Uncharacteristic evolution of copper type texture in the presence of shearable precipitates
Source abstract
Abstract
Abstract In the present work, development of rolling texture in the presence of shearable precipitates is analyzed using age hardenable aluminum magnesium silicon alloy (AA 6061) and aluminum-copper-lithium alloy (AA 2195). A characteristic Brass type texture evolves upon rolling of AA 6061 alloy containing β’’ (Mg5Si6) precipitates, whereas an unexpected Copper type texture develops upon rolling of AA 2195 alloy containing T1 (Al2CuLi) precipitates. The present work highlights that rolling texture evolution in the presence of shearable precipitates cannot be generalized and depends strongly upon the shearing propensity of these precipitates.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. The brass-type texture and its deviation from the copper-type texture10.1016/j.pmatsci.2008.09.002 ↗
2. New insights into the development of microstructure and deformation texture in nickel–60wt.% cobalt alloy10.1016/j.actamat.2014.06.031 ↗
3. Texture transition in cold-rolled nickel–40wt.% cobalt alloy10.1016/j.actamat.2014.03.066 ↗
4. Unexpected brass-type texture in rolling of ultrafine-grained copper10.1016/j.scriptamat.2014.08.012 ↗
5. Overview no. 76: mechanism of deformation and development of rolling textures in polycrystalline f.c.c. metals—I. Description of rolling texture development in homogeneous CuZn alloys10.1016/0001-6160(88)90172-1 ↗
6. Rolling textures of pure nickel, nickel-iron and nickel-cobalt alloys10.1016/0956-7151(95)90169-8 ↗
7. The early stages of the development of rolling texture in copper and brass10.1155/TSM.8-9.467 ↗
8. On the development of the brass-type texture10.1155/TSM.22.53 ↗
9. Deformation behaviour at macro-and nano-length scales: the development of orientation gradients10.1016/j.matlet.2013.02.074 ↗
10. Deformation texture transition in brass: critical role of micro-scale shear bands10.1016/S1359-6454(00)00050-1 ↗
11. Deformation rate dependence of rolling texture in brass containing 5% zinc10.1016/0036-9748(68)90192-0 ↗
12. Strain rate sensitivity of flow stress and its effect on hot rolling texture development10.1016/0956-716X(93)90475-8 ↗
13. Texture evolution and operative mechanisms during large-strain deformation of nanocrystalline nickel10.1080/14786435.2010.530621 ↗
14. Deformation mechanisms during large strain deformation of nanocrystalline nickel10.1063/1.3132085 ↗
15. Micro-mechanisms of deformation texture evolution in nanocrystalline nickel-cobalt alloys10.1016/j.actamat.2016.08.036 ↗
16. Texture evolution via combined slip and deformation twinning in rolled silver–copper cast eutectic nanocomposite10.1016/j.ijplas.2010.05.007 ↗
17. Texture development in Al 1.8 wt% Cu depending on the precipitation state—I. Rolling textures10.1016/0001-6160(89)90308-8 ↗
18. The shearable–non-shearable transition in Al–Mg–Si–Cu precipitation hardening alloys: implications on the distribution of slip, work hardening and fracture10.1080/14786430500154935 ↗
19. The influence of precipitation on plastic deformation of Al–Cu–Li alloys10.1016/j.actamat.2013.03.015 ↗
20. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al–Li–Cu–X alloy10.1016/S1471-5317(00)00002-X ↗
21. On the stability of the ideal orientations of rolling textures for F.C.C. polycrystals10.1016/0956-7151(92)90481-S ↗
22. Hosford · 1993 · 248
23. Lattice rotation of the cube orientation to the β fiber during cold rolling of AA 5052 aluminum alloy10.1016/S1359-6462(01)01074-0 ↗
24. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al–Cu–Li alloy10.1016/j.msea.2014.03.024 ↗