016/j.corsci.2025.113573 ↗
42. Accelerated corrosion mechanism of AA5083 coupled with al–zn–in anodes: an impedance analysis10.1016/j.corsci.2025.113448 ↗
43. Effect of Si network continuity on the localized corrosion of AlSi10Mg alloy fabricated by selective laser melting10.1016/j.corsci.2025.113336 ↗
44. Localized corrosion of chromate-passivated AA5052 in NaCl solution: electrochemical and microstructural insights10.1016/j.corsci.2026.113757 ↗
45. Corrosion degradation of AA5083 long-scale specimen exposed to the seawater-air interface of the bohai sea for 2.5 years10.1016/j.matchemphys.2026.132167 ↗