journal article·2026-06

Aluminization and pre-oxidation treatments for enhanced nitridation resistance of reformer alloys under high-pressure ammonia cracking

Nicole Laws, Estefany Sarabia, William L. Roberts, Felipe Campuzano

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metal and Thin Film Mechanics · High-Temperature Coating Behaviors · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. Integrated modeling of steam methane reforming and carbon capture for blue hydrogen production
2. A quicker route to hydrogen economy with ammonia10.1016/j.ijhydene.2024.08.067 ↗
3. Catalytic ammonia cracking: future of material chemistry research for sustainable hydrogen energy economy
4. Techno-economic analysis of ammonia cracking for large scale power generation10.1016/j.ijhydene.2024.05.308 ↗
5. Large-scale decomposition of green ammonia for pure hydrogen production10.1016/j.ijhydene.2021.07.188 ↗
6. Ammonia as a carbon-free energy carrier: NH3 cracking to H210.1021/acs.iecr.3c01419 ↗
7. The technological prospects of repurposing methane steam reformers into ammonia crackers for decarbonized H2 production10.1016/j.apenergy.2024.124244 ↗
8. Effect of high temperature service on the complex through-wall microstructure of centrifugally cast HP40 reformer tube10.1016/j.matchar.2021.111070 ↗
9. High-temperature nitriding of refractory alloys10.1023/B:MSAT.0000029595.28616.40 ↗
10. Growth kinetics and corrosion properties of pack-borided Ti-5Al-2.5Sn alloy10.1016/j.surfcoat.2023.130003 ↗
11. Corrosion and wear behaviors of Inconel 718 nickel-based alloy by boroaluminizing10.1016/j.surfcoat.2024.130500 ↗
12. Microstructure and wear properties of powder-pack borided Ti–5Al–2.5Sn alloy10.1016/j.jmrt.2023.02.052 ↗
13. Microstructure and high-temperature oxidation behaviors of surface layer on TA2 pure titanium by boriding and aluminizing two-steps method10.1016/j.ceramint.2021.11.109 ↗
14. Metal organic chemical vapor deposition of Al2O3 and Cr2O3 on nickel as oxidation barriers10.1016/j.surfcoat.2003.11.022 ↗
15. Behavior of free-standing atmospheric plasma sprayed Al2O3–Cr2O3 solid solution-based coatings under cyclic heating at 1000 °C10.1016/j.surfcoat.2024.131180 ↗
16. Microstructure and wear behaviors of Cr2O3-Al2O3 composite coatings deposited by atmospheric plasma spraying10.1016/j.surfcoat.2022.128619 ↗
17. High temperature oxidation resistance of γ-TiAl alloy with pack aluminizing and electrodeposited SiO2 composite coating10.1016/j.corsci.2018.10.031 ↗
18. Formation of Al2O3 layer on steel10.1023/A:1024785208322 ↗
19. Oxidation resistance and corrosion behavior of hot-dip aluminized coatings on commercial-purity titanium10.1016/j.surfcoat.2011.08.042 ↗
20. High temperature oxidation behavior of aluminized Haynes 23010.1016/j.corsci.2020.108835 ↗
21. Deposition of Ni-Al coatings by pack cementation and corrosion resistance in high temperature and marine environments10.1016/j.corsci.2018.11.003 ↗
22. The oxidation of aluminum at high temperature studied by Thermogravimetric Analysis and Differential Scanning Calorimetry
23. Effect of pre-oxidation and sea salt on the hot corrosion behavior of MCrAlY coatings and AlSi coatings10.1016/j.surfcoat.2023.130354 ↗
24. Microstructural characteristics and long-term high-temperature oxidation resistance of Ti-Al-Si composite coating onTi65 alloy prepared by two-step hot-dipping plus pre-oxidation method10.1016/j.corsci.2025.112808 ↗
25. Thermal performance determination of binary Fe-Al alloys at elevated temperatures10.1016/j.jallcom.2017.01.131 ↗
26. High temperature isothermal oxidation behavior of superheater materials
27. The effect of pre-oxidation treatment on corrosion behavior of ni–cu–fe–al anode in molten CaCl2 salt10.1007/s11085-017-9806-5 ↗
28. Effect of pre-oxidation on the hot corrosion of CoNiCrAlYRe alloy10.1016/j.corsci.2010.09.045 ↗
29. Electrochemical characterization of chromia- and alumina-forming nickel-based superalloys in molten silicates10.1016/j.apsusc.2015.10.176 ↗
30. Failure analysis of FeCrAl heating coils exposed to a high-temperature, high-pressure ammonia environment10.1016/j.engfailanal.2024.108286 ↗
31. Effect of heating rates on non-isothermal and isothermal oxidation behavior of additive friction stir deposited nickel base superalloy IN62510.1016/j.corsci.2025.113174 ↗
32. Influence of high heating rates on evolution of oxides on directed laser energy additively fabricated IN71810.1038/s41529-021-00193-2 ↗
33. High temperature corrosion of Hastelloy C22 in molten alkali salts: the effect of pre-oxidation treatment10.1016/j.corsci.2020.108761 ↗
34. Oxidation mechanism and kinetics of nuclear-grade FeCrAl alloys in the temperature range of 500–1500 °C in steam
35. Design and performance assessment of an experimental rig to conduct material nitridation studies at extreme ammonia conditions
36. ASTM G111-21a. Standard Guide for Corrosion Tests in High Temperature or High Pressure Environment, or Both. doi: 10.1520/G0111-21A.10.1520/G0111-21A ↗
37. High pressure ammonia decomposition on Ru–K/CaO catalysts10.1039/D0CY00686F ↗
38. Kinetics of ammonia synthesis on promoted iron catalysts
39. A Langmuir–Hinshelwood approach to the kinetic modelling of catalytic ammonia decomposition in an integral reactor10.1039/c3cp50715g ↗
40. ASTM G1-03 Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens. doi: 10.1520/G0001-03.10.1520/G0001-03 ↗
41. ASTM E3-11 Standard Guide for Preparation of Metallographic Specimens. doi: 10.1520/E0003-11R17.10.1520/E0003-11R17 ↗
42. Aluminizing of iron-nickel-base alloys for resistance to high-temperature gaseous environments10.1016/0010-938X(92)90065-B ↗
43. Formation of Al2O3/Fe-Al layers on SS 316 surface by pack aluminizing and heat treatment10.1016/j.matchemphys.2017.01.002 ↗
44. Effects of aluminization via thermo-chemical diffusion on the wear behavior of structural materials for high-temperature gas-cooled reactors10.1007/s11661-021-06236-2 ↗
45. Mechanical degradation of coating systems in high-temperature cyclic oxidation10.1016/0257-8972(95)02551-0 ↗
46. On the rumpling mechanism in nickel-aluminide coatings: part I: an experimental assessment
47. A novel single-phase γ′ nanocrystalline coating with high resistance to oxidation and scale rumpling yet mitigated interdiffusion with the alloy substrate10.1016/j.corsci.2021.109866 ↗
48. Evolution of oxide scales on aluminide coatings under isothermal and cyclic conditions10.4028/www.scientific.net/MSF.595-598.11 ↗
49. Diffusion mechanisms and microstructure development in pack aluminizing of Ni-based alloys10.1016/j.surfcoat.2013.11.034 ↗
50. Chapter 6 - oxidation- and corrosion-resistant coatings
51. Determination of alpha and beta alumina in ceramic alumina by X-ray diffraction10.1016/S0584-8547(00)00225-1 ↗
52. Evolution of alumina phase structure in thermal plasma processing10.1016/j.ceramint.2023.03.263 ↗
53. Diffusion–reaction of aluminum and oxygen in thermally grown Al2O3 oxide layers10.1007/s00231-013-1249-1 ↗
54. On the growth of Al2O3 scales10.1016/j.actamat.2013.07.024 ↗
55. Influence of annealing temperature on the phase transformation of Al2O310.1063/1.4941627 ↗
56. Experimental study of thermal expansion and phase transformations in iron-rich Fe-Al alloys10.1016/S0364-5916(99)00014-0 ↗
57. Effect of interface phase transformations on diffusion and segregation in high-angle grain boundaries10.1103/PhysRevLett.110.255502 ↗
58. Wear and oxidation characteristics of aluminized INC738 with different pack contents10.1016/j.surfcoat.2025.132698 ↗
59. Aluminizing for enhanced oxidation resistance of ductile refractory high-entropy alloys10.1016/j.intermet.2018.10.004 ↗
60. Theory of the Kirkendall effect during grain boundary interdiffusion10.1016/j.actamat.2010.10.070 ↗
61. Effect of aluminisation characteristics on the microstructure of single phase β-(Ni,Pt)Al coating and the isothermal oxidation behaviour10.1016/j.corsci.2016.01.024 ↗
62. Production of aluminide layers on AISI 304 stainless steel at low temperatures using the slurry process10.1007/s11665-020-04748-3 ↗
63. Effect of interdiffusion on mechanical and thermal expansion properties at high temperature of a MCrAlY coated Ni-based superalloy10.1016/j.surfcoat.2016.08.059 ↗
64. Effect of Pt on diffusion-controlled growth characteristics of interdiffusion zone between CM247LC superalloy and Ni(Pt)Al bond coat10.1007/s10853-022-08058-y ↗
65. Review on strategies for inhibiting interdiffusion between protective coatings and superalloys under high temperature oxidation10.1007/s11085-023-10197-9 ↗
66. Effect of alloying elements in Ni-base substrate material on interdiffusion processes in MCrAlY-coated systems10.1016/j.surfcoat.2018.07.020 ↗
67. Time evolution of Kirkendall porosity in single-phase Ni-based diffusion couples10.1016/j.actamat.2025.121022 ↗
68. Relationship between porosity, pore parameters and properties of microarc oxidation film on AZ91D magnesium alloy10.1016/j.rinp.2019.01.095 ↗
69. Stress corrosion cracking behaviors of carbon steel in liquid ammonia
70. Cyclic hot corrosion of austenitic stainless steel in molten chloride salts: effect of pre-oxidation treatment10.1016/j.corsci.2025.113428 ↗
71. Acceleration of pitting corrosion of 70Cu–30Ni alloy in seawater by NH4+ and stress10.1016/j.jmrt.2022.12.184 ↗
72. Efficacy of an external chromia layer in reducing nitridation of high temperature alloys10.1016/j.corsci.2021.110050 ↗
73. High-temperature nitridation of Ni-Cr alloys10.1007/BF02647747 ↗
74. Internal nitridation during creep of IN617 superalloy10.1016/j.corsci.2022.110763 ↗
75. Formation and compensation of internal stresses during internal nitridation of nickel-base alloys10.1016/S0921-5093(00)01670-1 ↗